6 resultados para high-strength steel


Relevância:

100.00% 100.00%

Publicador:

Resumo:


Experimental tests have been completed for high-strength 8.8 bolts for studying their mechanical performance subjected to tensile loading. As observed from these tests, failure of structural bolts has been identified as in one of two ways: threads stripping and necking of the threaded portion of the bolt shank, which is possibly due to the degree of fit between internal and external threads. Following the experimental work, a numerical approach has been developed for demonstration of the tensile performance with proper consideration of tolerance class between bolts and nuts. The degree of fit between internal and external threads has been identified as a critical factor affecting failure mechanisms of high-strength structural bolts in tension, which is caused by the machining process. In addition, different constitutive material laws have been taken into account in the numerical simulation, demonstrating the entire failure mechanism for structural bolts with different tolerance classes in their threads. It is also observed that the bolt capacities are closely associated with their failure mechanisms.

Relevância:

90.00% 90.00%

Publicador:

Resumo:


Natural pozzolans can be activated and condensed with sodium silicate in an alkaline environment to synthesize high performance cementitious construction materials with low environmental impact. The nature of the starting materials including mineral composition, chemical composition and crystal structure groups affects the formation of the geopolymer gel phase. In this paper, the pozzolanic activities of five natural pozzolans are studied. From XRD and XRF results, most of the raw materials contain zeolite clay minerals and have a high loss on ignition. Therefore, before use, samples were calcined at 700, 800 and 900 °C, respectively. The improvement in pozzolanic properties was studied following heat treatment including calcinations and/or elevated curing temperature by using alkali solubility and compressive strength tests. The results show that pozzolan containing sodium zeolite clinoptilolite can be used to prepare a moderate to high strength binder by heat treatment and calcinations can impart disorder hornblende as a constituent of pozzolan with no amorphous phase to prepare a moderate strength binder.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This letter attempts to comment on an article by dos Reis et al., in the aspects of creep considerationand chemical analysis in maraging steels.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Web openings could be used in cold-formed steel beam members, such as wall studs or floor joints, to facilitate ease of services in buildings. In this paper, a combination of tests and non-linear finite element analyses is used to investigate the effect of such holes on web crippling under end-one-flange (EOF) loading condition; the cases of both flanges fastened and unfastened to the bearing plates are considered. The results of 74 web crippling tests are presented, with 22 tests conducted on channel sections without web openings and 52 tests conducted on channel sections with web openings. In the case of the tests with web openings, the hole was either located centred above the bearing plates or having a horizontal clear distance to the near edge of the bearing plates. A good agreement between the tests and finite element analyses was obtained in term of both strength and failure modes.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

A parametric study of cold-formed steel sections with web openings subjected to web crippling under end-one-flange (EOF) loading condition is undertaken, using finite element analysis, to investigate the effects of web holes and cross-section sizes. The holes are located either centred above the bearing plates or with a horizontal clear distance to the near edge of the bearing plates. It was demonstrated that the main factors influencing the web crippling strength are the ratio of the hole depth to the depth of the web, the ratio of the length of bearing plates to the flat depth of the web and the location of the holes as defined by the distance of the hole from the edge of the bearing plate divided by the flat depth of web. In this study, design recommendations in the form of web crippling strength reduction factor equations are proposed, which are conservative when compared with the experimental and finite element results.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Use of higher proportions of fly ash as a cement replacement in concrete has obvious environmental and performance benefits but high volumes of fly ash are not commonly used due to perceived lower early age strengths. In this investigation, addition of cement kiln dust (CKD) and gypsum to activate the fly ash was studied and the proportions used in the paste mixes were designed to optimize the mixture ingredients to achieve the highest early age compressive strength. Change of mineral phase composition and micro structure of the composites was analyzed. It was found that CKD was much more effective in activating the fly ash than gypsum. Appreciable early age compressive strengths were achieved for fly ash contents up to 60% of the binder and these observations were supported by analysis of the mineral phases.