3 resultados para elastic fiber
Resumo:
Composites of recycled carbon fiber (CF) with up to 30 wt % loading with polyethylene (PE) were prepared via melt compounding. The morphology of the composites and the degree of dispersion of the CF in the PE matrix was examined using scanning electron microscopy, and revealed the CF to be highly dispersed at all loadings and strong interfacial adhesion to exist between the CF and PE. Raman and FTIR spectroscopy were used to characterize the surface chemistry and potential bonding sites of recycled CF. Both the Young's modulus and ultimate tensile stress increased with increasing CF loading, but the percentage stress at break was unchanged up to 5 wt % loading, then decreased with further successive addition of CF. The effect of CF on the elastic modulus of PE was examined using the Halpin-Tsai and modified Cox models, the former giving a better fit with the values determined experimentally. The electrical conductivity of the PE matrix was enhanced by about 11 orders of magnitude on addition of recycled CF with a percolation threshold of 7 and 15 wt % for 500-mu m and 3-mm thick samples. (c) 2007 Wiley Periodicals, Inc.
Resumo:
This article discusses the effects of laser welding parameters such as power, welding speed, and focus position on the weld bead profile, microstructure, pseudo-elasticity (PE), and shape memory effect (SME) of NiTi foil with thickness of 250 um using 100W CW fiber laser. The parameter settings to produce the NiTi welds for analysis in this article were chosen from a fractional factorial design to ensure the welds produced were free of any apparent defect. The welds obtained were mainly of cellular dendrites with grain sizes ranging from 2.5 to 4.8 um at the weld centerline. A small amount of Ni3Ti was found in the welds. The onset of transformation temperatures (As and Ms) of the NiTi welds shifted to the negative side as compared to the as-received NiTi alloy. Ultimate tensile stress of the NiTi welds was comparable to the as received NiTi alloy, but a little reduction in the pseudo-elastic property was noted. Full penetration welds with desirable weld bead profiles and mechanical properties were successfully obtained in this study.
Resumo:
Natural fibers can be used in rotational molding process to obtain parts with improved mechanical properties. Different approaches have been followed in order to produce formulations containing banana or abaca fiber at 5% weight, in two- and three-layer constructions. Chemically treated abaca fiber has also been studied, causing some problems in processability. Fibers used have been characterized by Fourier transform infrared (FTIR) spectroscopy, thermogravimetric analysis (TGA), optical microscopy, and single-fiber mechanical tests. Rotomolded parts have been tested for tensile, flexural, and impact properties, demonstrating that important increases in elastic modulus are achieved with these fibers, although impact properties are reduced. © 2013 Copyright Taylor and Francis Group, LLC.