5 resultados para Elastomer rods
Resumo:
The deposition of stiff and strong coatings onto porous templates offers a novel strategy for fabricating macroscale materials with controlled architectures at the micro- and nanoscale. Here, layer-by-layer assembly is utilized to fabricate nanocomposite-coated foams with highly customizable properties by depositing polymer–nanoclay coatings onto open-cell foam templates. The compressive mechanical behavior of these materials evolves in a predictable manner that is qualitatively captured by scaling laws for the mechanical properties of cellular materials. The observed and predicted properties span a remarkable range of density-stiffness space, extending from regions of very soft elastomer foams to very stiff, lightweight honeycomb and lattice materials.
Resumo:
A matrix-type silicone elastomer vaginal ring providing 28-day continuous release of dapivirine (DPV) - a lead candidate human immunodeficiency virus type 1 (HIV-1) microbicide compound - has recently demonstrated moderate levels of protection in two Phase III clinical studies. Here, next-generation matrix and reservoir-type silicone elastomer vaginal rings are reported for the first time offering simultaneous and continuous in vitro release of DPV and the contraceptive progestin levonorgestrel (LNG) over a period of between 60 and 180days. For matrix-type vaginal rings comprising initial drug loadings of 100, 150 or 200mg DPV and 0, 16 or 32mg LNG, Day 1 daily DPV release values were between 4132 and 6113μg while Day 60 values ranged from 284 to 454μg. Daily LNG release ranged from 129 to 684μg on Day 1 and 2-91μg on Day 60. Core-type rings comprising one or two drug-loaded cores provided extended duration of in vitro release out to 180days, and maintained daily drug release rates within much narrower windows (either 75-131μg/day or 37-66μg/day for DPV, and either 96-150μg/day or 37-57μg/day for LNG, depending on core ring configuration and ignoring initial lag release effect for LNG) compared with matrix-type rings. The data support the continued development of these devices as multi-purpose prevention technologies (MPTs) for HIV prevention and long-acting contraception.
Resumo:
In this study, fibre optic sensors (FOS) were used to investigate the interfacial stress-strain behaviour of bonded-in basalt fibre reinforced polymer (BFRP) rods loaded into glulam members. Pull-out tests were conducted to examine the effect of bonded length and load-to-grain direction on the distribution of stress at the BFRP rod/adhesive zone. It was observed that the stress concentration at the loaded end of the BFRP rod of the samples was significantly the highest while the unloaded end showed the lowest. Increasing the bonded length at the same loading configuration resulted in a decrease in stress concentration at the loaded end. The stress concentration at the loaded end of the perpendicular to the grain samples was relatively higher than that of the corresponding parallel to the grain samples.