Post-weld heat-treatment (PWHT) was applied to NiTi weldments to improve the corrosion behaviour by modifying the microstructure and surface composition. The surface oxide film on the weldments is principally TiO2, together with some Ti, TiO, and Ti2O3. The surface Ti/Ni ratio of the weldments after PWHT is increased. The oxide film formed in Hanks’ solution is thicker on the weldments after PWHT. The pitting resistance of the weldments is increased by PWHT. The galvanic effect in the weldments is very small. The weldment with PWHT at 350 °C shows the best corrosion resistance among other heat-treated weldments in this study.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this study, the environmentally induced cracking behaviour of the NiTi weldment with and without post-weld heat-treatment (PWHT) in Hanks’ solution at 37.5 °C at OCP were studied by tensile and cyclic slow-strain-rate tests (SSRT), and compared with those tested in oil (an inert environment). Our previous results in the tensile and cyclic SSRT showed that the weldment without PWHT showed high susceptibility to the hydrogen cracking, as evidenced by the degradation of tensile and super-elastic properties when testing in Hanks' solution. The weldment after PWHT was much less susceptible to hydrogen attack in Hanks' solution as no obvious degradation in the tensile and super-elastic properties was observed, and only a very small amount of micro-cracks were found in the fracture surface. The susceptibility to hydrogen cracking of the NiTi weldment could be alleviated by applying PWHT at the optimized temperature of 350 °C after laser welding.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this study, the stress-corrosion cracking (SCC) behaviour of laser-welded NiTi wires before and after post-weld heat-treatment (PWHT) was investigated. The samples were subjected to slow strain rate testing (SSRT) under tensile loading in Hanks’ solution at 37.5 °C (or 310.5 K) at a constant anodic potential (200 mVSCE). The current density of the samples during the SSRT was captured by a potentiostat, and used as an indicator to determine the susceptibility to SCC. Fractography was analyzed using scanning-electron microscopy (SEM). The experimental results showed that the laser-welded sample after PWHT was immune to the SCC as evidenced by the stable current density throughout the SSRT. This is attributed to the precipitation of fine and coherent nano-sized Ni4Ti3 precipitates in the welded regions (weld zone, WZ and heat-affected zone, HAZ) after PWHT, resulting in (i) enrichment of TiO2 content in the passive film and (ii) higher resistance against the local plastic deformation in the welded regions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

NiTi wires of 0.5 mm diameter were laser welded using a CW 100-W fiber laser in an argon shielding environment with or without postweld heat-treatment (PWHT). The microstructure and the phases present were studied by scanning-electron microscopy (SEM), transmission-electron microscopy (TEM), and X-ray diffractometry (XRD). The phase transformation behavior and the cyclic stress–strain behavior of the NiTi weldments were studied using differential scanning calorimetry (DSC) and cyclic tensile testing. TEM and XRD analyses reveal the presence of Ni4Ti3 particles after PWHT at or above 623 K (350 °C). In the cyclic tensile test, PWHT at 623 K (350 °C) improves the cyclic deformation behavior of the weldment by reducing the accumulated residual strain, whereas PWHT at 723 K (450 °C) provides no benefit to the cyclic deformation behavior. Welding also reduces the tensile strength and fracture elongation of NiTi wires, but the deterioration could be alleviated by PWHT.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The relationship between microstructure and deformation and damage behaviour during dynamic compression in Ti-3Al-5Mo-5V alloy has been studied using several experimental techniques, including optical microscopy, scanning electron microscopy and microhardness measurements. It was found that the deformation behaviour during dynamic compression was closely related to deformation parameters. After dynamic deformation, the deformation shear band that formed in the titanium alloy had microhardness similar to that of the matrix. However, the microhardness of the white shear band was much higher than the matrix microhardness. The effects of deformation parameters, including deformation rate and deformation degree, on deformation localisation were investigated. Based on the results from the present work, the microstructure and deformation processing parameters can be optimised. In addition, treatment methods after dynamic compression were explored to restore alloy properties. Using post-deformation heat treatment, the microstructure and property inhomogeneity caused by shear bands could be largely removed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this study, two L27 Taguchi experiments were carried out to study the effect of fibre laser welding parameters and their interactions upon the weld bead aspect ratio of nickel–titanium thin foil. The optimum parameters to produce full penetrated weld with the largest aspect ratio and desirable microstructure were successfully obtained by the Taguchi experimental design. The corrosion property of the optimized NiTi weld in Hank’s solution at 37.5 °C was studied and compared with the as-received NiTi. To improve the corrosion properties of the weld, the effect of post-weld-heat-treatments ranging from 573 to 1173 K was investigated. The corrosion properties, surface morphology, microstructure and Ti/Ni ratio of the heat-treated NiTi weld were analysed. It was found that a post-weld heat treatment at 573 K for 1 h provided the best pitting corrosion resistance at the weld zone.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Post-weld heat-treatment (PWHT) has been established as one of the cost-effective ways to improve the functional properties, namely shape memory and super-elastic effects (SME and SE), of laser-welded NiTi alloys. However, the functional performance of the laser-welded joint at different working temperatures has not been explored yet. The purpose of this study is to investigate the effect of different working temperatures on the functional properties of the laser-welded NiTi alloys before and after PWHT by applying cyclic deformation tests. Two laser-welded samples: as-welded and heat-treated sample (after PWHT at 350 oC or 623 K) were tested in this work at room temperature, 50 oC (or 323 K) and 75 oC (or 348 K) respectively. The samples were cyclically loaded and unloaded for 10 cycles up to 4 % strain. The critical stress to induce the martensitic transformation and the residual strain after the cyclic tests were recorded. The results indicate that the heat-treated sample exhibited better functional properties than the as-welded sample at room temperature and 50 oC (or 323 K). However, both the as-welded and heat-treated samples failed in the cyclic tests at 75 oC (or 348 K). These findings are important to determine the feasible working temperature range for the laser-welded NiTi components to exhibit desirable functional properties in engineering applications involving cyclic loading.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Issues of authenticity and identity are particularly significant in cities where social and cultural change is shaping active transformation of its urban fabric and structure in the post-war condition. In search of sustainable future, Iraqi cities are stretched between the two ends of the spectrum, authentic quarters with its traditional fabric and modern districts with their global sense of living. This paper interrogates the reciprocal influences, distinct qualities and sustainable performance of both authentic and modern quarters of Erbil, the
capital of the Iraqi province of Kurdistan, as factors in shaping sustainable urban forms for Iraqi cities. In doing so, the paper, firstly, seeks to highlight the urban identity as an effective factor in relation to sustainable urban form. Secondly, the city of Erbil in Iraq has been chosen as a field study, due to its regional, social, political and historical role in the region. Thirdly, the study emphasises the dynamic activities and performance of residential projects according to rational sustainable criteria. The research concludes that urban identity and the sense of place in traditional and historical places should inform design strategies in order to achieve a more sustainable urban context.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Post-apartheid South Africa is characterized by centralized, neo-liberal policymaking that perpetuates, and in some cases exaggerates, socio-economic inequalities inherited from the apartheid era. The African National Congress (ANC) leadership’s alignment with powerful international and domestic market actors produces tensions within the Tripartite Alliance and between government and civil society. Consequently, several characteristics of ‘predatory liberalism’ are evident in contemporary South Africa: neo-liberal restructuring of the economy is combined with an increasing willingness by government to assert its authority, to marginalize and delegitimize those critical of its abandonment of inclusive governance. A new form of oligarch power, combining entrenched economic interests with those of a new ‘black bourgeoisie’ promoted by narrowly implemented Black Economic Empowerment policies, diminishes prospects for broad-based socio-economic transformation. Because the new policy environment is failing to resolve tensions between global market demands for increasing market liberalization and domestic popular demands for poverty-alleviation and socio-economic transformation, the ANC leadership is forced increasingly to confront ‘ultra-leftists’ who are challenging its credentials as defender of the National Democratic Revolution which was the cornerstone in the anti-apartheid struggle.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Ionic liquids are organic salts with low melting points. Many of these compounds are liquid at room temperature in their pure state. Since they have negligible vapor pressure and would not contribute to air pollution, they are being intensively investigated for a variety of applications, including as solvents for reactions and separations, as non-volatile electrolytes, and as heat transfer fluids. We present melting temperatures, glass transition temperatures, decomposition temperatures, heat capacities, and viscosities for a large series of pyridinium-based ionic liquids. For comparison, we include data for several imidazolium and quaternary ammonium salts. Many of the compounds do not crystallize, but form glasses at temperatures between 188 K and 223 K. The thermal stability is largely determined by the coordinating ability of the anion, with ionic liquids made with the least coordinating anions, like bis(trifluoromethylsulfonyl)imide, having the best thermal stability. In particular, dimethylaminopyridinium bis(trifluoromethylsulfonyl)imide salts have some of the best thermal stabilities of any ionic liquid compounds investigated to date. Heat capacities increase approximately linearly with increasing molar mass, which corresponds with increasing numbers of translational, vibrational, and rotational modes. Viscosities generally increase with increasing number and length of alkyl substituents on the cation, with the pyridinium salts typically being slightly more viscous than the equivalent imidazolium compounds. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Electroless nickel (EN) coatings are recognised for their hardness and wear resistance in automotive and aerospace industries. In this work, electroless Ni–P coatings were deposited on aluminium alloy substrate LM24 (Al–9 wt.% Si alloy) and the effect of post treatment on the wear resistance was studied. The post treatments included heat treatment and lapping with two different surface textures. Scanning electron microscopy (SEM), energy dispersive spectrometry (EDS), X-ray diffraction (XRD) and micro-abrasion tester were used to analyse morphology, structure and abrasive wear resistance of the coatings. Post heat treatment significantly improved the coating density and structure, giving rise to enhanced hardness and wear resistance. Microhardness of electroless Ni–P coatings with thickness of about 15 μm increased due to the formation of Ni3P after heat treatment.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper focuses on the revival of private property and its limits in urban China. It explores the emergence of urban property markets; urban property-holding in relation to the complexity of urban governance; “minor property rights apartments” that form a de facto real estate market and cross over the urban-rural divide; the “grey areas” of blurring legal and administrative boundaries in modern China; and recent changes to the rural land system and the rural-urban divide. The conclusion flags the theme of the city as laboratory with regard to the blurring legal and governmental urban-rural distinction.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The formation of ATP breakdown products in chicken M. pectoralis major post-slaughter is reported. The concentrations of metabolites were followed in chicken breast throughout the carcass processing post-slaughter and during chilled storage. The concentration of glucose remains similar throughout the period whilst that of glucose-6-phosphate decreases linearly. Glucose and glucose-6-phosphate concentrations were inversely related to the pHu of the breast meat throughout chilled storage. Rapid post-mortem glycolysis and high pHu values suggest the occurrence of stress at and pre-slaughter. Whilst ATP, ADP and AMP were rapidly broken down, the concentration of IMP rose rapidly and remained high. Concentrations of inosine, ribose and hypoxanthine increased gradually post-slaughter but an initial increase in ribose phosphate was not sustained. Most of the potential ribose present in chicken meat, believed to be important for flavor formation, remains bound in the form of inosine and IMP. There is evidence that additional breakdown pathways for ribose and ribose-5-phosphate may deplete the concentrations of these precursors.