Resumo:

Twenty-five patients with chronic venous leg ulcers were treated in general practice by pinch grafting. Fifteen of the ulcers (60%) were completely healed one year after grafting. Prior to grafting 19 patients (76%) complained of daily pain in the ulcer. These patients experienced complete relief from pain after grafting. Pinch grafting is a simple, safe and effective therapy when applied in a domiciliary environment.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Abstract There is considerable interest in developing medical devices that provide controlled delivery of biologically active agents, for example, to reduce the incidence of device-related infection. Silicone elastomers are one of the commonest biomaterials used in medical device production. However, they have a relatively high coefficient of friction and the resulting lack of lubricity can cause pain and tissue damage on device insertion and removal. Novel silicone cross-linking agents have recently been reported that produce inherently ‘self-lubricating’ silicone elastomers with very low coefficients of friction. In this study, the model antibacterial drug metronidazole has been incorporated into these self-lubricating silicone elastomers to produce a novel bioactive biomaterial. The in vitro release characteristics of the bioactive component were evaluated as a function of cross-linker composition and drug loading. Although conventional matrix-type release kinetics were observed for metronidazole from the silicone systems, it was also observed that increasing the concentration of the cross-linking agent responsible for the lubricious character (tetra(oleyloxy)silane) relative to that of the standard non-lubricious cross-linking agent (tetrapropoxysilane) produced an increase in the metronidazole flux rate by up to 65% for a specified drug loading. The results highlight the potential for developing lubricious silicone medical devices with enhanced drug release characteristics.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Silicone has a relatively high coefficient of friction and silicone medical devices therefore lack inherent lubricity, leading to pain on device insertion and potential tissue trauma. In this study, higher molecular weight tetra(alkoxy) silanes, particularly tetra(oleyloxy) silane, have been used as crosslinkers in the condensation cure of a hydroxy end-functionalised linear poly(dimethylsiloxane). The resulting elastomers displayed a persistent lubricous surface of oleyl alcohol, and coefficients of friction (static and dynamic) approaching zero. Chemical structures of the synthesised silanes and surface alcohol exudate were confirmed by nuclear magnetic resonance spectroscopy. Mechanical properties of the elastomers, which were chemically identical to conventionally cured systems, suggested that an 80/20 mixture of tetra(oleyloxy) silane and tetra(propoxysilane) gave the best compromise between desirable mechanical and frictional properties.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The development of self-lubricating silicone elastomeric biomaterials, prepared using the novel crosslinking agent tetra( oleyloxy) silane and having very low coefficients of friction, has recently been reported. In this study, the in vitro release characteristics of lubricious oleyl alcohol produced during the silicone curing reaction have been quantitatively evaluated for a range of tetra( propoxy) silane/tetra(oleyloxy) silane crosslinker compositions using a novel evaporative light scattering detection method in combination with high performance liquid chromatography. The mechanism of oleyl alcohol release was seen to deviate from a simple, matrix-controlled diffusion process and instead obeyed an anomalous transport mechanism. An explanation for the observed release behaviour has been proposed based on competitive reaction kinetics between the tetra( oleyloxy) silane and tetra( propoxy) silane substituents of the silicone crosslinking agents.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

There is currently a need to expand the range of graft materials available to orthopaedic surgeons. This study investigated the effect of ternary phosphate based glass (PBG) compositions on the behaviour of osteoblast and osteoblast-like cells. PBGs of the formula in mol% P2O5 (50)-CaO (50-X)-Na2O (X), where X was either 2, 4, 6, 8 or 10 were produced and their influence on the proliferation, differentiation and death in vitro of adult human bone marrow stromal cells (hBMSCs) and human fetal osteoblast 1.19 (HFOB 1.19) cells were assessed. Tissue culture plastic (TCP) and hydroxyapatite (HA) were used as controls. Exposure to PBGs in culture inhibited cell adhesion, proliferation and increased cell death in both cell types studied. There was no significant difference in %cell death between the PBGs which was significantly greater than the controls. However, compared to other PBGs, a greater number of cells was found on the 48 mol% CaO which may have been due to either increased adherence, proliferation or both. This composition was capable of supporting osteogenic proliferation and early differentiation and supports the notion that chemical modification of the glass could to lead to a more biologically compatible substrate with the potential to support osteogenic grafting. Realisation of this potential should lead to the development of novel grafting strategies for the treatment of problematic bone defects.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Heterogeneous immobilized ionic liquid catalysts were prepared via grafting of 1,3-dimethyl-3-(3-triethoxysilylpropyl)-imidazolium tetrafluoroborate or bist{(trifluoromethyl)sulfonyl} imide ([NTf2](-)) on silica supports with different surfaces and pore size. In addition to the adsorption-desorption isotherms of nitrogen at -196C, the catalysts were characterized by TG-DTA, XPS, DRIFTS, DR-UV-vis, NMR, and XRD techniques. The catalytic behavior was checked in the acylation of three different sulfonamines: benzenesulfonamine, p-nitrobenzene-sulfonamine, and p-methoxybenzene-sulfonamine with acetic acid, acetic anhydride and maleic anhydride. These tests confirmed the acid Lewis properties of these catalysts. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An extensive chloride profiling program was undertaken on concrete pier stems erected in the vicinity of the Dornoch Bridge located at the Dornoch Firth in Northeast Scotland. The pier stems were 2 m (6.562 ft) high and octagonal in plan with 0.66 m (2.165 ft) wide faces. The piers were constructed in sets of three with the lowest of each set in the tidal zone and the highest in the atmospheric zone. The pier stems were placed in such a way that they would represent the exposure conditions of the actual bridge piers of the Dornoch Bridge. In all, six of the pier stems were made using plain ordinary portland cement (OPC) concrete (with three of these having the surface treated with silane); the remaining three pier stems had a concrete containing caltite as an additive. Three exposurezones were studied: the tidal zone, the splash zone, and the atmospheric zone. The tidal zone was further subdivided into two levels defined as low-level and high-level. Chloride profiles were obtained from the different regimes over a period of 7 years for all nine pier stems. This paper describes the nature of chloride ingress and the usefulness of diffusion parameters in classifying each exposure regimes. Furthermore, the effectiveness of silane and caltite in protecting concrete from chloride ingress in different exposure zones was studied.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Microbial adhesion to silicone elastomer biomaterials is a major problem often resulting in infection and medical device failure. Several strategies have been employed to modulate eukaryotic cell adhesion and to hamper bacterial adherence to polymeric biomaterials. Chemical modification of the surface by grafting of polyethylene glycol (PEG) chains or the incorporation of non-antibiotic antimicrobial agents such as triclosan into the biomaterial matrix may reduce bacterial adhesion. Here, such strategies are simultaneously applied to the preparation of both condensation-cure and addition-cure silicone elastomer systems, seeking a sustained release antimicrobial device biomaterial. The influence of triclosan incorporation and degree of pegylation on antimicrobial release, surface microbial adherence and persistence (Escherichia coli and Staphylococcus epidermidis) were evaluated in vitro. Non-pegylated silicone elastomers provided an increased percentage release of triclosan extending over a relatively short duration (99% release by day 64) compared with their pegylated (4% w/w) counterparts (65% and 72% release by day 64, for condensation and addition-cure systems respectively). Viable E. coli adherence to a non-pegylated silicone elastomer containing 1% w/w triclosan was reduced by over 99% after 24 h compared to the non-pegylated silicone elastomer containing no triclosan. No viable S. epidermidis adhered to any of the triclosan-loaded (>0.1% w/w) formulations other than the control. Persistence of the antimicrobial activity of the triclosan-loaded pegylated silicone elastomers continued for at least 70 days compared to the triclosan-loaded non-pegylated elastomers (at least 49 days). Understanding how PEG affects the release of triclosan from silicone elastomers may prove useful in the development of a biomaterial providing prolonged, effective antimicrobial activity.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Ta2O5-SiO2 catalysts were prepared by a sol-gel method using tetraethyl orthosilicate (TEOS) and tantalum (V) ethoxide as the sources of silicon and tantalum, and two families of quaternary ammonium salts, [CnH(2n+1)(CH3)(3)N]Br (n = 14, 16, 18) and [(CnH(2n+1))(4)N]Br (n = 10, 12, 16, 18) as surfactants. The catalysts were compared for the selective suffoxidation of 4,6-dimethyl-2-thiomethylpyrimidine using peroxide as an oxidising agent in a range of ionic liquids and organic solvents. The sol-gel catalysts were also compared with tantalum on MCM-41 prepared by grafting. The catalysts were characterized from adsorption-desorption isotherms of N-2, XRD patterns, small-angle X-ray scattering, IR spectra from adsorbed pyridine and CDCl3, XPS spectra, and Si-29 magic angle spinning (MAS) NNIR experiments. The effect of recycling on the catalyst leaching and selectivity/activity was also studied. High activities and selectivities were found in [NTf2](-) based ionic liquids and organic solvents with good recyclability of the catalyst. Tantalum was found in the solution after reaction; however, this was determined to be due to entrapment of catalyst particulates, as opposed to leaching of the active metal. (c) 2005 Elsevier Inc. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Two different procedures were compared for the preparation of cellulose nanofibres from flax and microcrystalline cellulose (MCC). The first involved a combination of high energy ball milling, acid hydrolysis and ultrasound, whilst the second employed a high pressure homogenisation technique, with and without various pre-treatments of the fibrous feedstock. The geometry and microstructure of the cellulose nanofibres were observed by SEM and TEM and their particle size measured using image analysis and dynamic light scattering. Aspect ratios of nanofibres made by microfluidisation were orders of magnitude greater than those achieved by acid hydrolysis. FTIR, XRD and TGA were used to characterise changes to chemical functionality, cellulose crystallinity and thermal stability resulting from the approaches used for preparing the cellulose nanofibres. Hydrolysis using sulphuric acid gave rise to esterification of the cellulose nanofibres, a decrease in crystallinity with MCC, but an increase with flax, together with an overall reduction in thermal stability. Increased shear history of flax subjected to multiple passes through the microfluidiser, raised both cellulose nanofibril crystallinity and thermal stability, the latter being strongly influenced by acid, alkaline and, most markedly, silane pretreatment.