2 resultados para La2O3
em QUB Research Portal - Research Directory and Institutional Repository for Queen's University Belfast
Resumo:
A series of Cu-zirconia catalysts containing various additives (Y2O3, La2O3, Al2O3 and CeO2) have been prepared by coprecipitation and their activities and stabilities under operating conditions have been obtained for the steam reforming of methanol. It has been found that an yttria-promoted catalyst containing 30 mol% Cu and 20 mol% of Y2O3 is not only very active but is also very stable under reaction conditions. The yttria appears to stabilise a high copper surface area and may also have a slight promotional effect on the copper. The results obtained with this material compare very favourably with data for the best catalysts reported in the literature. (C) 2007 Published by Elsevier B.V.
Resumo:
La3FMo4O16 crystallizes in the triclinic crystal system with space group P (1) over bar [a = 724.86(2) pm, b = 742.26(2) pm, c = 1469.59(3) pm, a = 101.683(2)degrees, beta 102.118(2)degrees, gamma = 100.279(2)degrees] with two formula units per unit cell. The three crystallographically independent La3+ cations show a coordination number of nine each, with one F- and eight O2- anions forming distorted monocapped square antiprisms. The fluoride anion is coordinated by all three lanthanum cations to form a nearly planar triangle. Besides three crystallographically independent tetrahedral [MoO4](2-) units, a fourth one with a higher coordination number (CN = 4 +1) can be found in the crystal structure, forming a dimeric entity with a formula of [Mo2O8](4-) consisting of two edge-connected square pyramids. Several spectroscopic measurements were performed on the title compound, such as infrared, Raman, and diffuse reflectance spectroscopy. Furthermore, La3FMo4O16 was investigated for its capacity to work as host material for doping with luminescent active cations, such as Ce3+ or Pr3+. Therefore, luminescence spectroscopic as well as EPR measurements were performed with doped samples of the title compound. Both the pure and the doped compounds can be synthesized by fusing La2O3, LaF3 and MoO3 (ratio 4:1:12; ca. 1 % CeF3 and PrF3 as dopant, respectively) in evacuated silica ampoules at 850 degrees C for 7 d.