420 resultados para Drug Packaging
em QUB Research Portal - Research Directory and Institutional Repository for Queen's University Belfast
Resumo:
Abstract There is considerable interest in developing medical devices that provide controlled delivery of biologically active agents, for example, to reduce the incidence of device-related infection. Silicone elastomers are one of the commonest biomaterials used in medical device production. However, they have a relatively high coefficient of friction and the resulting lack of lubricity can cause pain and tissue damage on device insertion and removal. Novel silicone cross-linking agents have recently been reported that produce inherently ‘self-lubricating’ silicone elastomers with very low coefficients of friction. In this study, the model antibacterial drug metronidazole has been incorporated into these self-lubricating silicone elastomers to produce a novel bioactive biomaterial. The in vitro release characteristics of the bioactive component were evaluated as a function of cross-linker composition and drug loading. Although conventional matrix-type release kinetics were observed for metronidazole from the silicone systems, it was also observed that increasing the concentration of the cross-linking agent responsible for the lubricious character (tetra(oleyloxy)silane) relative to that of the standard non-lubricious cross-linking agent (tetrapropoxysilane) produced an increase in the metronidazole flux rate by up to 65% for a specified drug loading. The results highlight the potential for developing lubricious silicone medical devices with enhanced drug release characteristics.
Resumo:
The silicone elastomer solubilities of a range of drugs and pharmaceutical excipients employed in the development of silicone intravaginal drug delivery rings (polyethylene glycols, norethisterone acetate, estradiol, triclosan, oleyl alcohol, oxybutynin) have been determined using dynamic mechanical analysis. The method involves measuring the concentration-dependent decrease in the storage modulus associated with the melting of the incorporated drug/excipient, and extrapolation to zero change in storage modulus. The study also demonstrates the effect of drug/excipient concentrations on the mechanical stiffness of the silicone devices at 37°C.
Resumo:
Conventional differential scanning calorimetry (DSC) techniques are commonly used to quantify the solubility of drugs within polymeric-controlled delivery systems. However, the nature of the DSC experiment, and in particular the relatively slow heating rates employed, limit its use to the measurement of drug solubility at the drug's melting temperature. Here, we describe the application of hyper-DSC (HDSC), a variant of DSC involving extremely rapid heating rates, to the calculation of the solubility of a model drug, metronidazole, in silicone elastomer, and demonstrate that the faster heating rates permit the solubility to be calculated under non-equilibrium conditions such that the solubility better approximates that at the temperature of use. At a heating rate of 400 degrees C/min (HDSC), metronidazole solubility was calculated to be 2.16 mg/g compared with 6.16 mg/g at 20 degrees C/min. (C) 2005 Elsevier B.V. All rights reserved.
Resumo:
Ultra-high molecular weight polyethylene (UHMWPE) is used for wear applications in total hip prostheses and total knee prostheses. Sterilisation of these prostheses is commonly by gamma-irradiation. This process creates reactive free radicals in the UHMWPE, greatly increasing its susceptibility to oxidative degradation. This study has investigated the influence of air and vacuum packaging on the properties of gamma-irradiated UHMWPE (GUR1050) following 3 years of shelf ageing. The findings indicate that vacuum packaging minimises oxidative degradation reactions that occur for UHMWPE during shelf ageing. However, gamma-irradiation of vacuum-packaged UHMWPE promotes a degree of cross-linking. It is proposed that this may enhance the wear performance of UHMWPE. Accelerated ageing studies indicate that 3 years of shelf ageing would also seem to reduce the susceptibility of gamma-irradiated UHMWPE to oxidative degradation upon removal from its vacuum packaging.