120 resultados para Probiotic strain
Resumo:
This paper addresses the problems of effective in situ measurement of the real-time strain for bridge weigh in motion in reinforced concrete bridge structures through the use of optical fiber sensor systems. By undertaking a series of tests, coupled with dynamic loading, the performance of fiber Bragg grating-based sensor systems with various amplification techniques were investigated. In recent years, structural health monitoring (SHM) systems have been developed to monitor bridge deterioration, to assess load levels and hence extend bridge life and safety. Conventional SHM systems, based on measuring strain, can be used to improve knowledge of the bridge's capacity to resist loads but generally give no information on the causes of any increase in stresses. Therefore, it is necessary to find accurate sensors capable of capturing peak strains under dynamic load and suitable methods for attaching these strain sensors to existing and new bridge structures. Additionally, it is important to ensure accurate strain transfer between concrete and steel, adhesives layer, and strain sensor. The results show the benefits in the use of optical fiber networks under these circumstances and their ability to deliver data when conventional sensors cannot capture accurate strains and/or peak strains.
Resumo:
In this Letter, an unambiguous synthetic strategy is reported for the preparation of enantiomerically purecis-5-halo-piperazic acid derivatives in single diastereoisomer form. Contrary to the recent report by Shin and co-workers (Chem. Lett. 2001, 1172), in which it is claimed that the Ph3P and N-chlorosuccinimide (NCS)-mediated chlorination of (3R,5S)-trans-N(1),N(2)-di-t-Boc-5-hydroxy-piperazic acid derivative 1proceeds with retention of configuration at C(5) to give 2, we now show that this and related Ph3P-mediated halogenations all occur with SN2 inversion at the alcohol center, as is customary for such reactions. Specifically, we demonstrate that the (3R,5S)-trans-5-Cl-piperazic acid derivative 2 claimed by Shin and co-workers (Chem. Lett. 2001, 1172) is in actual fact the chlorinated (3S,5R)-enantiomer 6, which must have been prepared from the cis-(3S,5S)-alcohol 3, a molecule whose synthesis is not formally described in the Shin paper. We further show here that the cis-(3R,5R)-5-Cl-Piz 13 claimed by Shin and co-workers inChem. Lett. 2001, 1172, is also (3S,5R)-trans-5-Cl-Piz 6. Authentic 13 has now been synthesized by us, for the very first time, here. Since Lindsley and Kennedy have recently utilized the now invalid Shin and co-workers’ retentive Ph3P/NCS chlorination procedure on 1 in their synthetic approach to piperazimycin A (Tetrahedron Lett. 2010, 51, 2493), it follows that their claimed 5-Cl-Piz-containing dipeptide 25 probably has the alternate structure 26, where the 5-Cl-Piz residue has a 3,5-cis-configuration. The aforementioned stereochemical misassignments appear to have come from a mix-up of starting materials by Shin and co-workers (Chem. Lett. 2001, 1172), and an under-appreciation of the various steric and conformational effects that operate in N(2)-acylated piperazic acid systems, most especially rotameric A1,3-strain. The latter has now been unambiguously delineated and defined here under the banner of the A1,3-rotamer effect.
Resumo:
In the research of the microstructural influence on dynamic compression, an assumption that the α and the β phases in titanium alloys were linearly strengthened was proposed, and a two-dimensional model using ANSYS (ANSYS, Inc., Canonsburg, PA) focusing on the role of microgeometrical structure was developed. By comparing the stress and strain distributions of different microstructures, the roles of cracks and phase boundaries in titanium compression were studied.
Resumo:
Existing studies have shown conclusively that the measured fibre reinforced polymer (FRP) rupture strain in FRP wrapped concrete columns is usually significantly smaller than the rupture strain obtained from flat coupon tests. One of the main causes for this phenomenon is the existence of geometrical discontinuities at both ends of the FRP sheets. This study proposes a new strengthening method in which continuous FRP spiral wrapping is used to eliminate strain concentrations due to the geometrical discontinuities and thus increase the FRP rupture strain at column failure. The effect of the spiral angle of FRP on the FRP rupture strain in FRP wrapped specimens was experimentally investigated. The test results indicate that the spiral wrapping with a small angle with respect to the column circumference can significantly increase the strain efficiency of FRP and thus enhance the axial compression capacity of the strengthened cylinders.
Resumo:
Deep-seated progressive failures of cuttings in heavily overconsolidated clays have been observed in the field and are well documented, especially for London Clays (Potts, Kovacevic, & Vaughan, 1997; Smethurst, Powrie, & Clarke, 2006; Take, 2003), however, the process of softening and the development of a rupture surface in other clays, including the clay fraction of glacial tills, is still to be established. Recent decades have witnessed extreme weather conditions in Northern Ireland with dry summers and wet winters. The dynamics of this pore pressure variation can trigger strength reduction and progressive plastic straining, both of which will lead to slope failure. The aim of this research is to evaluate the effect of pore pressure variations on the deformation and long-term stability of large cuttings in glacial tills in Northern Ireland. This paper outlines the overall research program and presents initial laboratory findings (Carse, 2013).
Resumo:
Stiffness values in geotechnical structures can range over many orders of magnitude for relatively small operational strains. The typical strain levels where soil stiffness changes most dramatically is in the range 0.01-0.1%, however soils do not exhibit linear stress-strain behaviour at small strains. Knowledge of the in situ stiffness at small strain is important in geotechnical numerical modelling and design. The stress-strain regime of cut slopes is complex, as we have different principle stress directions at different positions along the potential failure plane. For example, loading may be primarily in extension near the toe of the slope, while compressive loading is predominant at the crest of a slope. Cuttings in heavily overconsolidated clays are known to be susceptible to progressive failure and subsequent strain softening, in which progressive yielding propagates from the toe towards the crest of the slope over time. In order to gain a better understanding of the rate of softening it would be advantageous to measure changes in small strain stiffness in the field.
Resumo:
In order to assess the susceptibility of candidate structural materials to liquid metal embrittlement, this work investigated the tensile behaviors of ferritic-martensitic steel in static lead bismuth eutectic (LBE). The tensile tests were carried out in static lead bismuth eutectic under different temperatures and strain rates. Pronounced liquid metal embrittlement phenomenon is observed between 200 °C and 450 °C. Total elongation is reduced greatly due to the liquid metal embrittlement in LBE environment. The range of ductility trough is larger under slow strain rate tensile (SSRT) test.