118 resultados para coir fibre


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Weathering of stone is one of the major reasons for the damage of stone masonry structures and it takes place due to interlinked chemical, physical and biological processes in stones. The key parameters involved in the deterioration processes are temperature, moisture and salt. It is now known that the sudden variations in temperature and moisture greatly accelerate the weathering process of the building stone fabric. Therefore, in order to monitor these sudden variations an effective and continuous monitoring system is needed. Furthermore, it must consist of robust sensors which are accurate and can survive in the harsh environments experienced in and around masonry structures. Although salt penetration is important for the rate of deterioration of stone masonry structures, the processes involved are much slower than the damage associated with temperature and moisture variations. Therefore, in this paper a novel fibre optic temperature cum relative humidity sensor is described and its applicability in monitoring building stones demonstrated. The performance of the sensor is assessed in an experiment comprising wetting and drying of limestone blocks. The results indicate that the novel fibre optic relative humidity sensor which is tailor made for applications in masonry structures performed well in wetting and drying tests, whilst commercial capacitance based sensors failed to recover during the drying regime for a long period after a wetting regime. That is, the fibre optic sensor has the capability to measure both sorption and de-sorption characteristics of stone blocks. This sensor is used in a test wall in Oxford and the data thus obtained strengthened the laboratory observations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, the reliability and thus the suitability of optical fibre strain sensors for surface strain measurement in concrete structures was investigated. Two different configurations of optical strain sensors were used each having different mountings making them suitable for different uses in various structures. Due to the very limited time available to install the sensors and take result, commercially packaged sensors were used. In the tests carried out each sensor was mounted onto a concrete beam which was then subjected to a range of known and calibrated loadings. The performance of the optical strain sensors thus evaluated was compared with the results of conventional techniques. This comparison allows for selecting the best performing combination of sensor/mounting, i.e. long-gauge sensor with mounts bolted to threaded rods glued into the concrete for use in future work in a field test where a limited time window was available for installation, testing and post-test demounting. © 2012 Elsevier B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

To compare the efficacy and cost effectiveness of a senna-fibre combination and lactulose in treating constipation in long stay elderly patients.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A replicated field plot experiment was carried out in Northern Ireland in 1996 with flax, cv Ariane, and linseed, cv Flanders, each grown at seed rates of 500, 1000 and 1500 seeds/m(2), in which a comparison was made between netting of the standing crop, following desiccation by the trimesium salt of glyphosate (Touchdown, Zeneca Ltd.), and water or dew retting of the pulled crop. Application at 4 litres/ha on 9 August, 33 days after the mid-point of flowering (MPF), achieved both desiccation and partial retting of the crop within 14 days. Over 16 % clean long fibre was extracted by scutching the stand-netted flax straw, yielding 800 kg/ha fibre, while water retting achieved 20 extraction and 980 kg/ha yield and dew netting 8.5 % and 420 kg/ha respectively. The dew retting was uneven, resulting in high losses during fibre extraction, while water retting for 7 days at 25 degreesC did not achieve complete retting resulting in a high content of woody fragments in the fibre. Fibre yields increased by almost 50 % with the high v. low seed rate. Linseed was less well retted than flax and contained higher levels of impurity in the extracted long fibre which, after retting, yielded 120 to 310 kg/ha at extraction rates of 2.9 % to 7.5 %.

In a second experiment in 1998 flax cvs. Viola and Evelyn were treated with the timesium salt of glyphosate at rates of 2, 4 or 6 litres/ha 10, 20, 30 or 40 days after MPF on 5 July. Viola desiccated satisfactorily at all spray dates with 4 and 6 litres/ha glyphosate. The 20-day treatment desiccated more slowly than the 30-day and the 2 litres/ha rate did not achieve complete desiccation, but the trimesium salt of glyphosate achieved better desiccation at this timing than that found in earlier studies with the original form of glyphosate. Evelyn desiccated more slowly and less evenly than Viola particularly at the 20-day and 40-day timings. Spraying at MPF + 10 days interrupted early development of the seed and fibre significantly reducing yields. Due to slower desiccation the 20-day timing was no better than the 30-day, which was well retted by harvest 44 days after spraying, and gave the highest yield of clean long fibre. The spraying 40 days after MPF was considered too late in the season to be of practical use. It was concluded that retting of standing flax following desiccation with the trimesium salt of glyphosate was more effective than with the earlier formulation and that resting of the standing crop could achieve equivalent or better retting with similar fibre yields to traditional retting methods. The optimum spray timing was found to be about 30 days after MPF with 4 or 6 litres/ha, the lower rate being adequate for glyphosate responsive varieties such as Viola.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A fiber-optic multichannel correlator/convolver based on a two-dimensional systolic array architecture is described. Experimental verification of processor performance is presented.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The behaviour of Basalt Fibre Reinforced Polymer (BFRP) loaded perpendicular to glulam timber elements was investigated. It was found that pull-out load increased approximately linearly with the bonded length up to maximum which occurred at a bonded length of 250 mm (~15 times the hole diameter) and did not increase beyond this bonded length. Failure mode of the samples was mostly shear fracture which was located at the cylindrical zone at the timber/adhesive interface. Increased bonded lengths resulted in corresponding decrease in interfacial bond stress. At 250 mm bonded length, the pull-out capacity of the proposed design model was about 2% lower than that of the tests. The results also showed that the bond stress of the theoretical model (at the ascending and descending branches) of the stress–slip curve was approximately 5–10% of that of the experiment.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Multiscale micro-mechanics theory is extensively used for the prediction of the material response and damage analysis of unidirectional lamina using a representative volume element (RVE). Th is paper presents a RVE-based approach to characterize the materi al response of a multi-fibre cross-ply laminate considering the effect of matrix damage and fibre-matrix interfacial strength. The framework of the homogenization theory for periodic media has been used for the analysis of a 'multi-fibre multi-layer representative volume element' (M2 RVE) representing cross-ply laminate. The non-homogeneous stress-strain fields within the M2RVE are related to the average stresses and strains by using Gauss theorem and the Hill-Mandal strain energy equivalence principle. The interfacial bonding strength affects the in-plane shear stress-strain response significantl y. The material response predicted by M2 RVE is in good agreement with the experimental results available in the literature. The maximum difference between the shear stress predicted using M2 RVE and the experimental results is ~15% for the bonding strength of 30MPa at the strain value of 1.1%

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The results of a combined experimental and numerical study of hat-stiffened co-cured carbon-fibre composite panels loaded in uniaxial compression are presented. All panels consisted of two integrated stiffeners separated by an eight-ply thick skin bay of lay-up [*45/0190], . The effects of a 100 mm circular cutout in the skin was also investigated. The ultimate strength of all panels was governed by the load carrying capacity of the stiffeners. A change in the skin's buckling mode-shape was also observed for all panels loaded deep in the postbuckling region. The strains induced at the interior free-edge were not found to be critical. Non-linear finite element results correlated well with the prebuckling and initial postbuckling strain and displacements results obtained by experiment.