190 resultados para Self-consolidating concrete (SCC) , compressive membrane action, basalt fibre reinforced polymer
Resumo:
Self-compacting concrete (SCC) flows into place and around obstructions under its own weight to fill the formwork completely and self-compact without any segregation and blocking. Elimination of the need for compaction leads to better quality concrete and substantial improvement of working conditions. This investigation aimed to show possible applicability of genetic programming (GP) to model and formulate the fresh and hardened properties of self-compacting concrete (SCC) containing pulverised fuel ash (PFA) based on experimental data. Twenty-six mixes were made with 0.38 to 0.72 water-to-binder ratio (W/B), 183–317 kg/m3 of cement content, 29–261 kg/m3 of PFA, and 0 to 1% of superplasticizer, by mass of powder. Parameters of SCC mixes modelled by genetic programming were the slump flow, JRing combined to the Orimet, JRing combined to cone, and the compressive strength at 7, 28 and 90 days. GP is constructed of training and testing data using the experimental results obtained in this study. The results of genetic programming models are compared with experimental results and are found to be quite accurate. GP has showed a strong potential as a feasible tool for modelling the fresh properties and the compressive strength of SCC containing PFA and produced analytical prediction of these properties as a function as the mix ingredients. Results showed that the GP model thus developed is not only capable of accurately predicting the slump flow, JRing combined to the Orimet, JRing combined to cone, and the compressive strength used in the training process, but it can also effectively predict the above properties for new mixes designed within the practical range with the variation of mix ingredients.
Resumo:
The use of self-compacting concrete (SCC) facilitates the placing of concrete by eliminating the need for compaction by vibration. Given the highly flowable nature of such concrete, care is required to ensure excellent filling ability and adequate stability. This is especially important in deep structural members and wall elements where concrete can block the flow, segregate and exhibit bleeding and settlement which can result in local defects that can reduce mechanical properties, durability and quality of surface finish. This paper shows results of an investigation of fresh properties of self-compacting concrete, such as filling ability measured by slump flow and flow time (measured by Orimet) and plastic fresh settlement measured in a column. The SCC mixes incorporated various combinations of fine inorganic powders and admixtures. The slump flow of all SCCs was greater than 580 mm and the time in which the slumping concrete reached 500 rnm was less than 3 s. The flow time was less than 5 s. The results on SCCs were compared to a control mix. The compressive strength and splitting tensile strength of SCCs were also measured. The effects of water/powder ratio, slump and nature of the sand on the fresh settlement were also evaluated. The volume of coarse aggregate and the dosage of superphsticizer were kept constant. It can be concluded that the settlement of fresh self-compacting concrete increased with the increase in water/powder ratio and slump. The nature of sand influenced the maximum settlement.
Resumo:
This paper reports a study carried out to assess the impact of the use of self-compacting concrete (SCC) on bond and interfacial properties around steel reinforcement in practical concrete element. The pull-out tests were carried out to determine bond strength between reinforcing steel bar and concrete, and the depth-sensing nano-indentation technique was used to evaluate the elastic modulus and micro-strength of the interracial transition zone (ITZ) around steel reinforcement. The bond and interracial properties around deformed steel bars in different SCC mixes with strength grades of 35 MPa and 60 MPa (C35, C60) were examined together with those in conventional vibrated reference concrete with the same strength grades. The results showed that the maximum bond strength decreased when the diameter of the steel bar increased from 12 to 20 mm. The normalised bond strengths of the SCC mixes were found to be about 10-40% higher than those of the reference mixes for both bar diameters (12 and 20 mm). The study of the interfacial properties revealed that the elastic modulus and the micro-strength of the ITZ were lower on the bottom side of a horizontal steel bar than on the top side, particularly for the vibrated reference concrete. The difference of ITZ properties between top and bottom side of the horizontal steel bar appeared to be less pronounced for the SCC mixes than for the corresponding reference mixes.
Resumo:
Ettringite and thaumasite can be found among the deterioration products of cementitious materials exposed to sulfate and hydrochloric attack. The results of a test program to investigate the acid resistance of self-compacting concrete (SCC) and conventional concrete (CC), immersed up to 18 weeks at 20°C in sulfuric and hydrochloric acid solutions, are described. The SCC was prepared with 47% carboniferous limestone powder, as a replacement for cement, and an ordinary portland cement. The CC was prepared with portland cement only. The water-binder ratios of the SCC and CC were 0.36 and 0.46, respectively. The parameter investigated was the time, in weeks, taken to cause 10% mass loss of fully immersed concrete specimens in a 1% solution of sulfuric acid and the same amount of loss in a 1% solution of hydrochloric acid. The investigation indicated that the SCC performed better than the CC in sulfuric solution but was slightly more vulnerable to hydrochloric acid attack compared to CC. The mode of attack between the two solutions was different.
Resumo:
Improvements in the structural performance of glulam timber beams by the inclusion of reinforcing materials can increase both the service performance and ultimate capacity. This paper describes a series of four-point bending tests conducted, under service loads and to failure, on unreinforced, reinforced and post-tensioned glulam timber beams, where the reinforcing tendon used is 12 mm dia. basalt fibre-reinforced polymer. The research is designed to evaluate the benefits offered by including an active reinforcement in contrast to the passive reinforcement typically used within timber strengthening works, in addition to establishing the effect that bonding the reinforcing tendon has on the material's performance. Further experimental tests have also been developed to investigate the long-term implications of this research, with emphasis placed upon creep and loss of post-tensioning; however, this is ongoing and is not presented in this paper. The laboratory investigations establish that the flexural strength and stiffness increase for both the unbonded and bonded post-tensioned timbers compared to the unreinforced and reinforced beams. Timber that is post-tensioned with an unbonded basalt fibre-reinforced polymer tendon shows a flexural strength increase of 2ṡ8% and an increase in stiffness of 8ṡ7%. Post-tensioned beams with a bonded basalt fibre-reinforced polymer tendon show increases in flexural strength and stiffness of 15ṡ4% and 11ṡ5% respectively.
Resumo:
Concrete cover separation is a common failure mode of reinforced concrete (RC) beams strengthened with a fibre-reinforced polymer (FRP) plate bonded to the tension face (FRP-plated RC beams). Plate-end FRP U-jackets have previously been explored as a mitigation measure to delay or suppress concrete cover separation, although its effectiveness needs further clarification. The paper presents the first systemic experimental study on the use of FRP U-jackets of different forms for mitigating the concrete cover separation failure. A total of ten full-scale FRP-plated RC beams were tested. The test results show that both the ultimate load and the ductility of the beams were enhanced by the U-jackets. Among the forms of U-jackets explored, those inclined at 45o are the most effective.
Resumo:
Improvements in the structural performance of glulam timber beams by the inclusion of reinforcing materials can increase both the service performance and ultimate capacity. In recent years research focusing on the addition of fibre reinforced polymers (FRP) to strengthen members has yielded positive results. However, the FRP material is still relatively expensive and its full potential in combination with structural timber has not been realised. This paper describes a series of four-point bending tests that were conducted, under service loads and to failure, on unreinforced, reinforced and post-tensioned glulam timber beams, where the reinforcing tendon used was 12mm diameter basalt fibre reinforced polymer (BFRP). The research was designed to evaluate the benefits offered by including an active reinforcement in contrast to the passive reinforcement typically used within timber strengthening works, in addition to establishing the affect that bonding the reinforcing tendon has on the material’s performance. Further experimental tests have been developed to investigate the long-term implications of this research, with emphasis placed upon creep and loss of post-tensioning.
The laboratory investigations established that the flexural strength and stiffness increased for both the unbonded and bonded post-tensioned timbers compared to the unreinforced beams. Timber that was post-tensioned with an unbonded BFRP tendon showed a flexural strength increase of 2.8% and an increase in stiffness of 8.7%. Post-tensioned beams with a bonded BFRP tendon showed increases in flexural strength and stiffness of 16.6% and 11.5% respectively.
Resumo:
In this study, fibre optic sensors (FOS) were used to investigate the interfacial stress-strain behaviour of bonded-in basalt fibre reinforced polymer (BFRP) rods loaded into glulam members. Pull-out tests were conducted to examine the effect of bonded length and load-to-grain direction on the distribution of stress at the BFRP rod/adhesive zone. It was observed that the stress concentration at the loaded end of the BFRP rod of the samples was significantly the highest while the unloaded end showed the lowest. Increasing the bonded length at the same loading configuration resulted in a decrease in stress concentration at the loaded end. The stress concentration at the loaded end of the perpendicular to the grain samples was relatively higher than that of the corresponding parallel to the grain samples.
Resumo:
Slurries with high penetrability for production of Self-consolidating Slurry Infiltrated Fiber Concrete (SIFCON) were investigated in this study. Factorial experimental design was adopted in this investigation to assess the combined effects of five independent variables on mini-slump test, plate cohesion meter, induced bleeding test, J-fiber penetration test and compressive strength at 7 and 28 days. The independent variables investigated were the proportions of limestone powder (LSP) and sand, the dosages of superplasticiser (SP) and viscosity agent (VA), and water-to-binder ratio (w/b). A two-level fractional factorial statistical method was used to model the influence of key parameters on properties affecting the behaviour of fresh cement slurry and compressive strength. The models are valid for mixes with 10 to 50% LSP as replacement of cement, 0.02 to 0.06% VA by mass of cement, 0.6 to 1.2% SP and 50 to 150% sand (% mass of binder) and 0.42 to 0.48 w/b. The influences of LSP, SP, VA, sand and W/B were characterised and analysed using polynomial regression which identifies the primary factors and their interactions on the measured properties. Mathematical polynomials were developed for mini-slump, plate cohesion meter, J-fiber penetration test, induced bleeding and compressive strength as functions of LSP, SP, VA, sand and w/b. The estimated results of mini-slump, induced bleeding test and compressive strength from the derived models are compared with results obtained from previously proposed models that were developed for cement paste. The proposed response models of the self-consolidating SIFCON offer useful information regarding the mix optimization to secure a highly penetration of slurry with low compressive strength
Resumo:
The corrosion of reinforcement in bridge deck slabs has been the cause of major deterioration and high costs in repair and maintenance.This problem could be overcome by reducing the amount of reinforcement and/or altering the location.This is possible because, in addition to the strength provided by the reinforcement, bridge deck slabs have an inherent strength due to the in-plane arching forces set up as a result of restraint provided by the slab boundary conditions. This is known as arching action or Compressive Membrane Action (CMA). It has been recognised for some time that laterally restrained slabs exhibit strengths far in excess of those predicted by most design codes but the phenomenon has not been recognised by the majority of bridge design engineers. This paper presents the results of laboratory tests on fifteen reinforced concrete slab strips typical of a bridge deck slab and compares them to predicted strengths using the current codes and CMA theory. The tests showed that the strength of laterally restrained slabs is sensitive to both the degree of external lateral restraint and the concrete compressive strength.The tests particularly highlighted the benefits in strength obtained from very high strength concrete slabs. The theory extends the existing knowledge of CMA in slabs with concrete compressive strengths up to 100 N/mm[2] and promotes more economical and durable bridge deck construction by utilising the benefits of high strength concrete.