32 resultados para Hot-water heating
Resumo:
This study was carried out to assess the properties of vermiculites from Tanzania with respect to the temperature used to expand them. Vermiculites from five locations in the Mozambique Belt of Tanzania were sampled and heated at 15, 200, 400, 600 and 800 °C in a muffle furnace. Palabora Europe Ltd provided one sample for comparison from their South Africa deposit which provides vermiculite used worldwide as a soil amendment. Water release characteristic, cation exchange capacity, pH, mass loss, and bulk density were among the properties assessed. All six vermiculites responded differently on heating, and had a significant variation in their agronomic properties. Water release characteristic varied with the degree of exfoliation and phase composition. Although vermiculites from Tanzania expanded on heating, their capacity to retain plant available water was relatively low as compared to vermiculite from Palabora. Disintegration on heating and the presence of a high amount of iron could be among the factors affecting their water release characteristic. Loss of hydroxyl water was higher in vermiculites than in hydrobiotites. Dehydroxylation enhanced the availability of exchangeable K+ and reduced significantly the cation exchange capacity of vermiculites. The optimum exchangeable K+ was obtained on heating at a temperature of 600 °C. The pH was unaffected by heating to a temperature of less than 600 °C. At higher temperature, the pH increased in some samples and was accompanied by substantial amounts of exchangeable Mg2+. Thus, it was concluded that initial characterization of vermiculites is essential prior to potential agricultural applications in order to optimize their agronomic potential. © 2008 Elsevier B.V. All rights reserved.
Resumo:
Objectives: Amorphous drug forms provide a useful method of enhancing the dissolution performance of poorly water-soluble drugs; however, they are inherently unstable. In this article, we have used Flory–Huggins theory to predict drug solubility and miscibility in polymer candidates, and used this information to compare spray drying and melt extrusion as processes to manufacture solid dispersions.
Method: Solid dispersions were characterised using a combination of thermal (thermogravimetric analysis and differential scanning calorimetry) and spectroscopic (Fourier transform infrared spectroscopy (FTIR) and X-ray diffraction methods.
Key Findings: Spray drying permitted generation of amorphous solid dispersions to be produced across a wider drug concentration than melt extrusion. Melt extrusion provided sufficient energy for more intimate mixing to be achieved between drug and polymer, which may improve physical stability. It was also confirmed that stronger drug–polymer interactions might be generated through melt extrusion. Remixing and dissolution of recrystallised felodipine into the polymeric matrices did occur during the modulated differential scanning calorimetry analysis, but the complementary information provided from FTIR confirms that all freshly prepared spray-dried samples were amorphous with the existence of amorphous drug domains within high drug-loaded samples.
Conclusion: Using temperature–composition phase diagrams to probe the relevance of temperature and drug composition in specific polymer candidates facilitates polymer screening for the purpose of formulating solid dispersions.