Resumo:
For the first time, the coupling of fast transient kinetic switching and the use of an isotopically labelled reactant (15NO) has allowed detailed analysis of the evolution of all the products and reactants involved in the regeneration of a NOx storage reduction (NSR) material. Using realistic regeneration times (ca. 1 s) for Pt, Rh and Pt/Rh-containing Ba/Al2O3 catalysts we have revealed an unexpected double peak in the evolution of nitrogen. The first peak occurred immediately on switching from lean to rich conditions, while the second peak started at the point at which the gases switched from rich to lean. The first evolution of nitrogen occurs as a result of the fast reaction between H2 and/or CO and NO on reduced Rh and/or Pt sites. The second N2 peak which occurs upon removal of the rich phase can be explained by reaction of stored ammonia with stored NOx, gas phase NOx or O2. The ammonia can be formed either by hydrolysis of isocyanates or by direct reaction of NO and H2.
The study highlights the importance of the relative rates of regeneration and storage in determining the overall performance of the catalysts. The performance of the monometallic 1.1%Rh/Ba/Al2O3 catalyst at 250 and 350 °C was found to be dependent on the rate of NOx storage, since the rate of regeneration was sufficient to remove the NOx stored in the lean phase. In contrast, for the monometallic 1.6%Pt/Ba/Al2O3 catalyst at 250 °C, the rate of regeneration was the determining factor with the result that the amount of NOx stored on the catalyst deteriorated from cycle to cycle until the amount of NOx stored in the lean phase matched the NOx reduced in the rich phase. On the basis of the ratio of exposed metal surface atoms to total Ba content, the monometallic 1.6%Pt/Ba/Al2O3 catalyst outperformed the Rh-containing catalysts at 250 and 350 °C even when CO was used as a reductant.
Resumo:
Dissociative adsorption is one of the most important reactions in catalysis. In this communication we propose a model aiming to generalize the important factors that affect dissociation reactions. Specifically, for a dissociation reaction, say AB -->A + B, the model connects the dissociation barrier with the association barrier, the chemisorption energies of A and B at the final state and the bonding energy of AB in the gas phase. To apply this model, we have calculated CO dissociation on Ru(0001), Rh(111), Pd(111) (4d transition metals), Os(0001), Ir(111), and Pt(111) (5d transition metals) using density function theory (DFT). All the barriers are determined. We find that the DFT results can be rationalized within the model. The model can also be used to explain many experimental observations. (C) 2001 American Institute of Physics.
Resumo:
This paper discusses a number of checks that should be carried out to ensure that the kinetic and spectroscopic measurements made using a DRIFTS cell are meaningful. The observations reported here demonstrate how an appropriately modified commercial DRIFTS cell can provide pertinent kinetic information about both gaseous products and the related surface intermediates. The oxidation of CO with 02 was used as a test to assess the catalyst bed bypass by the reaction mixture. Full CO conversion was obtained after the light-off temperature in the case of the modified cell, contrary to the case of the original cell, for which 80% of the reaction mixture bypassed the catalyst bed. The water-gas shift reaction over a Pt/CeO2 catalyst was used as a model reaction to further characterize the behavior of the cell under reaction conditions. The catalyst bed was shown not to be a dead-zone and was purged in essentially the same time as that needed to purge the cell. The reaction chamber globally operated in a quasi plug-flow mode and the gas composition in the thin catalyst bed appears to be homogeneous when operated under differential conditions. The production of the gas-phase reaction product CO2 could be simultaneously followed both by mass spectrometry and DRIFTS, both techniques leading to identical results. Various IR bands integration methods were discussed to allow a precise and accurate determination of the surface concentration of adsorbates during isotopic exchange. (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
Supported ionic liquid membranes (SILMs) has the potential to be a new technological platform for gas/organic vapour separation because of the unique non-volatile nature and discriminating gas dissolution properties of room temperature ionic liquids (ILs). This work starts with an examination of gas dissolution and transport properties in bulk imidazulium cation based ionic liquids [Cnmim][NTf2] (n = 2.4, 6, 8.10) from simple gas H2, N2, to polar CO2, and C2H6, leading to a further analysis of how gas dissolution and diffusion are influenced by molecular specific gas-SILMs interactions, reflected by differences in gas dissolution enthalpy and entropy. These effects were elucidated again during gas permeation studies by examining how changes in these properties and molecular specific interactions work together to cause deviations from conventional solution–diffusion theory and their impact on some remarkably contrasting gas perm-selectivity performance. The experimental perm-selectivity for all tested gases showed varied and contrasting deviation from the solution–diffusion, depending on specific gas-IL combinations. It transpires permeation for simpler non-polar gases (H2, N2) is diffusion controlled, but strong molecular specific gas-ILs interactions led to a different permeation and selectivity performance for C2H6 and CO2. With exothermic dissolution enthalpy and large order disruptive entropy, C2H6 displayed the fastest permeation rate at increased gas phase pressure in spite of its smallest diffusivity among the tested gases. The C2H6 gas molecules “peg” on the side alkyl chain on the imidazulium cation at low concentration, and are well dispersed in the ionic liquids phase at high concentration. On the other hand strong CO2-ILs affinity resulted in a more prolonged “residence time” for the gas molecule, typified by reversed CO2/N2 selectivity and slowest CO2 transport despite CO2 possess the highest solubility and comparable diffusivity in the ionic liquids. The unique transport and dissolution behaviour of CO2 are further exploited by examining the residing state of CO2 molecules in the ionic liquid phase, which leads to a hypothesis of a condensing and holding capacity of ILs towards CO2, which provide an explanation to slower CO2 transport through the SILMs. The pressure related exponential increase in permeations rate is also analysed which suggests a typical concentration dependent diffusion rate at high gas concentration under increased gas feed pressure. Finally the strong influence of discriminating and molecular specific gas-ILs interactions on gas perm-selectivity performance points to future specific design of ionic liquids for targeted gas separations.
Resumo:
We report the combined studies of density functional theory (DFT) calculations and electrochemical in situ FTIR spectroscopy on surface oxidants and mechanisms of CO oxidation at the Ru(0001) electrodes. It is shown that CO can co-adsorb with both O and OH species at lower potential region where a low coverage of the (2 x 2)-O/OH adlayer formed; the oxidation of CO adsorbates takes place at higher potentials where a high coverage of the (1 x 1)-O/OH adlayer formed. Surface O species are not the active oxidants under all coverages studied, due to the high reaction barriers between CO and O (>1 eV). However, surface OH species with higher coverage are identified as the active oxidants, and CO oxidation takes place via a two-steps' mechanism of CO + 3OH -> COOH + 2OH -> CO2 + H2O + OH, in which three nearby OH species are involved in the CO2 formation: CO reacts with OH, forming COOH; COOH then transfers the H to a nearby OH to form H2O and CO2, at the same time, another H in the H2O transfers to a nearby OH to form a weak adsorbed H2O and a new OH. The reaction barrier of these processes is reduced significantly to around 0.50 eV. These new results not only provide an insight into surface active oxidants on Ru, which is directly relevant to fuel cell catalysis, but also reveals the extra complexity of catalytic reactions taking place at solid/liquid electrochemical interface in comparison to the relatively simpler ones at solid/gas phase.
Resumo:
On-stream deactivation during a water gas shift (WGS) reaction over gold supported on a ceria-zirconia catalyst was examined. Although the fresh catalyst has very high low temperature (<200 degrees C) for WGS activity, a significant loss of CO conversion is found under steady-state operations over hours. This has been shown to be directly related to the concentration of water in the gas phase. The same catalyst also undergoes thermal deactivation above 250 degrees C, and using a combined experimental and theoretical approach, a common deactivation mechanism is proposed. In both cases, the gold nanoparticles, which are found under reaction conditions, are thought to detach from the oxide support either through hydrolysis, <200 degrees C, or thermally, > 200 degrees C. This process reduces the metal-support interaction, which is considered to be critical in determining the high activity of the catalyst.
Resumo:
The H-2-assisted hydrocarbon selective catalytic reduction (HC-SCR) of NO, was investigated using fast transient kinetic analysis coupled with isotopically labelled (NO)-N-15. This allowed monitoring of the evolution of products and reactants during switches of H-2 in and out of the SCR reaction mix. The results obtained with a time resolution of less than 1 s showed that the effect on the reaction of the removal or addition of H-2 was essentially instantaneous. This is consistent with the view that H-2 has a direct chemical effect on the reaction mechanism rather than a secondary one through the formation of "active" Ag clusters. The effect of H-2 partial pressure was investigated at 245 degrees C, it was found that increasing partial pressure of H-2 resulted in increasing conversion of NO and octane. It was also found that the addition of H-2 at 245 degrees C had different effects on the product distribution depending on its partial pressure. The change of the nitrogen balance over time during switches in and out of hydrogen showed that significant quantities of N-containing species were stored when hydrogen was introduced to the system. The positive nitrogen balance on removal of H-2 from the gas phase showed that these stored species continued to react after removal of hydrogen to form N-2. (c) 2006 Elsevier Inc. All rights reserved.
Resumo:
Oxidative dehydrogenation of ethane was performed under conventional microreactor and TAP reactor conditions over a Pt/Al2O3 catalyst between 100 and 600 degreesC. During TAP studies, no ethene was produced whereas under flow conditions small but significant ethene formation was observed. This is consistent with a mechanism involving the gas-phase production of ethene rather than via a surface reaction. In comparison, both hydrogen and methane formation were found under TAP conditions and the trends with temperature and surface oxide composition are interpreted in terms of successive dehydrogenation steps on the catalyst surface. It is further observed that periodic introduction of the reactants can minimize deactivation processes. (C) 2003 Elsevier Inc. All rights reserved.
Resumo:
The change in the Pt electronic structure following the adsorption of an a,ß-unsaturated aldehyde and ketone was followed by in situ HERFD-XANES in the liquid phase. The resulting shift in the Pt Fermi energy is in good agreement with the molecule adsorption energy trends calculated by DFT and provides insight into the reaction selectivity.
Resumo:
Methods to control the dispersion of gold in supported heterogeneous catalysts are very valuable due to the strong nanoparticle size dependence on their activity and selectivity towards many reactions. Additionally, the ability to disperse large, inactive gold nanoparticles to smaller nanoparticles provides an opportunity to reactivate, stabilise and increase the lifetime of gold catalysts making them more practical for industrial applications. Previously it has been demonstrated that the use of gas phase iodomethane (J. Am. Chem. Soc., 2009, 131, 6973; Angew. Chem., Int. Ed., 2011, 50, 8912) was able to re-disperse gold from >20 nm particles to dimers and trimers. In the current work, we show that this technique can be applied using less hazardous halohydrocarbons treatments, both in the gas phase and the liquid phase. The ability of these individual halohydrocarbons to re-disperse gold as well as the extent to which leaching occurs is assessed.
Resumo:
The performance of NOx storage and reduction over 1.5 wt% Pt/20 wt% KNO3/K2Ti8O17 and 1.5 wt% Pt/K2Ti8O17 catalysts has been investigated using combined fast transient kinetic switching and isotopically labelled (NO)-N-15 at 350 degrees C. The evolution of product N-2 has revealed two significant peaks during 60 s lean/1.3 s rich switches. It also found that the presence of CO2 in the feed affects the release of N-2 in the second peak. Regardless of the presence/absence of water in the feed, only one peak of N-2 was observed in the absence of CO2. Gas-phase NH3 was not observed in any of the experiments. However, in the presence of CO2 the results obtained from in situ DRIFTS-MS analysis showed that isocyanate species are formed and stored during the rich cycles, probably from the reaction between NOx and CO, in which CO was formed via the reverse water-gas shift reaction.
Resumo:
This paper reports the detailed description and validation of a fully automated, computer controlled analytical method to spatially probe the gas composition and thermal characteristics in packed bed systems. This method has been designed to limit the invasiveness of the probe, a characteristic assessed using CFD. The thermocouple is aligned with the sampling holes to enable simultaneous recording of the gas composition and temperature profiles. This analysis technique has been validated by studying CO oxidation over a 1% Pt/Al2O3 catalyst. The resultant profiles have been compared with a micro-kinetic model, to further assess the strength of the technique.
Resumo:
Mechanochemical preparation of Ag/Al2O3 catalysts used for the selective catalytic reduction of NOx using hydrocarbons has been shown to substantially increase the activity of the catalyst in comparison with Ag/Al2O3 prepared by wet impregnation. The effect of using different ball-milling experimental parameters on both the structure of the material as well as the catalyst activity has been investigated and the optimum conditions established. A phase transition from γ- to α-alumina was observed milling at high speeds which was found to result in lower catalyst activities. At lower milling speeds both fracturing and agglomeration of the alumina support can be observed depending on the grinding time. However, due to ball-milling, a general enhancement in the NOx reduction activity was observed for all catalysts compared with the conventionally prepared catalysts irrespective of the reductant used. Transient DRIFTS-MS experiments were performed to investigate the effect of H2 in the absence and presence of water on the SCR reaction over catalysts prepared by both ball milling and wet impregnation. In-situ DRIFTS-MS analysis revealed significant differences in both gas phase and surface species. Most notably, isocyanate species were formed significantly more quickly and at higher surface concentration in the case of the mechanochemically prepared catalyst.
Resumo:
This paper describes a novel doped titania immobilised thin film multi tubular photoreactor which has been developed for use with liquid, vapour or gas phase media. In designing photocatalytic reactors measuring active surface area of photocatalyst within the unit is one of the critical design parameters. This dictate greatly limits the applicability of any semi-conductor photocatalyst in industrial applications, as a large surface area equates to a powder catalyst. This demonstration of a thin film coating, doped with a rare earth element, novel photoreactor design produces a photocatalytic degradation of a model pollutant (methyl orange) which displayed a comparable degradation achieved with P25 TiO2. The use of lanthanide doping is reported here in the titania sol gel as it is thought to increase the electron hole separation therefore widening the potential useful wavelengths within the electromagnetic spectrum. Increasing doping from 0.5% to 1.0% increased photocatalytic degradation by ∼17% under visible irradiation. A linear relationship has been seen between increasing reactor volume and degradation which would not normally be observed in a typical suspended reactor system. © 2012 Elsevier B.V.
Resumo:
Dry reforming is a promising reaction to utilise the greenhouse gases CO2 and CH4. Nickel-based catalysts are the most popular catalysts for the reaction, and the coke formation on the catalysts is the main obstacle to the commercialisation of dry reforming. In this study, the whole reaction network of dry reformation on both flat and stepped nickel catalysts (Ni(111) and Ni(211)) as well as nickel carbide (flat: Ni3C(001); stepped: Ni3C(111)) is investigated using density functional theory calculations. The overall reaction energy profiles in the free energy landscape are obtained, and kinetic analyses are utilised to evaluate the activity of the four surfaces. By careful examination of our results, we find the following regarding the activity: (i) flat surfaces are more active than stepped surfaces for the dry reforming and (ii) metallic nickel catalysts are more active than those of nickel carbide, and therefore, the phase transformation from nickel to nickel carbide will reduce the activity. With respect to the coke formation, the following is found: (i) the coke formation probability can be measured by the rate ratio of CH oxidation pathway to C oxidation pathway (r(CH)/r(C)) and the barrier of CO dissociation, (ii) on Ni(111), the coke is unlikely to form, and (iii) the coke formations on the stepped surfaces of both nickel and nickel carbide can readily occur. A deactivation scheme, using which experimental results can be rationalised, is proposed.