28 resultados para Enamel Microhardness
Palaeobiology of an extinct Ice Age mammal: Stable isotope and cementum analysis of giant deer teeth
Resumo:
The extinct giant deer, Megaloceros giganteus, is among the largest and most famous of the cervids. Megaloceros remains have been uncovered across Europe and western Asia. but the highest concentrations come from Irish bogs and caves Although Megaloceros has enjoyed a great deal of attention over the centuries, paleobiological study has focused oil morphometric and distributional work until now. This paper presents quantitative data that have implications for understanding its sudden extirpation in western Europe during a period of global climate change approximately 10.600 C-14 years ago (ca 12,500 calendar years BP). We report here the first stable isotope analysis of giant deer teeth. which we combine with dental cementum accretion in order to document age, diet and life-history seasonality from birth until death Enamel delta C-13 and delta O-18 measured in the second and third molars from seven individual giant deer Suggest a grass and forbbased diet supplemented with browse in a deteriorating. possibly water-stressed, environment, and a season of birth around spring/early summer Cementurm data indicate that the ages of the specimens ranged from 6.5 to 14 years and that they possessed mature antlers by autumn, similar to extant cervids. In addition. the possibility for combining these two techniques in future mammalian paleoccological studies is considered. The data presented in this study imply that Megoloceros would have indeed been vulnerable to extirpation during the terminal Pleistocene in Ireland. and this information is relevant to understanding the broader pattern of its extinction.
Resumo:
Electroless nickel (EN) coatings are recognised for their hardness and wear resistance in automotive and aerospace industries. In this work, electroless Ni–P coatings were deposited on aluminium alloy substrate LM24 (Al–9 wt.% Si alloy) and the effect of post treatment on the wear resistance was studied. The post treatments included heat treatment and lapping with two different surface textures. Scanning electron microscopy (SEM), energy dispersive spectrometry (EDS), X-ray diffraction (XRD) and micro-abrasion tester were used to analyse morphology, structure and abrasive wear resistance of the coatings. Post heat treatment significantly improved the coating density and structure, giving rise to enhanced hardness and wear resistance. Microhardness of electroless Ni–P coatings with thickness of about 15 μm increased due to the formation of Ni3P after heat treatment.
Resumo:
Electroless plating of binary Ni-P, ternary Ni-Sn-P and Ni-W-P, and quaternary Ni-W-Sn-P alloy coatings was carried out in alkalicitrate baths. After the plating, several kinds of test were carried out to determine the improvement in the characteristics and properties due to the additional elements as well as to study the change in behaviour when heat treatment was applied to these coatings. The coatings were subjected to X-ray diffraction analysis where it was found that all the coatings were amorphous. Interesting surface morphology features were examined using scanning electron microscopy. Addition of a third element improved the hardness.
Resumo:
The relationship between microstructure and deformation and damage behaviour during dynamic compression in Ti-3Al-5Mo-5V alloy has been studied using several experimental techniques, including optical microscopy, scanning electron microscopy and microhardness measurements. It was found that the deformation behaviour during dynamic compression was closely related to deformation parameters. After dynamic deformation, the deformation shear band that formed in the titanium alloy had microhardness similar to that of the matrix. However, the microhardness of the white shear band was much higher than the matrix microhardness. The effects of deformation parameters, including deformation rate and deformation degree, on deformation localisation were investigated. Based on the results from the present work, the microstructure and deformation processing parameters can be optimised. In addition, treatment methods after dynamic compression were explored to restore alloy properties. Using post-deformation heat treatment, the microstructure and property inhomogeneity caused by shear bands could be largely removed.
Resumo:
Porous titanium samples were manufactured using the 3D printing and sintering method in order to determine the effects of final sintering temperature on morphology and mechanical properties. Cylindrical samples were printed and split into groups according to a final sintering temperature (FST). Irregular geometry samples were also printed and split into groups according to their FST. The cylindrical samples were used to determine part shrinkage, in compressive tests to provide stress-strain data, in microCT scans to provide internal morphology data and for optical microscopy to determine surface morphology. All of the samples were used in microhardness testing to establish the hardness. Below 1100 C FST, shrinkage was in the region of 20% but increased to approximately 30% by a FST of 1300 C. Porosity varied from a maximum of approximately 65% at the surface to the region of 30% internally. Between 97 and 99% of the internal porosity is interconnected. Average pore size varied between 24 µm at the surface and 19 µm internally. Sample hardness increased to in excess of 300 HV0.05 with increasing FST while samples with an FST of below 1250 C produced an elastic-brittle stress/strain curve and samples above this displayed elastic-plastic behaviour. Yield strength increased significantly through the range of sintering temperatures while the Young's modulus remained fairly consistent. © 2013 Elsevier B.V.
Resumo:
The 1950s excavations by Charles McBurney in the Haua Fteah, a large karstic cave on the coast of northeast Libya, revealed a deep sequence of human occupation. Most subsequent research on North African prehistory refers to his discoveries and interpretations, but the chronology of its archaeological and geological sequences has been based on very early age determinations. This paper reports on the initial results of a comprehensive multi-method dating program undertaken as part of new work at the site, involving radiocarbon dating of charcoal, land snails and marine shell, cryptotephra investigations, optically stimulated luminescence (OSL) dating of sediments, and electron spin resonance (ESR) dating of tooth enamel. The dating samples were collected from the newly exposed and cleaned faces of the upper 7.5m of the ~14.0m-deep McBurney trench, which contain six of the seven major cultural phases that he identified. Despite problems of sediment transport and reworking, using a Bayesian statistical model the new dating program establishes a robust framework for the five major lithostratigraphic units identified in the stratigraphic succession, and for the major cultural units. The age of two anatomically modern human mandibles found by McBurney in Layer XXXIII near the base of his Levalloiso-Mousterian phase can now be estimated to between 73 and 65ka (thousands of years ago) at the 95.4% confidence level, within Marine Isotope Stage (MIS) 4. McBurney's Layer XXV, associated with Upper Palaeolithic Dabban blade industries, has a clear stratigraphic relationship with Campanian Ignimbrite tephra. Microlithic Oranian technologies developed following the climax of the Last Glacial Maximum and the more microlithic Capsian in the Younger Dryas. Neolithic pottery and perhaps domestic livestock were used in the cave from the mid Holocene but there is no certain evidence for plant cultivation until the Graeco-Roman period. © 2013 Elsevier Ltd.
Resumo:
Titanium has good biocompatibility and so its alloys are used as implant materials, but they suffer from having poor wear resistance. This research aims to improve the wear resistance and the tensile strength of titanium alloys potentially for implant applications. Titanium alloys Ti–6Al–4V and Ti–6Al–7Nb were subjected to shotpeening process to study the wear and tensile behavior. An improvement in the wear resistance has been achieved due to surface hardening of these alloys by the process of shotpeening. Surface microhardness of shotpeened Ti–6Al–4V and Ti–6Al–7Nb alloys has increased by 113 and 58 HV(0.5), respectively. After shotpeening, ultimate tensile strength of Ti–6Al–4V increased from 1000 MPa to 1150 MPa, higher than improvement obtained for heat treated titanium specimens. The results confirm that shotpeening pre-treatment improved tensile and sliding wear behavior of Ti–6Al–4V and Ti–6Al–7Nb alloys. In addition, shotpeening increased surface roughness.
Resumo:
The electroless nickel composite (ENC) with various silicon carbide contents was deposited onto aluminium alloy (LM24) substrate. The wear behaviour and the microhardness of the composite coating samples were investigated and compared with particles free and aluminium substrate samples using micro-scale abrasion tester and microhardness tester respectively. The wear scar marks and wear volume were analysed by optical microscope. The wear tracks were further studied using scanning electron microscopy (SEM). The embedded particles were found to get pressed into the matrix which helps resisting further wearing process for composite samples. However, random orientation of microcuts and microfallow were seen for ENC sample but more uniform wearing was observed for EN sample. The composite coating with low content of SiC was worn minimum. Early penetration into the substrate was seen for samples with higher SiC content. Microhardness was improved after heat treatment for all the samples containing various SiC content. Under dry sliding condition, inclusion of particles in the matrix did not improve the wearing resistance performance in as-deposited state. The wearing worsened as the content of the particles increased generally. However, on heat treatment, the composite coatings exhibited improved wear resistance and the best result was obtained from the one with low particle contents.
Resumo:
With a significant growth in the use of titanium alloys in the aviation manufacturing industry, the key challenge of making high-quality holes in the aircraft assembly process needs to be addressed. In this work, case studies deploying traditional drilling and helical milling technologies are carried out to investigate the tool life and hole surface integrity for hole-making of titanium alloy. Results show that the helical milling process leads to much longer tool life, generally lower hole surface roughness, and higher hole subsurface microhardness. In addition, no plastically deformed layer or white layer has been observed in holes produced by helical milling. In contrast, a slightly softened region was always present on the drilled surface. The residual stress distributions within the hole surface, including compressive and tensile residual stress, have also been investigated in detail.
Resumo:
Electroless nickel composite coatings with silicon carbide, SiC, as reinforcing particles deposited with Ni–P onto aluminium alloy, LM24, having zincating as under layer were subjected to heat treatment using air furnace. The changes at the interface were investigated using scanning electron microscope (SEM) and energy dispersive X-ray (EDX) to probe the chemistry changes upon heat treatment. Microhardness tester with various loads using both Knoop and Vickers indenters was used to study the load effect clubbed with the influence of second phase particles on the coating at the vicinity of the interface. It was observed that zinc was absent at the interface after elevated temperature heat treatment at 400–500 °C. Precipitation of copper and nickel with a distinct demarcation (copper rich belt) along the coating interface was seen with irregular thickness of the order of 1 μm. Migration of copper from the bulk aluminium alloy could have been the factor. Brittleness of the coating was confirmed on heat treatment when indented with Vickers. However, in composite coating the propagation of the microcrack was stopped by the embedded particles but the microcracks continue in the matrix when not interrupted by second phase particles (SiC).
Resumo:
YAl2p/Mg-14Li-1Al composite was made by a stir-casting technique. The aging behavior of the composite was investigated using hardness test, differential scanning calorimetry, and X-ray diffraction. The results show that the microhardness variations of both the matrix alloy and its composite are related to the precipitation and decomposition of θ-MgLi2Al phase. The strengthening of the composite is from the addition of YAl2 particulates and the precipitation in matrix alloy. The former contribution is stable, but the latter is unstable and depends on the aging behavior. The addition of YAl2 particulates delays occurring of the aging behavior of composite.
Resumo:
Electroless nickel (EN) and electroless nickel composite (ENC) coatings were deposited on aluminium alloy substrate, LM24. The micro abrasion test was conducted to study the wear behaviour of the coatings with the effect of SiC concentration. Microhardness of the coatings was tested also. The wear scars were analysed using optical microscope and scanning electron microscope (SEM). The wear resistance was found to be improved in composite coating that has higher microhardness as compared to particles free and the bare aluminium substrate. In as-deposited condition for the composite coating, the wear volume increases on increase in SiC percentage in the coating but is found to be minimum for lower SiC percentage. The increase in hardness on heat treatment at 400°C is due to the hardening or grain coarsening with the formation Ni3P.
Resumo:
PURPOSE: This systematic review reports on the survival of feldspathic porcelain veneers.
MATERIALS AND METHODS: The Cochrane Library, MEDLINE (OVID), Embase, Web of Knowledge, selected journals, clinical trials registers, and conference proceedings were searched independently by two reviewers. Academic colleagues were also contacted to identify relevant research. Inclusion criteria were human cohort studies (prospective and retrospective) and controlled trials assessing outcomes of feldspathic porcelain veneers in more than 15 patients and with at least some of the veneers in situ for 5 years. Of 4,294 articles identified, 116 studies underwent full-text screenings and 69 were further reviewed for eligibility. Of these, 11 were included in the qualitative analysis and 6 (5 cohorts) were included in meta-analyses. Estimated cumulative survival and standard error for each study were assessed and used for meta-, sensitivity, and post hoc analyses. The I2 statistic and the Cochran Q test and its associated P value were used to evaluate statistical heterogeneity, with a random-effects meta-analysis used when the P value for heterogeneity was less than .1. Galbraith, forest, and funnel plots explored heterogeneity, publication patterns, and small study biases.
RESULTS: The estimated cumulative survival for feldspathic porcelain veneers was 95.7% (95% confidence interval [CI]: 92.9% to 98.4%) at 5 years and ranged from 64% to 95% at 10 years across three studies. A post hoc meta-analysis indicated that the 10-year best estimate may approach 95.6% (95% CI: 93.8% to 97.5%). High levels of statistical heterogeneity were found.
CONCLUSIONS: When bonded to enamel substrate, feldspathic porcelain veneers have a very high 10-year survival rate that may approach 95%. Clinical heterogeneity is associated with differences in reported survival rates. Use of clinically relevant survival definitions and careful reporting of tooth characteristics, censorship, clustering, and precise results in future research would improve metaanalytic estimates and aid treatment decisions.