40 resultados para Alkali activated systems


Relevância:

100.00% 100.00%

Publicador:

Resumo:

The development of alkali-activated binders with superior engineering properties and longer durability has emerged as an alternative to ordinary portland cement (OPC). It is possible to use alkali-activated natural pozzolans to prepare environmentally friendly geopolymer cement leading to the concept of sustainable development. This paper presents a summary of an experimental work that was conducted to determine mechanical strength, modulus of elasticity, ultrasonic pulse velocity, and shrinkage of different concrete mixtures prepared with alkali-activated Iranian natural pozzolans—namely Taftan andesite and Shahindej dacite, both with and without calcining. Test data were used for Taftan pozzolan to identify the effects of water-binder ratios (w/b) and curing conditions on the properties of the geopolymer concrete, whereas the influence of material composition was studied by activating Shahindej pozzolan both in the natural and calcined states. The results show that alkali-activated natural pozzolan (AANP) concretes develop moderate-to-high mechanical strength with a high modulus of elasticity and a shrinkage much lower than with OPC.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Natural pozzolans are raw materials from geological deposits with a range of chemical compositions that when combined with suitable alkali activators can be converted to geopolymer cement for concrete production. In this paper the concept of adding mineral additives to enhance the properties of geopolymer cement is introduced. Taftan andesite, a natural Iranian pozzolan, was used to study the effect of adding mineral additives such as kaolinite, lime and other calcined pozzolans on the compressive strength of geopolymer cement under both normal and autoclave curing. Scanning electron microscopy (SEM)/energy dispersive X-ray (EDX) was used to determine the composition of the gel phase in both alkali-activated Taftan pozzolan with and without mineral additions. The work has shown that deficiencies in SiO2, Al2O3 and CaO content in the raw natural pozzolan can be compensated for by adding mineral additives for enhanced properties.

Relevância:

100.00% 100.00%

Publicador:

Resumo:


Natural pozzolans can be activated and condensed with sodium silicate in an alkaline environment to synthesize high performance cementitious construction materials with low environmental impact. The nature of the starting materials including mineral composition, chemical composition and crystal structure groups affects the formation of the geopolymer gel phase. In this paper, the pozzolanic activities of five natural pozzolans are studied. From XRD and XRF results, most of the raw materials contain zeolite clay minerals and have a high loss on ignition. Therefore, before use, samples were calcined at 700, 800 and 900 °C, respectively. The improvement in pozzolanic properties was studied following heat treatment including calcinations and/or elevated curing temperature by using alkali solubility and compressive strength tests. The results show that pozzolan containing sodium zeolite clinoptilolite can be used to prepare a moderate to high strength binder by heat treatment and calcinations can impart disorder hornblende as a constituent of pozzolan with no amorphous phase to prepare a moderate strength binder.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

One of the important factors in the use of portland cement concrete is its durability, and most of the situations where durability is lacking have been identifi ed and strategies to manage durability have been implemented. Geopolymer concrete, made from an alkali-activated natural pozzolan (AANP), provides an important opportunity for the reduction of carbon dioxide (CO2) emissions associated with the manufacture of concrete but has a limited history of durability studies. Until its different properties are well understood there is no desire to adopt this new technology of unknown provenance by the concrete industry. This paper presents an experimental study of oxygen and chloride permeability of AANP concrete prepared by activating Taftan andesite and Shahindej dacite (Iranian natural pozzolans), with and without calcining, and the correlations between these properties and compressive strength. The results show that compared to ordinary portland cement (OPC) concrete, AANP concrete has lower oxygen permeability at later ages; but it shows moderate to high chloride ion penetrability.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In the near future, geopolymers or alkali-activated cementitious materials will be used as new high-performance construction materials of low environmental impact with a reasonable cost. This material is a good candidate to partially replace ordinary portland cement (OPC) in concrete as a major construction material that plays an outstanding role in the construction industry of different structures. Geopolymer materials are inorganic polymers based on alumina and silica units; they are synthesized from a wide range of dehydroxylated alumina-silicate powders condensed with alkaline silicate in a highly alkaline environment. Geopolymeric materials can be produced from a wide range of alumina-silica, including natural products--such as natural pozzolan and metakaolin--or coproducts--such as fly ash (coal and lignite), oil fuel ash, blast furnace or steel slag, and silica fume--and provide a route toward sustainable development. Using lesser amounts of calcium-based raw materials, lower manufacturing temperature, and lower amounts of fuel result in reduced carbon emissions for geopolymer cement manufacture up to 22 to 72% in comparison with portland cement. A study has been done by the authors to investigate the intrinsic nature of different types of Iranian natural pozzolans to determine the activators and methods that could be used to produce a geopolymer concrete based on alkali-activated natural pozzolan (AANP) and optimize mixture design. The mechanical behavior and durability of these types of geopolymer concrete were investigated and compared with normal OPC concrete mixtures cast by the authors and also reported in the literature. This paper summarizes the main conclusions of the research regarding pozzolanic activity, activator properties, engineering and durability properties, applications and evaluation of carbon footprint, and cost for AANP concrete.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The assessment of pozzolanic activity is essential for estimating the reaction of a material as pozzolan. Natural pozzolans can be activated and condensed with sodium silicate in an alkaline environment to synthesize high performance cementitious construction materials with low environmental impact. In this paper, the pozzolanic activities of five natural pozzolans are studied. The correlation between type and chemical composition of natural pozzolan, which affects the formation of the geopolymer gel phase, both for the calcined and untreated natural pozzolans, have been reviewed. The improvement in pozzolanic properties was studied following heat treatment including calcinations and/or elevated curing temperature by using alkali solubility, and compressive strength tests. A model was developed to allow prediction of the alkali-activated pozzolan strength versus their chemical compositions, alkali solubility, and crystallinity.


Relevância:

90.00% 90.00%

Publicador:

Resumo:

Interest in alkali-activated slag as a construction material is increasing, primarily due to its environmentally friendly nature. Although strong alkaline activators, such as sodium hydroxide and sodium silicate solution, are preferred for high strength, none of them exists naturally and their manufacturing process is quite energy intensive. Whilst sodium sulfate (NaSO ) can be obtained from natural resources, the early strength of NaSO activated slag is usually low. In this paper, the effects of slag fineness and NaSO dosage on strength, pH, hydration and microstructure were investigated and compared with those of a pure Portland cement (PC). Test results indicated that increasing the slag fineness is a more effective approach than increasing NaSO dosage for increasing both the early and long-term strength of NaSO activated slags. In addition, increasing the slag fineness can also increase the strength without increasing the pH of the hardened matrix, which is beneficial for immobilizing certain types of nuclear waste containing reactive metals and resins.© 2012 Elsevier Ltd. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Several factors affecting the reactivity of pulverised fuel ash (pfa) as a precursor for geopolymer concrete have been investigated. These include physical and chemical properties of various pfa sources, inclusion of ground granulated blast furnace slag (ggbs), chemical activator dosages and curing temperature. Alkali-activated pfa was found to require elevated curing temperatures and high alkali concentrations. A mixture of sodium hydroxide and sodium silicate was used and this was shown to result in high strengths, as high as 70 MPa at 28-days. The presence of silicates in solution was found to be a key factor. Detailed physical and chemical characterisation was carried out on thirteen pfa sources from the UK. The most important factor affecting the reactivity was found to be the particle size of pfa. The loss on ignition (LOI) and the amorphous content are also important parameters that need to be considered for the selection of pfa for use in geopolymer concrete. The partial replacement of pfa by ground granulated blast furnace slag (ggbs) was found to be beneficial in not only avoiding the need for elevated curing temperatures but also in improving compressive strengths. Microstructural characterisation with scanning electron microscope (SEM) coupled with energy dispersive X-ray spectroscopy (EDS) was performed on pfa/ggbs pastes. The reaction product of pfa and ggbs in these binary systems was calcium aluminium silicate hydrate gel (C-A-S-H) with inclusion of Na in the structure.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Worldwide, the building sector requires the production of 4 billion tonnes of cement annually, consuming more than 40% of global energy. Alkali activated “cementless” binders have recently emerged as a novel eco-friendly construction material with a promising potential to replace ordinary Portland cement. These binders consist of a class of inorganic polymer formed mainly by the reaction between an alkaline solution and an aluminosilicate source. Precursor materials for this reaction can be found in secondary material streams from different industrial sectors, from energy to agro-alimentary. However, the suitability of these materials in developing the polymerisation reaction must be assessed through a detailed chemical and physical characterisation, ensuring the availability of required chemical species in the appropriate quantity and physical state. Furthermore, the binder composition needs to be defined in terms of proper alkali activation dosages, water content in the mix, and curing conditions. The mix design must satisfy mechanical requirements and compliance to desired engineering properties (workability, setting time) for ensuring the suitability of the binder in replacing Portland cement in concrete applications. This paper offers a structured approach for the development of secondary material-based binders, from their identification to mix design and production procedure development. Essential features of precursor material can be determined through chemical and physical characterisation methods and advanced microscope techniques. Important mixing parameters and binder properties requirements are examined and some examples of developed binders are reported.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The building sector requires the worldwide production of 4 billion tonnes of cement annually, consuming more than 40% of global energy and accounting for about 8% of the total CO2 emissions. The SUS-CON project aimed at integrating waste materials in the production cycle of concrete, for both ready-mixed and pre-cast applications, resulting in an innovative light-weight, ecocompatible and cost-effective construction material, made by all-waste materials and characterized by enhanced thermal insulation performance and low embodied energy and CO2. Alkali activated “cementless” binders, which have recently emerged as eco-friendly construction materials, were used in conjunction with lightweight recycled aggregates to produce sustainable concrete for a range of applications. This paper presents some results from the development of a concrete made with a geopolymeric binder (alkali activated fly ash) and aggregate from recycled mixed plastic. Mix optimisation was achieved through an extensive investigation on production parameters for binder and aggregate. The mix recipe was developed for achieving the required fresh and hardened properties. The optimised mix gave compressive strength of about 7 MPa, flexural strength of about 1.3 MPa and a thermal conductivity of 0.34 W/mK. Fresh and hardened properties were deemed suitable for the industrial production of precast products. Precast panels were designed and produced for the construction of demonstration buildings. Mock-ups of about 2.5 x 2.5 x 2.5 m were built at a demo park in Spain both with SUS-CON and Portland cement concrete, monitoring internal and external temperatures. Field results indicate that the SUS-CON mock-ups have better insulation. During the warmest period of the day, the measured temperature in the SUS-CON mock-ups was lower.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The construction industry is one of the largest consumers of raw materials and energy and one of the highest contributor to green-houses gases emissions. In order to become more sustainable it needs to reduce the use of both raw materials and energy, thus lim-iting its environmental impact. Developing novel technologies to integrate secondary raw materials (i.e. lightweight recycled aggre-gates and alkali activated “cementless” binders - geopolymers) in the production cycle of concrete is an all-inclusive solution to im-prove both sustainability and cost-efficiency of construction industry. SUS-CON “SUStainable, Innovative and Energy-Efficiency CONcrete, based on the integration of all-waste materials” is an European project (duration 2012-2015), which aim was the inte-gration of secondary raw materials in the production cycle of concrete, thus resulting in innovative, sustainable and cost-effective building solutions. This paper presents the main outcomes related to the successful scaling-up of SUS-CON concrete solutions in traditional production plants. Two European industrial concrete producers have been involved, to design and produce both pre-cast components (blocks and panels) and ready-mixed concrete. Recycled polyurethane foams and mixed plastics were used as aggre-gates, PFA (Pulverized Fuel Ash, a by-product of coal fuelled power plants) and GGBS (Ground Granulated Blast furnace Slag, a by-product of iron and steel industries) as binders. Eventually, the installation of SUS-CON concrete solutions on real buildings has been demonstrated, with the construction of three mock-ups located in Europe (Spain, Turkey and Romania)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This study reports the formulation/characterisation of novel polymeric platforms designed to behave as low-viscosity systems in the nonaqueous state, however, following uptake of aqueous ?uids, exhibit rheological structuring and mucoadhesion. The rheological/mechanical and mucoadhesive properties of platforms containing poly(acrylic acid) (PAA, 1%, 3%, 5%, w/w) and poloxamines (Tetronic 904, 901, 704, 701, 304), both in the absence and presence of phosphate buffered saline (PBS, pH 7.4) are described. With the exception of Tetronic 904, all formulations exhibited Newtonian ?ow in the nonaqueous state, whereas, all aqueous formulations displayed pseudoplastic ?ow. The consistency and viscoelastic properties were dependent on the concentrations of PAA and PBS and Tetronic grade. PBS signi?cantly increased the consistency, viscoelasticity and mucoadhesion, reaching a maximum at a de?ned concentration of PBS that was dependent on PAA concentration and Tetronic grade. Formulations containing Tetronic 904 exhibited greatest consistency and elasticity both prior to and after dilution with PBS. Increasing PAA concentration enhanced the mucoadhesive properties. Prolonged drug release of metronidazole was observed from formulations containing 10% (w/w) PBS, 3% and, particularly, 5% (w/w) PAA. It is suggested that the physicochemical properties of formulations containing 3% or 5% (w/w) PAA and Tetronic 904, would render them suitable platforms for administration to body cavities.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The central theme of this investigation is to evaluate the feasibility of using bituminous coal as a precursor material for the production of chars and activated carbons using physical and chemical activation processes. The chemical activation process was accomplished by impregnating the raw materials with different dehydrating agents in different ratios and concentrations, prior to heat treatment (ZnCl2, KCl, KOH, NaOH and Fe2(SO4)3·xH2O). Steam activation of the precursor material was adopted for the preparation of activated carbon using physical activation technology. Different types of bituminous coal; namely, contaminated Columbian (contaminated with pet. coke), pure Columbian, Venezuelan and New Zealand bituminous coal were used in the production processes. BET surface area, micropore area, pore size distribution and total pore volume of the chars and activated carbons were determined from N2 adsorption/desorption isotherm, measured at 77 K. Charring conditions, charring temperature of 800 °C and charring time of 4 h, proved to be the optimum conditions for preparing chars. Contaminated Columbian were found to be the best precursor material for the production of char with reasonable physical characteristics (surface area = 138.1 m2 g-1 and total pore volume of 8.656 × 10-0.2 cm3 g-1). An improvement in the physical characteristics of the activated carbons was obtained upon the treatment of coal with dehydrating agents. Contaminated Columbian treated with 10 wt% ZnCl2 displayed the highest surface area and total pore volume (surface area = 231.5 m2 g-1 and total pore volume = 0.1227 cm3 g-1) with well-developed microporisity (micropore area = 92.3 m2 g-1). Venezuelan bituminous coal using the steam activation process was successful in producing activated carbon with superior physical characteristics (surface area = 863.50 m2 g-1, total pore volume = 0.469 cm3 g-1 and micropore surface area = 783.58 m2 g-1).