328 resultados para durability testing
Resumo:
With greater emphasis now being placed on the durability of concrete and the need for on-site characterization of concrete for durability, there is an increasing dependence on the measurement of the permeation properties of concrete. Such properties can be measured in the laboratory under controlled ambient conditions, namely, temperature and relative humidity, and comparisons made between samples not affected by testing conditions. An important factor that influences permeation measurements is the moisture state of the concrete prior to testing. Moisture gradients are known to exist in exposed concretes; therefore, all laboratory tests are generally carried out after preconditioning to a reference moisture state. This is reasonably easy to achieve in the laboratory, but more difficult to carry out on-site. Different methods of surface preconditioning in situ concrete are available; however, there is no general agreement on the suitability of any one method. Therefore, a comprehensive set of experiments was carried out with four different preconditioning methods. Results from these investigations indicated that only superficial drying could be achieved by using any of the preconditioning methods investigated and that significant moisture movement below a depth of 15 mm was not evident.
Resumo:
A range of seven test methods was used to assess the effectiveness of curing on C30 and C50 Portland cement concretes. Curing was by formwork retention, wrapping in wet hessian or wrapping in polythene for periods of between one and seven days. Specimens from each mix were also subjected to both air and water storage.
Resumo:
This paper investigates the influence of three fundamentally different durability enhancing products, viz. microsilica, controlled permeability formwork and silane, on some of the physical proper ties of near surface concrete. Microsilica (silica fume) is a pozzolan, controlled permeability formwork (CPF) is used to provide a free draining surface to a concrete form, while silane is a surface treatment applied to hardened concrete to reduce the ingress of water. Comparisons are made between the products when used individually and used in conjunction with each other, with a view to assessing whether the use of combinations of products may be desirable to improve the durability of concrete in certain circumstances. The effect of these materials on various durability parameters, such as freeze-thaw deterioration, carbonation resistance and chloride ingress, is considered in terms of their effect on permeation properties and surface strength. The results indicated that a combination of silane and CPF produces concrete with very low air permeability and sorptivity values. The influence of microsilica was more pronounced in increasing the surface strength of concrete.
Resumo:
It is widely accepted that concrete designed to perform satisfactorily in adverse environmental conditions must have a high cement content and a low water-cement ratio. In addition, in order to enhance its durability, many types of additive and admixture such as super-plasticizers, fly ash, silica fume, ggbfs, etc., have been used in the past. However, a close study of the published literature indicates that the effect of mix variables on the durability and the interaction between the various ingredients are not fully understood. Some of these apparent contradictions are due to the limitations in the design of the experimental programme. For instance, it is evident that relatively higher concentrations of aggregates increase the tortuosity of the flow path and hence reduce the permeability, which results in an improvement in the durability. Therefore, an increase in cement content without a proportional decrease in water-cement ratio may reduce the durability. In such cases, the interactive effects of factors can be established by resorting to a properly designed experimental programme, such as the factorial experimental design.