442 resultados para Pavements, Concrete.


Relevância:

30.00% 30.00%

Publicador:

Resumo:

The maintenance or even replacement of cracked pavements requires considerable financial resources and puts a large burden on the budgets of local councils. In addition to these costs, local councils also face liability claims arising from uneven or cracked pedestrian pavements. These currently cost the Manchester City Council and Preston City Council around £6 million a year each. Design procedures are empirical. A better understanding of the interaction between paving blocks, bedding sand and subbase was necessary in order to determine the mode of failure of pavements under load. Increasing applied stress was found to mobilise ‘‘rotational interlock’’, providing increased pavement stiffness and thus increased load dissipation resulting in lower transmitted stress on the subgrade. The indications from the literature
review were that pavements are designed to fail by excessive deformation and that paving blocks remained uncracked at failure. This was confirmed with experimental data which was obtained from tests on segments of pavements that were laid/constructed in a purpose built test frame in the laboratory.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of short and long term service load tests were undertaken on the sixth floor of the full-scale, seven storey, reinforced concrete building at the Large Building Test Facility of the Building Research Establishment at Cardington. By using internally strain gauged reinforcing bars cast into an internal and external floor bay during the construction process it was possible to gain a detailed record of slab strains resulting from the application of several arrangements of test loads. Short term tests were conducted in December 1998 and long term monitoring then ensued until April 2001. This paper describes the test programmes and presents results to indicate slab behaviour for the various loading regimes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The use of high-quality quarried crushed rock aggregates is generally required to comply with current specifications for unbound granular materials (UGMs) in pavements. The source of these high-quality materials can be a long distance from the site, resulting in high transportation costs. The use of more local sources of marginal materials or the use of secondary aggregates is not allowed if they do not fully comply with existing specifications. These materials can, however, be assessed for their suitability for use in a pavement by considering performance criteria such as resistance to permanent deformation and degradation instead of relying on compliance with inflexible specifications. The final thickness of the asphalt cover and the pavement depth are governed by conventional pavement design methods, which consider the number of vehicle passes, subgrade strength, and some material property, commonly the California bearing ratio or resilient modulus. A pavement design method that includes as a design criterion an assessment of the resistance to deformation of a UGM in a pavement structure at a particular stress state is proposed. The particular stress state at which the aggregate is to perform in an acceptable way is related to the in situ stress, that is, the stress that the aggregate is anticipated to experience at a particular depth in the pavement. Because the stresses are more severe closer to the pavement surface, the aggregates should be better able to resist these stresses the closer they are laid to the surface in the pavement. This method was applied to two Northern Ireland aggregates of different quality (NI Good and NI Poor). The results showed that the NI Poor aggregate performed at an acceptable level with respect to permanent deformation, provided that a minimum of 70 mm of asphalt cover was provided. It was predicted that the NI Good material would require 60 mm of asphalt cover.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The corrosion of reinforcement in bridge deck slabs has been the cause of major deterioration and high costs in repair and maintenance.This problem could be overcome by reducing the amount of reinforcement and/or altering the location.This is possible because, in addition to the strength provided by the reinforcement, bridge deck slabs have an inherent strength due to the in-plane arching forces set up as a result of restraint provided by the slab boundary conditions. This is known as arching action or Compressive Membrane Action (CMA). It has been recognised for some time that laterally restrained slabs exhibit strengths far in excess of those predicted by most design codes but the phenomenon has not been recognised by the majority of bridge design engineers. This paper presents the results of laboratory tests on fifteen reinforced concrete slab strips typical of a bridge deck slab and compares them to predicted strengths using the current codes and CMA theory. The tests showed that the strength of laterally restrained slabs is sensitive to both the degree of external lateral restraint and the concrete compressive strength.The tests particularly highlighted the benefits in strength obtained from very high strength concrete slabs. The theory extends the existing knowledge of CMA in slabs with concrete compressive strengths up to 100 N/mm[2] and promotes more economical and durable bridge deck construction by utilising the benefits of high strength concrete.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A full-scale, seven-story, reinforced concrete building frame was constructed in-place at the Building Research Establishment's Cardington Laboratory, which encompassed a range of different concrete mixtures and advanced construction techniques. This provided an opportunity to assess in-place nondestructive test methods, namely the pullout test, and more specifically the Danish version, which has been known as the Lok test, on a systematic basis during the construction of the building. It was used in conjunction with both standard and temperature-matched cube specimens to assess its practicality and accuracy under site conditions. Strength correlations were determined using linear and power function regression analysis. Strength predictions from these were found to be in very good agreement with the compressive strengths of temperature-matched cube specimens. When a general correlation is used, however, estimates for compressive strength are likely to have 95% confidence limits of around '20% of the mean value of four results.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The ingress of chlorides into concrete is predominantly by the mechanism of diffusion and the resistance of concrete to the transport of chlorides is generally represented by its coefficient of diffusion. The determination of this coefficient normally requires long test duration (many months). Therefore, rapid test methods based on the electrical migration of ions have widely been used. The current procedure of chloride ion migration tests involves placing a concrete disc between an ion source solution and a neutral solution and accelerating the transport of ions from the source solution to the neutral solution by the application of a potential difference across the concrete disc. This means that, in order to determine the chloride transport resistance of concrete cover, cores should be extracted from the structure and tested in laboratories. In an attempt to facilitate testing of the concrete cover on site, an in situ ion migration test (hereafter referred to as PERMIT ion migration test for the unique identification of the new test) was developed. The PERMIT ion migration test was validated in the lab by carrying out a comparative investigation and correlating the results with the migration coefficient from the one-dimensional chloride migration test, the effective diffusion coefficient from the normal diffusion test and the apparent diffusion coefficient determined from chloride profiles. A range of concrete mixes made with ordinary Portland cement was used for this purpose. In addition, the effects of preferential flow of ions close to the concrete surface and the proximity of reinforcement within the test area on the in situ migration coefficients were investigated. It was observed that the in situ migration index, found in one working day, correlated well with the chloride diffusion coefficients from other tests. The quality of the surface layer of the cover concrete and the location of the reinforcement within the test area were found to affect the flow of ions through the concrete during the test. Based on the data, a procedure to carry out the PERMIT ion migration test was standardised.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Self-compacting concrete (SCC) is generally designed with a relatively higher content of finer, which includes cement, and dosage of superplasticizer than the conventional concrete. The design of the current SCC leads to high compressive strength, which is already used in special applications, where the high cost of materials can be tolerated. Using SCC, which eliminates the need for vibration, leads to increased speed of casting and thus reduces labour requirement, energy consumption, construction time, and cost of equipment. In order to obtain and gain maximum benefit from SCC it has to be used for wider applications. The cost of materials will be decreased by reducing the cement content and using a minimum amount of admixtures. This paper reviews statistical models obtained from a factorial design which was carried out to determine the influence of four key parameters on filling ability, passing ability, segregation and compressive strength. These parameters are important for the successful development of medium strength self-compacting concrete (MS-SCC). The parameters considered in the study were the contents of cement and pulverised fuel ash (PFA), water-to-powder ratio (W/P), and dosage of superplasticizer (SP). The responses of the derived statistical models are slump flow, fluidity loss, rheological parameters, Orimet time, V-funnel time, L-box, JRing combined to Orimet, JRing combined to cone, fresh segregation, and compressive strength at 7, 28 and 90 days. The models are valid for mixes made with 0.38 to 0.72 W/P ratio, 60 to 216 kg/m3 of cement content, 183 to 317 kg/m3 of PFA and 0 to 1% of SP, by mass of powder. The utility of such models to optimize concrete mixes to achieve good balance between filling ability, passing ability, segregation, compressive strength, and cost is discussed. Examples highlighting the usefulness of the models are presented using isoresponse surfaces to demonstrate single and coupled effects of mix parameters on slump flow, loss of fluidity, flow resistance, segregation, JRing combined to Orimet, and compressive strength at 7 and 28 days. Cost analysis is carried out to show trade-offs between cost of materials and specified consistency levels and compressive strength at 7 and 28 days that can be used to identify economic mixes. The paper establishes the usefulness of the mathematical models as a tool to facilitate the test protocol required to optimise medium strength SCC.