2 resultados para flame soot

em QSpace: Queen's University - Canada


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Flame retardants (FRs) are added to materials to enhance the fire safety level of readily combustible polymers. Although they have been purported to aid in preventing fires in some cases, they have also become a significant cause for concern given the vast data on environmental persistence and human and animal adverse health effects. Evidence since the 1980s has shown that Canadian, American and Europeans have detectable levels of FRs in their bodies. North Americans in particular have high levels of these chemicals due to stringent flammability standards and the higher use of polybrominated diphenyl ethers (PBDEs) in North America as opposed to Europe. FRs have been detected in household dust and some evidence suggests that TVs could be a significant source of exposure to FRs. It is imperative to re-visit the flammability standard (UL94V) that allows for FR use in TVs plastic materials by providing a risk versus benefit analysis to determine if this standard provides a fire safety benefit and if it plays a major role in FR exposure. This report first examined the history of televisions and the progression to the UL94V flammability test standard to understand why FRs were first added to polymers used in the manufacturing of TVs. It has been demonstrated to be due to fire hazards resulting from the use of plastic materials in cathode-ray tube (CRT) TVs that had an “instant-on” feature and high voltage and operating temperatures. In providing a risk versus benefit analysis, this paper presents the argument that 1) by providing a market survey the current flammability test standard (UL94V) is outdated and lacks relevance to current technology as flat, thin, energy efficient Liquid Crystal Displays (LCDs) dominate over traditionally used heavy, bulky and energy-intensive CRTs; 2) FRs do not impart fire safety benefits considering that there is a lack of valid fire safety concern, such as reduced internal and external ignition and fire hazard, and a lack of valid fire data and hazard for television fires in general and finally; 3) the standard is overly stringent as it does not consider the risk due to exposure to FRs in household dust due to the proliferation and greater use of televisions in households. Therefore, this report argues that the UL94V standard has become trapped in history and needs to be updated as it may play a major role in FR exposure.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Cyclododecane (CDD) is a waxy, solid cyclic hydrocarbon (C12H24) that sublimes at room temperature and possesses strong hydrophobicity. In paper conservation CDD is used principally as a temporary fixative of water-soluble media during aqueous treatments. Hydrophobicity, ease of reversibility, low toxicity, and absence of residues are reasons often cited for its use over alternative materials although the latter two claims continue to be debated in the literature. The sublimation rate has important implications for treatment planning as well as health and safety considerations given the dearth of reliable information on its toxicity and exposure limits. This study examined how the rate of sublimation is affected by fiber type, sizing, and surface finish as well as delivery in the molten phase and as a saturated solution in low boiling petroleum ether. The effect of warming the paper prior to application was also evaluated. Sublimation was monitored using gravimetric analysis after which samples were tested for residues with gas chromatography-flame ionization detection (GC-FID) to confirm complete sublimation. Water absorbency tests were conducted to determine whether this property is fully reestablished. Results suggested that the sublimation rate of CDD is affected minimally by all of the paper characteristics and application methods examined in this study. The main factors influencing the rate appear to be the thickness and mass of the CDD over a given surface area as well as temperature and ventilation. The GC-FID results showed that most of the CDD sublimed within several days of its disappearance from the paper surface regardless of the application method. Minimal changes occurred in the water absorbency of the samples following complete sublimation.