When plastic pipe is solidified, it proceeds through a long cooling chamber. Inside this chamber, inside the hollow extrudate, the plastic is molten, and this inner surface solidifies last. Sag, the flow due to the self-weight of the molten plastic, then happens in this cooling chamber, and sometimes, thickened regions (called knuckles) arise in the lower quadrants, especially of large diameter thickwalled pipes. To compensate for sag, engineers normally shift the die centerpiece downward. This thesis focuses on the consequences of this decentering. Specifically, when the molten polymer is viscoelastic, as is normally the case, a downward lateral force is exerted on the mandrel. Die eccentricity also affects the downstream axial force on the mandrel. These forces govern how rigidly the mandrel must be attached (normally, on a spider die). We attack this flow problem in eccentric cylindrical coordinates, using the Oldroyd 8-constant constitutive model framework. Specifically, we revise the method of Jones (1964), called polymer process partitioning. We estimate both axial and lateral forces. We develop a corresponding map to help plastics engineers predict the extrudate shape, including extrudate knuckles. From the mass balance over the postdie region, we then predict the shape of the extrudate entering the cooling chamber. We further include expressions for the stresses in the extruded polymer melt. We include detailed dimensional worked examples to show process engineers how to use our results to design pipe dies, and especially to suppress extrudate knuckling.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Zr-Excel alloy (Zr-3.5Sn-0.8Nb-0.8Mo) is a dual phase (α + β) alloy in the as-received pressure tube condition. It has been proposed to be the pressure tube candidate material for the Generation-IV CANDU-Supercritical Water Reactor (CANDU-SCWR). In this dissertation, the effects of heavy ion irradiation, deformation and heat treatment on the microstructures of the alloy were investigated to enable us to have a better understanding of the potential in-reactor performance of this alloy. In-situ heavy ion (1 MeV) irradiation was performed to study the nucleation and evolution of dislocation loops in both α- and β-Zr. Small and dense type dislocation loops form under irradiation between 80 and 450 °C. The number density tends to saturate at ~ 0.1 dpa. Compared with the α-Zr, the defect yield is much lower in β-Zr. The stabilities of the metastable phases (β-Zr and ω-Zr) and the thermal-dynamically equilibrium phase, fcc Zr(Mo, Nb)2, under irradiation were also studied at different temperatures. Chemi-STEM elemental mapping was carried out to study the elemental redistribution caused by irradiation. The stability of these phases and the elemental redistribution are strongly dependent on irradiation temperature. In-situ time-of-flight neutron diffraction tensile and compressive tests were carried out at different temperatures to monitor lattice strain evolutions of individual grain families during these tests. The β-Zr is the strengthening phase in this alloy in the as-received plate material. Load is transferred to the β-Zr after yielding of the α-Zr grains. The temperature dependence of static strain aging and the yielding sequence of the individual grain families were discussed. Strong tensile/compressive asymmetry was observed in the {0002} grain family at room temperature. The microstructures of the sample deformed at 400 °C and the samples only subjected to heat treatment at the same temperature were characterized with TEM. Concentration of β phase stabilizers in the β grain and the morphology of β grain have significant effect on the stability of β- and ω-Zr under thermal treatment. Applied stress/strain enhances the decomposition of isothermal ω phase but suppresses α precipitation inside the β grains at high temperature. An α → ω/ZrO phase transformation was observed in the thin foils of Zr-Excel alloy and pure Zr during in-situ heating at 700 °C in TEM.