3 resultados para poly glutamic acid
em Greenwich Academic Literature Archive - UK
Resumo:
N-acetyl-L-glutamic acid, crystallizes in the orthorhombic space group P2(1)2(1)2(1) with unit cell parameters a = 4.747(3), b = 12.852(7), c = 13.906(7) Å, V = 848.5(8) Å3, Z = 4, density (calculated) = 1.481 mg/m3, linear absorption coefficient 0.127 mm−1. The crystal structure determination was carried out with MoKalpha X-ray data measured with liquid nitrogen cooling at 100(2) K temperature. In the final refinement cycle the data/restraints/parameter ratios were 1,691/0/131; goodness-of-fit on F(2) = 1.122. Final R indices for [I > 2sigma(I)] were R1 = 0.0430, wR2 = 0.0878 and R indices (all data) R1 = 0.0473, wR2 = 0.0894. The largest electron density difference peak and hole were 0.207 and −0.154 eÅ(−3). Details of the molecular geometry are discussed and compared with a model DFT structure calculated using Gaussian 98.
Resumo:
Solid state IR and Raman as well as aqueous solution state Raman spectra are reported for the linear di-amino acid peptide L-aspartyl-L-glutamic acid (L-Asp-L-Glu); the solution state Raman spectrum has also been obtained for the N,O-deuterated derivative. SCF-DFT calculations at the B3-LYP/cc-pVDZ level established that the structure and vibrational spectra of L-Asp-L-Glu can be interpreted using a model of the peptide with ten hydrogen-bonded water molecules, in conjunction with the conductor-like polarizable continuum solvation method. The DFT calculations resulted in the computation of a stable zwitterionic structure, which displays trans-amide conformation. The vibrational spectra were computed at the optimised molecular geometry, enabling normal coordinate analysis, which yielded satisfactory agreement with the experimental IR and Raman data. Computed potential energy distributions of the normal modes provided detailed vibrational assignments.
Resumo:
The aim of this study was determine whether bonding of glass-ionomer cements to non-carious dentine differed from that to carious dentine. Five commercial cements were used, namely Fuji IX GP, Fuji IX capsulated, Fuji IX Fast capsulated (all GC, Japan), Ketac-Molar and Ketac-Molar Aplicap (both 3M-ESPE, Germany). Following conditioning of the substrate with 10% poly (acrylic acid) for 10 s, sets of 10 samples of the cements were bonded to prepared teeth that had been removed for orthodontic reasons. The teeth used had either sound dentine or sclerotic dentine. Shear bond strengths were determined following 24 h storage. For the auto-mixed cements, shear bond strength to sound dentine was found not to differ statistically from shear bond strength to sclerotic dentine whereas for hand-mixed cements, shear bond to sound dentine was found to be higher than to carious dentine (to at least p < 0.05). This shows that the chemical effects arising from interactions of glass-ionomer cements with the mineral phase of the tooth are the most important in developing strong bonds, at least in the shorter term.