5 resultados para nucleation and growth

em Greenwich Academic Literature Archive - UK


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Probe-based scanning microscopes, such as the STM and the AFM, are used to obtain the topographical and electronic structure maps of material surfaces, and to modify their morphologies on nanoscopic scales. They have generated new areas of research in condensed matter physics and materials science. We will review some examples from the fields of experimental nano-mechanics, nano-electronics and nano-magnetism. These now form the basis of the emerging field of Nano-technology. A parallel development has been brought about in the field of Computational Nano-science, using quantum-mechanical techniques and computer-based numerical modelling, such as the Molecular Dynamics (MD) simulation method. We will report on the simulation of nucleation and growth of nano-phase films on supporting substrates. Furthermore, a theoretical modelling of the formation of STM images of metallic clusters on metallic substrates will also be discussed within the non-equilibrium Keldysh Green function method to study the effects of coherent tunnelling through different atomic orbitals in a tip-sample geometry.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The formation and growth of intermetallic compound layer thickness is one of the important issues in search for reliable electronic and electrical connections. Intermetallic compounds (IMCs) are an essential part of solder joints. At low levels, they have a strengthening effect on the joint; but at higher levels, they tend to make solder joints more brittle. If the solder joint is subjected to long-standing exposure of high temperature, this could result in continuous growth of intermetallic compound layer. The brittle intermetallic compound layer formed in this way is very much prone to fracture and cold therefore lead to mechanical and electrical failure of the joint. Therefore, the primary aim of this study is to investigate the growth of intermetallic compound layer thickness subjected to five different reflow profiles. The study also looks at the effect of three different temperature cycles (with maximum cycle temperature of 25 0C, 40 0C and 60 0C) on intermetallic compound formation and their growth behaviour.. Two different Sn-Ag-Cu solder pastes (namely paste P1 and paste P2) which were different in flux medium, were used for the study. The result showed that the growth of intermetallic compound layer thickness was a function of ageing temperature. It was found that the rate of growth of intermetallic compound layer thickness of paste P1 was higher than paste P2 at the same temperature condition. This behaviour could be related to the differences in flux mediums of solder paste samples used.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

AIM: To examine the concentrations of zinc and omega-6 polyunsaturated fatty acids (omega-6 PUFAs) in breast milk, the impact of zinc on omega-6 PUFA metabolism, and the growth rate of infants. METHODS: Forty-one mother-term infant pairs from a rural area of northern Beijing, China, who were 1 month (n = 18, group I) and 3 months (n = 23, group II) old and exclusively breastfed, were studied. The dietary records and the concentrations of zinc and omega-6 PUFAs in the milk of lactating women and the increase in weight and length of their infants during 1 and 3 postnatal months were analysed. RESULTS: The dietary intakes of mothers in the two groups were the same, i.e. high in carbohydrate and low in fat, protein and energy. The maternal zinc intake was 7.5mg/d and thus reached only 34.6% of the current Recommended Nutrient Intake (RNI). The levels of zinc and arachidonic acid (AA, C20:4 omega-6) in the milk of group I were significantly higher than those in group II. Furthermore, significant positive correlations were found between the concentrations of zinc and AA in the breast milk and between the level of milk AA and weight gain. CONCLUSION: Zinc may be a co-factor and essential for essential fatty acids (EFA) metabolism. Thus suboptimal zinc intake may cause EFA imbalance. Further studies of Chinese rural mother-infant pairs are necessary to determine whether zinc supplementation should be recommended when lactation exceeds 3 months.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A review of the atomistic modelling of the behaviour of nano-scale structures and processes via molecular dynamics (MD) simulation method of a canonical ensemble is presented. Three areas of application in condensed matter physics are considered. We focus on the adhesive and indentation properties of the solid surfaces in nano-contacts, the nucleation and growth of nano-phase metallic and semi-conducting atomic and molecular films on supporting substrates, and the nano- and multi-scale crack propagation properties of metallic lattices. A set of simulations selected from these fields are discussed, together with a brief introduction to the methodology of the MD simulation. The pertinent inter-atomic potentials that model the energetics of the metallic and semi-conducting systems are also given.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The dissolution of thin film under-bump-metallization (UBM) by molten solder has been one of the most serious processing problems in electronic packaging technology. Due to a higher melting temperature and a greater Sn content, a molten lead-free solder such as eutectic SnAg has a faster dissolution rate of thin film UBM than the eutectic SnPb. The work presented in this paper focuses on the role of 0.5 wt % Cu in the base Sn–3.5%Ag solder to reduce the dissolution of the Cu bond pad in ball grid array applications. We found that after 0.5 wt % Cu addition, the rate of dissolution of Cu in the molten Sn–3.5%Ag solder slows down dramatically. Systematic experimental work was carried out to understand the dissolution behavior of Cu by the molten Sn–3.5%Ag and Sn–3.5%Ag–0.5%Cu solders at 230–250 °C, for different time periods ranging from 1 to 10 min. From the curves of consumed Cu thickness, it was concluded that 0.5 wt % Cu addition actually reduces the concentration gradient at the Cu metallization/molten solder interface which reduces the driving force of dissolution. During the dissolution, excess Cu was found to precipitate out due to heterogeneous nucleation and growth of Cu6Sn5 at the solder melt/oxide interface. In turn, more Cu can be dissolved again. This process continues with time and leads to more dissolution of Cu from the bond pad than the amount expected from the solubility limit, but it occurs at a slower rate for the molten Sn–3.5%Ag–0.5%Cu solder. © 2003 American Institute of Physics.