The wettability of newly developed Sn-2.8Ag-0.5Cu-1.0Bi lead-free solder on Cu and Ni substrates was assessed through the wetting balance tests. The wettability assessment parameters such as contact angle (ϑc) and maximum wetting force (Fw) were documented for three solder bath temperatures with three commercial fluxes, namely, no-clean (NC), nonactivated (R), and water-soluble organic acid flux (WS). It was found that the lead-free Sn-2.8Ag-0.5Cu-1.0Bi solder exhibited less wetting force, i.e., poorer wettability, than the conventional Sn-37Pb solder for all flux types and solder bath temperatures. The wettability of Sn-2.8Ag-0.5Cu-1.0Bi lead-free solder on Cu substrate was much higher than that on Ni substrate. Nonwetting for Sn-2.8Ag-0.5Cu-1.0Bi and Sn-Pb solders on Ni substrate occurred when R-type flux was used. A model was built and simulations were performed for the wetting balance test. The simulation results were found very close to the experimental results. It was also observed that larger values of immersion depth resulted in a decrease of the wetting force and corresponding meniscus height, whereas the increase in substrate perimeter enhanced the wettability. The wetting reactions between the solder and Cu/Ni substrates were also investigated, and it was found that Cu atoms diffused into the solder through the intermetallic compounds (IMCs) much faster than did the Ni atoms. Rapid formation of IMCs inhibited the wettability of Sn-2.8Ag-0.5Cu-1.0Bi solder compared to the Sn-Pb solder.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The growth behavior of intermetallic layer with or without adding 0.3 wt% Ni into the Sn-0.7Cu solder was studied during the wetting reaction on Cu-substrate and thereafter in solid-state aging condition. The Cu-solder reaction couple was prepared at 255, 275 and 295 °C for 10 s. The samples reacted at 255 °C were then isothermally aged for 2-14 days at 150 °C. The reaction species formed for the Sn-0.7Cu/Cu and Sn-0.7Cu-0.3Ni/Cu soldering systems were Cu6Sn5 and (CuNi)6Sn5, respectively. The thickness of the intermetallic compounds formed at the solder/Cu interfaces and also in the bulk of both solders increased with the increase of reaction temperature. It was found that Ni-containing Sn-0.7Cu solder exhibited lower growth of intermetallic layer during wetting and in the early stage of aging and eventually exceeded the intermetallic layer thickness of Sn-0.7Cu/Cu soldering system after 6 days of aging. As the aging time proceeds, a non-uniform intermetallic layer growth tendency was observed for the case of Sn-0.7Cu-0.3Ni solder. The growth behavior of intermetallic layer during aging for both solders followed the diffusion-controlled mechanism. The intermetallic layer growth rate constants for Sn-0.7Cu and Sn-0.7Cu-0.3Ni solders were calculated as 1.41 × 10-17 and 1.89 × 10-17 m2/s, respectively which indicated that adding 0.3 wt% Ni with Sn-0.7Cu solder contributed to the higher growth of intermetallic layer during aging. © 2006 Elsevier B.V. All rights reserved.