5 resultados para Clientes OPC DA e AE
em Greenwich Academic Literature Archive - UK
Resumo:
Abstract not available
Resumo:
This paper investigates the use of the acoustic emission (AE) monitoring technique for use in identifying the damage mechanisms present in paper associated with its production process. The microscopic structure of paper consists of a random mesh of paper fibres connected by hydrogen bonds. This implies the existence of two damage mechanisms, the failure of a fibre-fibre bond and the failure of a fibre. This paper describes a hybrid mathematical model which couples the mechanics of the mass-spring model to the acoustic wave propagation model for use in generating the acoustic signal emitted by complex structures of paper fibres under strain. The derivation of the mass-spring model can be found in [1,2], with details of the acoustic wave equation found in [3,4]. The numerical implementation of the vibro-acoustic model is discussed in detail with particular emphasis on the damping present in the numerical model. The hybrid model uses an implicit solver which intrinsically introduces artificial damping to the solution. The artificial damping is shown to affect the frequency response of the mass-spring model, therefore certain restrictions on the simulation time step must be enforced so that the model produces physically accurate results. The hybrid mathematical model is used to simulate small fibre networks to provide information on the acoustic response of each damage mechanism. The simulated AEs are then analysed using a continuous wavelet transform (CWT), described in [5], which provides a two dimensional time-frequency representation of the signal. The AEs from the two damage mechanisms show different characteristics in the CWT so that it is possible to define a fibre-fibre bond failure by the criteria listed below. The dominant frequency components of the AE must be at approximately 250 kHz or 750 kHz. The strongest frequency component may be at either approximately 250 kHz or 750 kHz. The duration of the frequency component at approximately 250 kHz is longer than that of the frequency component at approximately 750 kHz. Similarly, the criteria for identifying a fibre failure are given below. The dominant frequency component of the AE must be greater than 800 kHz. The duration of the dominant frequency component must be less than 5.00E-06 seconds. The dominant frequency component must be present at the front of the AE. Essentially, the failure of a fibre-fibre bond produces a low frequency wave and the failure of a fibre produces a high frequency pulse. Using this theoretical criteria, it is now possible to train an intelligent classifier such as the Self-Organising Map (SOM) [6] using the experimental data. First certain features must be extracted from the CWTs of the AEs for use in training the SOM. For this work, each CWT is divided into 200 windows of 5E-06s in duration covering a 100 kHz frequency range. The power ratio for each windows is then calculated and used as a feature. Having extracted the features from the AEs, the SOM can now be trained, but care is required so that the both damage mechanisms are adequately represented in the training set. This is an issue with paper as the failure of the fibre-fibre bonds is the prevalent damage mechanism. Once a suitable training set is found, the SOM can be trained and its performance analysed. For the SOM described in this work, there is a good chance that it will correctly classify the experimental AEs.
Resumo:
In this study, a simplified Acoustic Emission (AE) equipment, in essence an AE signal conditioner and a USB (Universal Serial Bus) data acquisition system, is used to study what happens in paper structures during mechanical loading. By the use of such equipment, some parameters that can be extracted are e.g. the stress and strain at onset of AE, the stress and strain at the onset of rapid AE defined as some numerical factor (larger then one) times the initial emission rate, the emission rate at the first stage of loading and the stress and strain at final failure i.e. when the specimen loses its load carrying ability.In this study however, the interest is focused on one particular parameter i.e. the elastic strain energy density W c at onset of AE. This is a parameter with a clear physical meaning and in this study, the correlation between this parameter and a fracture toughness measure, is investigated.The conclusion is that when nine different paper materials (with a large span regarding properties) are considered, there is a correlation (however not linear) between these two parameters.
Resumo:
The investigation of the long-term performance of solidified/stabilized (S/S) contaminated soils was carried out in a trial site in southeast UK. The soils were exposed to the maximum natural weathering for four years and sampled at various depths in a controlled manner. The chemical properties (e.g., degree of carbonation (DOC), pH, electrical conductivity (EC)) and physical properties (e.g., moisture content (MC), liquid limit (LL), plastic limit (PL), plasticity index (PI)) of the samples untreated and treated with the traditional and accelerated carbonated S/S processes were analyzed. Their variations on the depths of the soils were also studied. The result showed that the broad geotechnical properties of the soils, manifested in their PIs, were related to the concentration of the water soluble ions and in particular the free calcium ions. The samples treated with the accelerated carbonation technology (ACT), and the untreated samples contained limited number of free calcium ions in solutions and consequently interacted with waters in a similar way. Compared with the traditional cement-based S/S technology, e.g., treatment with ordinary portland cement (OPC) or EnvirOceM, ACT caused the increase of the PI of the treated soil and made it more stable during long-term weathering. The PI values for the four soils ascended according to the order: the EnvirOceM soil, the OPC soil, the ACT soil, and the untreated soil while their pH and EC values descended according to the same order.
Resumo:
Freshly-mixed and partially-cured ordinary Portland cement (OPC) pastes have been shown to exhibit good biological compatibility with a range of cells and tissue-types; particularly those associated with bone formation. Formulations based on OPC have been used as dental restoratives and are now being investigated for their potential use in orthopaedic repair. Despite the current clinical interest in OPCs, very little is known about their chemistry in the physiological environment. In this respect, research to investigate aspects of the interactions between a white Portland cement (WPC) paste and simulated body fluid (SBF) has been carried out in vitro. Exposure to SBF has been found to promote the precipitation of a layer of 'bone-like' hydroxyapatite on the surface of WPC paste which underpins its ability to integrate with living tissue. The dissolution of portlandite and formation of calcite were also observed on contact with SBF.