6 resultados para POLY(EPSILON-CAPROLACTONE) C BLOCK
em DigitalCommons@University of Nebraska - Lincoln
Resumo:
The structures and association properties of thermosensitive block copolymers of poly(methoxyoligo( ethylene glycol) norbornenyl esters) in D2O were investigated by small angle neutron scattering (SANS). Each block is a comblike polymer with a polynorbornene (PNB) backbone and oligo ethylene glycol (OEG) side chains (one side chain per NB repeat unit). The chemical formula of the block copolymer is (OEG3NB) 79- (OEG6.6NB) 67, where subscripts represent the degree of polymerization (DP) of OEG and NB in each block. The polymer concentration was fixed at 2.0 wt % and the structural changes were investigated over a temperature range between 25 and 68°C. It was found that at room temperature polymers associate to form micelles with a spherical core formed by the block (OEG3NB) 79 and corona formed by the block (OEG6.6NB) 67 and that the shape of the polymer in the corona could be described by the form factor of rigid cylinders. At elevated temperatures, the aggregation number increased and the micelles became more compact. At temperatures around the cloud point temperature (CPT) T ) 60 °C a correlation peak started to appear and became pronounced at 68 °C due to the formation of a partially ordered structure with a correlation length ∼349 Å.
Resumo:
The high electronegativity and small size of the fluorine atom and the high stability of C-F bonds impart interesting properties and applications to fluorine containing polymers. The unique properties of fluoropolymers include high thermal stability, improved chemical resistance, low surface energies, low coefficients of friction, and low dielectric constants. Applications of fluorinated polymers include use as noncorrosive materials, polymer processing aids, chemically resistant and antifouling coatings, as well as interlayer dielectrics. Fluorine-containing polymers can be directly synthesized via polymerization of fluorine-containing monomers or by post-polymerization modification. The latter method can be used to attach fluorinated species, such as perfluoroalkyl groups, onto conventional polymer chains, thereby imparting properties of fluorine-containing polymers into conventional polymers and widening their range of potential applications.
Resumo:
Preferential adsorption of poly(2-vinylpyridine)-deuterated polystyrene-poly(2-vinylpyridine) (PVP-dPS-PVP) triblock copolymers from toluene onto silicon leads to the formation of dPS loops tethered by the PVP end blocks. Using neutron reflectometry, we have determined the segment density profiles of these looped polymer brushes in toluene, a good solvent for the dPS block, and in cyclohexane at 20 °C (poor solvent), 32 °C, (near-Θ solvent), and 50 °C (marginal solvent). While the swelling behavior qualitatively agrees with that observed for singly grafted brushes, there are interesting differences in the local structural details: In a good solvent, the segment density profiles are composed of an inner parabolic region and a long, extended tail. In cyclohexane, the profiles are described by exponential decays. We ascribe these features to a novel polydispersity effect that arises due to tethering the PS loops by both ends. The results also show that the less dense layers undergo more significant changes in swollen height as solvent quality is changed and that the looped brushes of different molecular weight, asymmetry, and tethering density adhere to scaling relationships derived for lightly cross-linked polymer gels.
Resumo:
The reaction of living anionic polymers with 2,2,5,5-tetramethyl-1-(3-bromopropyl)-1-aza-2,5- disilacyclopentane (1) was investigated using coupled thin layer chromatography and matrix-assisted laser desorption/ionization time-of-flight mass spectrometry. Structures of byproducts as well as the major product were determined. The anionic initiator having a protected primary amine functional group, 2,2,5,5-tetramethyl- 1-(3-lithiopropyl)-1-aza-2,5-disilacyclopentane (2), was synthesized using all-glass high-vacuum techniques, which allows the long-term stability of this initiator to be maintained. The use of 2 in the preparation of well-defined aliphatic primary amine R-end-functionalized polystyrene and poly(methyl methacrylate) was investigated. Primary amino R-end-functionalized poly(methyl methacrylate) can be obtained near-quantitatively by reacting 2 with 1,1-diphenylethylene in tetrahydrofuran at room temperature prior to polymerizing methyl methacrylate at -78 °C. When 2 is used to initiate styrene at room temperature in benzene, an additive such as N,N,N',N'- tetramethylethylenediamine is necessary to activate the polymerization. However, although the resulting polymers have narrow molecular weight distributions and well-controlled molecular weights, our mass spectra data suggest that the yield of primary amine α-end-functionalized polystyrene from these syntheses is very low. The majority of the products are methyl α-end-functionalized polystyrene.
Resumo:
Living anionic polymerization of 4-vinylbenzocylobutene was performed in benzene at room temperature using sec-butyllithium as the initiator. Results of the kinetic studies indicated the termination- and transfer-free nature of the polymerization. Homopolymers with predictable molecular weights and narrow molecular weight distributions were produced, excluding the interference of the cyclobutene rings during initiation and propagation. Thermogravimetric analysis of poly(4-vinylbenzocyclobutene) in air showed a small weight gain at ~200 °C, a rapid decomposition at ~455 °C, and a gradual decomposition at ~566 °C. This behavior was attributed to the formation of radicals from the pendent benzocyclobutene functionality through o-quinodimethane intermediates and simultaneous decomposition/cross-linking reactions at high temperature. The living nature of the polymerization was also examined via sequential copolymerization with butadiene to form diblock copolymers.
Resumo:
ABSTRACT: One way to produce high order in a block copolymer thin film is by solution casting a thin film and slowly evaporating the solvent in a sealed vessel. Such a solvent-annealing process is a versatile method to produce a highly ordered thin film of a block copolymer. However, the ordered structure of the film degrades over time when stored under ambient conditions. Remarkably, this aging process occurs in mesoscale thin films of polystyrene-polyisoprene triblock copolymer where the monolayer of vitrified 15 nm diameter polystyrene cylinders sink in a 20 nm thick film at 22 °C. The transformation is studied by atomic force microscopy (AFM). We describe the phenomena, characterize the aging process, and propose a semiquantitative model to explain the observations. The residual solvent effects are important but not the primary driving force for the aging process. The study may lead to effective avenue to improve order and make the morphology robust and possibly the solvent-annealing process more effective.