6 resultados para electrochromic displays
em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo
Resumo:
In this work, two ruthenium complexes, [Ru(bpy)(3)](PF6)(2) and [Ru(ph2phcn)(3)](PF6)(2) in poly(inethylinethacrylate) matrix were employed to build single-layer light-emitting electrochemical cells by spin coating on indium tin oxide substrate. In both cases the electroluminescence spectra exhibit a relatively broad band with maxima near to 625 rim and CIE (x, y) color coordinates of (0.64, 0.36), which are comparable with the photoluminescence data in the same medium. The best result was obtained with the [Ru(bpy)(3)](PF6)(2) device where the optical output power approaches 10 mu W at the band maximum with a wall-plug efficiency higher than 0.03%. The lowest driving voltage is about 4 V for an electrical current of 20 mA. (c) 2008 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
Gel Polymer Electrolytes (GPE) based on agar and containing LiClO4 have been prepared, characterized and applied to electrochromic devices. The ionic conductivity revealed the best result of 6.5 x 10(-5) S/cm for the sample with 17 wt.% of LiClO4, which increased to 5.4 x 10(-4) S/cm at 72 degrees C. TheGPE have been used in electrochromic devices (ECD) with K-glass/WO3/GPE/CeO2-TiO2/K-glass configuration. The ECD changed transmittance values up to 30% between the colored and transparent states. The charge density measurements revealed an increase of 5.5 to 7.5 mC/cm(2) from the first to 500th cycles and then a decrease to 4.4 mC/cm(2) during the next 4500 cycles. Coloration efficiency (eta) of 25 cm(2)/C was obtained.
Resumo:
The electrochromic behavior of iron complexes derived from tetra-2-pyridyl-1,4-pyrazine (TPPZ) and a hexacyanoferrate species in polyelectrolytic multilayer adsorbed films is described for the first time. This complex macromolecule was deposited onto indium-tin oxide (ITO) substrates via self-assembly, and the morphology of the modified electrodes was studied using atomic force microscopy (AFM), which indicated that the hybrid film containing the polyelectrolyte multilayer and the iron complex was highly homogeneous and was approximately 50 nm thick. The modified electrodes exhibited excellent electrochromic behavior with both intense and persistent coloration as well as a chromatic contrast of approximately 70%. In addition, this system achieved high electrochromic efficiency (over 70 cm(2) C-1 at 630 nm) and a response time that could be measured in milliseconds. The electrode was cycled more than 10(3) times, indicating excellent stability.
Resumo:
Air conditioning and lighting costs can be reduced substantially by changing the optical properties of "intelligent windows." The electrochromic devices studied to date have used copper as an additive. Copper, used here as an electrochromic material, was dissolved in an aqueous animal protein-derived gel electrolyte. This combination constitutes the electrochromic system for reversible electrodeposition. Cyclic voltammetry, chronoamperometric and chromogenic analyses indicated that were obtained good conditions of transparency (initial transmittance of 70%), optical reversibility, small potential window (2.1 V), variation of transmittance in visible light (63.6%) and near infrared (20%) spectral regions. Permanence in the darkened state was achieved by maintaining a lower pulse potential (-0.16 V) than the deposition potential (-1.0 V). Increasing the number of deposition and dissolution cycles favored the transmittance and photoelectrochemical reversibility of the device. The conductivity of the electrolyte (10(-3) S/cm) at several concentrations of CuCl2 was determined by electrochemical impedance spectroscopy. A thermogravimetric analysis confirmed the good thermal stability of the electrolyte, since the mass loss detected up to 100 degrees C corresponded to water evaporation and decomposition of the gel started only at 200 degrees C. Micrographic and small angle X-ray scattering analyses indicated the formation of a persistent deposit of copper particles on the ITO. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
Ionic conducting membranes of gelatin plasticized with glycerol and containing LiI/I-2 have been obtained and characterized by X-ray diffraction measurements, UV-Vis-NIR spectroscopy, thermal analysis and impedance spectroscopy. The transparent (80-90% in the visible range) membranes showed ionic conductivity value of 5 x 10(-5) S/cm at room temperature, which increased to 3 x 10(-3) S/cm at 80 degrees C. All the ionic conductivity measurements as a function of temperature showed VTF dependence and activation energy of 8 kJ/mol. These samples also showed low glass transition temperature of -76 degrees C. Moreover the samples were predominantly amorphous. The membranes applied to small electrochromic devices showed 20% of color change from colored to bleached states during more than 70 cronoamperometric cycles.
Resumo:
The combination of semiconducting oxides and polyaniline in the nanoscale range may result in hybrid materials having enhanced properties, such as electrochromism and charge capacity. This paper reports the spectroscopic, morphological and electrochromic characterization of hybrid films made up of hexaniobate one-dimensional (1D) nanoscrolls and polyaniline prepared by the layer-by-layer assembly technique (LbL). Secondary electron imaging and backscattered electron imaging techniques performed using a scanning electron microscope showed that polyaniline is adsorbed on the hexaniobate nanoscrolls, which confirms the combination of the components in the nanoscale domain. UV-VIS-NIR electronic spectra of the LbL hybrid films showed the absorption tail in the NIR region, assigned to delocalized polarons of the polyaniline. Resonance Raman spectra in the 1000-1700 cm(-1) range indicated that hybrid films present a higher relative intensity of polaron bands at 1337 and 1508 cm(-1) than pristine polyaniline in the emeraldine salt form. These results suggest that hexaniobate nanoscrolls induce a secondary doping of polyaniline. The cyclic voltammetry (CV) data for the hybrid film showed a specific capacity of 870 C cm(-3). According to CV results, the synergistic effect on charge storage properties of the hybrid material is attributed to the enhanced electroactivity of the hexaniobate component in the LbL film. Spectroelectrochemical experiments showed that the electrochromic efficiencies at 420 nm are ca. -41 and 24 cm(2) C-1 as the potential changes from 0.8 to -0.9 V and from -0.9 to -1.8 V, respectively, whereas at 800 nm the efficiencies are ca. -55 and 8 cm(2) C-1 for the same potential ranges. The electrochromic efficiencies and multi-colour character of the LbL film of hexaniobate nanoscrolls and polyaniline indicate that this novel hybrid material is an interesting modified electrode for electrochromic devices.