Resumo:
Objectives: To evaluate the effect of additives on the water sorption characteristics of Bis-GMA based copolymers and composites containing TEGDMA, CH(3)Bis-GMA or CF(3)Bis-GMA. Material and methods: Fifteen experimental copolymers and corresponding composites were prepared combining Bis-GMA and TEGDMA, CH(3)Bis-GMA or CF(3)Bis-GMA, with aldehyde or diketone (24 and 32 mol%) totaling 30 groups. For composites, barium aluminosilicate glass and pyrogenic silica was added to comonomer mixtures. Photopolymerization was effected by 0.2 wt% each of camphorquinone and N,N-dimethyl-p-toluidine. Specimen densities in dry and water saturated conditions were obtained by Archimedes' method. Water sorption and desorption were evaluated in a desorption-sorption-desorption cycle. Water uptake (%WU), water desorption (%WD), equilibrium solubility (ES; mu g/mm(3)), swelling (f) and volume increase (%V) were calculated using appropriate equations. Results: All resins with additives had increased %WU and ES. TEGDMA-containing systems presented higher %WU, %WD, ES, f and %V values, followed by resins based on CH(3)Bis-GMA and CF(3)Bis-GMA. Conclusions: Aldehyde and diketone led to increases in the water sorption characteristics of experimental resins.
Resumo:
The effect of different propionaldehyde ratios on the properties of bis-GMA-based comonomers and copolymers diluted with propoxylated bis-GMA (CH3bis-GMA) was evaluated. Five experimental comonomers were prepared combining bis-GMA with CH3bis-GMA and propionaldehyde at 0, 2, 8, 16, 24 mol%. Light polymerization was effected with the use of 0.2 wt. (%) each of camphorquinone and N,N-dimethyl-p-toluidine. Resin degrees of conversion (%DC) were evaluated by FT-IR spectrophotometry and Tg by Differential Scanning Calorimeter. Complex viscosity (η*), the effect of temperature on η*, and Microhardness (H) for dry and wet samples were also determined. Data were analyzed by Student's t-test, one-way ANOVA and Tukey-Kramer test (α = 0.05). The group with 24 mol% additive had a significant increase in %DC and H, and the lowest comonomer Tg and η*. No remarkable variation was noted in copolymers Tg s. All resins presented Newtonian behavior of viscosity, which linearly decreased with increased temperature. The η* decreased sigmoidally as the additive ratio increased.
Resumo:
Objectives. The purpose of this study was to evaluate the reactivity and polymerization kinetics behavior of a model dental adhesive resin with water-soluble initiator systems. Methods. A monomer blend based on Bis-GMA, TEGDMA and HEMA was used as a model dental adhesive resin, which was polymerized using a thioxanthone type (QTX) as a photoinitiator. Binary and ternary photoinitiator systems were formulated using 1 mol% of each initiator. The co-initiators used in this study were ethyl 4-dimethylaminobenzoate (EDAB), diphenyliodonium hexafluorophosphate (DPIHFP), 1,3-diethyl-2-thiobarbituric acid (BARB), p-toluenesulfinic acid and sodium salt hydrate (SULF). Absorption spectra of the initiators were measured using a UV-Vis spectrophotometer, and the photon absorption energy (PAE) was calculated. The binary system camphorquinone (CQ)/amine was used as a reference group (control). Twelve groups were tested in triplicate. Fourier-transform infrared spectroscopy (FTIR) was used to investigate the polymerization reaction during the photoactivation period to obtain the degree of conversion (DC) and maximum polymerization rate (R-p(max)) profile of the model resin. Results. In the analyzed absorption profiles, the absorption spectrum of QTX is almost entirely localized in the UV region, whereas that of CQ is in the visible range. With respect to binary systems, CQ + EDAB exhibited higher DC and R-p(max) values. In formulations that contained ternary initiator systems, the group CQ + QTX + EDAB was the only one of the investigated experimental groups that exhibited an R-p(max) value greater than that of CQ + EDAB. The groups QTX + EDAB + DPIHFP and QTX + DPIHFP + SULF exhibited values similar to those of CQ + EDAB with respect to the final DC; however, they also exhibited lower reactivity. Significance. Water-soluble initiator systems should be considered as alternatives to the widely used CQ/amine system in dentin adhesive formulations. (C) 2012 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Phosphorylated poly(styrene-co-divinylbenzene) copolymers prepared by aromatic electrophilic substitution reaction with PCl3/AlCl3 were reacted with carbon dissulfite in order to introduce sulfophosphorylated groups into copolymers. These modifications were characterized by FTIR, elemental analysis, spectrophotometry, optical and scanning electron microscopy. The antibacterial activities of the phosphorylated and sulfophorylated copolymers were assessed against Escherichia coli ATCC25922 suspensions (10(3)-10(7) cells mL(-1)) using a column system. The unmodified copolymers did not have antibacterial activity against the E. coil suspensions but the phosphorylated and sulfophorylated copolymers showed significant bactericidal action for all E. coli concentrations. The sulfophosphorylated copolymers had higher antibacterial activity than the phosphorylated ones, mainly for high concentrations of E. coli cells. Published by Elsevier B.V.
Resumo:
Objectives: This study aimed to compare the micro-tensile bond strength of methacrylate resin systems to a silorane-based restorative system on dentin after 24 hours and six months water storage. Material and Methods: The restorative systems Adper Single Bond 2/Filtek Z350 (ASB), Clearfil SE Bond/Z350 (CF), Adper SE Plus/Z350 (ASEP) and P90 Adhesive System/Filtek P90 (P90) were applied on flat dentin surfaces of 20 third molars (n=5). The restored teeth were sectioned perpendicularly to the bonding interface to obtain sticks (0.8 mm2) to be tested after 24 hours (24 h) and 6 months (6 m) of water storage, in a universal testing machine at 0.5 mm/min. The data was analyzed via two-way Analysis of Variance/Bonferroni post hoc tests at 5% global significance. Results: Overall outcomes did not indicate a statistical difference for the resin systems (p=0.26) nor time (p=0.62). No interaction between material × time was detected (p=0.28). Mean standard-deviation in MPa at 24 h and 6 m were: ASB 31.38 (4.53) and 30.06 (1.95), CF 34.26 (3.47) and 32.75 (4.18), ASEP 29.54 (4.14) and 33.47 (2.47), P90 30.27 (2.03) and 31.34 (2.19). Conclusions: The silorane-based system showed a similar performance to methacrylate-based materials on dentin. All systems were stable in terms of bond strength up to 6 month of water storage.