4 resultados para desulfurization
em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo
Resumo:
The objective of this paper is to present an analysis of the use of residual marble mixtures in the pig iron desulfurization process. The study involved the use of: marble waste, fluorspar, lime, and hot metal. Four mixtures were made and added to a liquid hot metal - with known chemical composition - at a temperature of 1450ºC. The mass of each element was calculated from its chemical analysis and compared with an industrial mixture. All of the four mixtures used in the experiments were stirred by a mechanical stirrer. Samples were collected by vacuum sampling for times of 5, 10, 15, 20, and 30 minutes, and analysis was performed to check sulfur variation in the bath with time. The results were analyzed and they verified that it was possible to use marble waste as a desulfurizer.
Resumo:
Na[AuCl4].2H(2)O reacts with tridentate thiosemicarbazide ligands, H(2)L1, derived from N-[N',N'-dialkylamino(thiocarbonyl)]benzimidoyl chloride and thiosemicarbazides under formation of air-stable, green [AuCl(L1)] complexes. The organic ligands coordinate in a planar SNS coordination mode. Small amounts of gold(I) complexes of the composition [AuCl(L3)] are formed as side-products, where L3 is an S-bonded 5-diethylamino-3-phenyl-1-thiocarbamoyl-1,2,4-triazole. The formation of the triazole L3 can be explained by the oxidation of H(2)L1 to an intermediate thiatriazine L2 by Au3+, followed by a desulfurization reaction with ring contraction. The chloro ligands in the [AuCl(L1)] complexes can readily be replaced by other monoanionic ligands such as SCN- or CN- giving [Au(SCN)(L1)] or [Au(CN)(L1)] complexes. The complexes described in this paper represent the first examples of fully characterized neutral Gold(III) thiosemicarbazone complexes. All the [AuCl(L1)] compounds present a remarkable cell growth inhibition against human MCF-7 breast cancer cells. However, systematic variation of the alkyl groups in the N(4)-position of the thiosemicarbazone building blocks as well as the replacement of the chloride by thiocyanate ligands do not considerably influence the biological activity. On the other hand, the reduction of Au-III to Au-I leads to a considerable decrease of the cytotoxicity.
Resumo:
A variety of seemingly unrelated processes, such as core-mantle interaction, desulfurization, and direct precipitation from a silicate melt have been proposed to explain the formation of Ru-Os-Ir alloys (here referred to as osmiridiums) found in terrestrial mantle rocks. However, no consensus has yet been reached on how these important micrometer-sized phases form. In this paper we report the results of an experimental study on the solubilities of Ru, Os and Ir in sulfide melts (or mattes) as a function of alloy composition at 1300 degrees C. Considering the low solubilities of Ru, Os, and Ir in silicate melts, coupled with their high matte/silicate-melt partition coefficients, our results indicate that these elements concentrate initially at the ppm level in a matte phase in the mantle source region. During partial melting, the extraction of sulfur into silicate melt leads to a decrease in fS(2) that triggers the exsolution of osmiridiums from the refractory matte in the residue. The newly formed osmiridiums may persist in the terrestrial mantle for periods exceeding billions of years. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Esse trabalho consiste na caracterização do resíduo de mármore, lama fina de aciaria e borra de alumínio, para averiguar a viabilidade técnica da utilização de tais resíduos na dessulfuração e desfosforação de ferro-gusa líquido. A caracterização desses resíduos foi feita através de análises químicas, granulométricas, difração de raios X e microscopia eletrônica de varredura (MEV) com micro análise por Espectroscopia por Energia Dispersiva de Raios X (EDS). A lama fina de aciaria apresenta um teor de FeO de 84,90%, o resíduo de mármore apresentou um teor de 61,5% de CaO e 33,9% de MgO e a borra de alumínio apresentou 36,5% de Al metálico e 62% de Al2O3. A granulometria do resíduo de mármore apresentou um tamanho de grão médio igual 42,810 µm. Já, na borra de alumínio, o tamanho médio foi de 101,803 µm. A lama fina de aciaria LD apresentou, em torno de 54,7% de sua granulometria, entre 0,15 e 0,075mm. Esses resultados apontam para a viabilidade técnica da utilização desses materiais na dessulfuração e desfosforação do ferro-gusa.