4 resultados para aluminum alloy
em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo
Resumo:
A 7.4 mm thick strip of 3003 aluminum alloy produced by the industrial twin-roll casting (TRC) process was homogenized at 500 °C for 12 hours, after which it was cold rolled in two conditions: 1) to reduce the strip's thickness by 67%, and 2) to reduce it by 91%. The alloy was annealed at 400 °C for 1 hour in both conditions. The results revealed that a rotated cube texture, the {001}<110> component, predominated in the as-cast condition and was transformed into brass, copper and S type textures during the cold rolling process. There was practically no difference between the deformation textures at the two thickness reductions.
Resumo:
The fatigue crack behavior in metals and alloys under constant amplitude test conditions is usually described by relationships between the crack growth rate da/dN and the stress intensity factor range Delta K. In the present work, an enhanced two-parameter exponential equation of fatigue crack growth was introduced in order to describe sub-critical crack propagation behavior of Al 2524-T3 alloy, commonly used in aircraft engineering applications. It was demonstrated that besides adequately correlating the load ratio effects, the exponential model also accounts for the slight deviations from linearity shown by the experimental curves. A comparison with Elber, Kujawski and "Unified Approach" models allowed for verifying the better performance, when confronted to the other tested models, presented by the exponential model. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
The aims of this work are: (i) to produce new experimental data for fretting fatigue considering the presence of a mean bulk stress and (ii) to assess two design methodologies against failure by fretting fatigue. Tests on a cylinder–flat contact configuration were conducted using a fretting apparatus mounted on a servo-hydraulic machine. The material used for both the pads and fatigue specimen was an aeronautical 7050-T7451 Al alloy. The experimental program was designed with all relevant parameters, apart from the mean bulk load (always applied before the contact loads), kept constant. The mean bulk stress varied from compressive to tensile values while maintaining a high peak pressure in order to encourage crack initiation. Two methodologies against fretting fatigue are proposed and confronted against the experimental data. The non-local stress-based methodology considers the evaluation of a critical plane fatigue criterion at the center of a process zone located beneath the contacting surfaces. The results showed that it correctly predicts crack initiation, but was not capable to provide successful prediction of the integrity of the specimens. Alternatively, we considered a crack arrest criterion which has the potential to provide a more complete description about the integrity of the specimens.
Resumo:
In recent years, different beta titanium alloys have been developed for biomedical applications with a combination of mechanical properties including a low Young's modulus, high strength, fatigue resistance and good ductility with excellent corrosion resistance. From this perspective, a new metastable beta titanium Ti-12Mo-3Nb alloy was developed with the replacement of both vanadium and aluminum from the traditional Ti-6Al-4V alloy. This paper presents the microstructure, mechanical properties and corrosion resistance of the Ti-12Mo-3Nb alloy heat-treated at 950 degrees C for 1 h. The material was characterized by X-ray diffraction and by scanning electron microscopy. Tensile tests were carried out at room temperature. Corrosion tests were performed using Ringer's solution at 25 degrees C. The results showed that this alloy could potentially be used for biomedical purposes due to its good mechanical properties and spontaneous passivation. (c) 2011 Elsevier B.V. All rights reserved.