Resumo:

The egg surface structure of Thalassophryne amazonica, a freshwater toadfish from the Amazon basin is described. Eggs of this species show a remarkable, highly unusual system of parallel ridges and intermittent grooves that originate at the equator of the egg and lead to the micropylar pit, at which they end in a spiralling pattern. A similar egg surface structure has so far been described only from a group of Asian anabantoid percomorphs, obviously not closely related to Thalassophryne. This egg surface pattern may enhance fertilization success by guiding sperm to the micropyle. We review museum records for T amazonica, present an updated map of its occurrence in the Amazon basin, and provide information on its habitat.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Aim To compare the changes in the surface structure and elemental distribution, as well as the percentage of ion release, of four calcium silicate-containing endodontic materials with a well-established epoxy resin-based sealer, submitted to a solubility test. Methodology Solubility of AH Plus, iRoot SP, MTA Fillapex, Sealapex and MTA-Angelus (MTA-A) was tested according to ANSI/ADA Specification 57. The deionized water used in the solubility test was submitted to atomic absorption spectrophotometry to determine and quantify Ca2+, Na+, K+, Zn2+, Ni2+ and Pb2+ ions release. In addition, the outer and inner surfaces of nonsubmitted and submitted samples of each material to the solubility test were analysed by means of scanning electron microscopy and energy-dispersive spectroscopy (SEM/EDX). Statistical analysis was performed by using one-way anova and Tukeys post hoc tests (a = 0.05). Results Solubility results, in percentage, sorted in an increasing order were -1.24 +/- 0.19 (MTA-A), 0.28 +/- 0.08 (AH Plus), 5.65 +/- 0.80 (Sealapex), 14.89 +/- 0.73 (MTA Fillapex) and 20.64 +/- 1.42 (iRoot SP). AH Plus and MTA-A were statistically similar (P > 0.05), but different from the other materials (P < 0.05). High levels of Ca2+ ion release were observed in all groups except AH Plus sealer. MTA-A also had the highest release of Na2+ and K+ ions. Zn+2 ion release was observed only with AH Plus and Sealapex sealers. After the solubility test, all surfaces had morphological changes. The loss of matrix was evident and the filler particles were more distinguishable. EDX analysis displayed high levels of calcium and carbon at the surface of Sealapex, MTA Fillapex and iRoot SP. Conclusions AH Plus and MTA-A were in accordance with ANSI/ADAs requirements regarding solubility whilst iRoot SP, MTA Fillapex and Sealapex did not fulfil ANSI/ADAs protocols. High levels of Ca2+ ion release were observed in all materials except AH Plus. SEM/EDX analysis revealed that all samples had morphological changes in both outer and inner surfaces after the solubility test. High levels of calcium and carbon were also observed at the surface of all materials except AH Plus and MTA-A.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

We investigated the electrochemical oxidation of glycerol on low-index Pt single crystals in acidic media (H2SO4 and HClO4) by cyclic voltammetry and Fourier Transform Infrared (FTIR) spectroscopy and we verified that this is a surface sensitive reaction. Pt(100) and Pt(110) surface structures favor the breaking of the C-C-C bond at low potentials (say 0.05 V), as seen by the formation of CO, one of the adsorbed residues of the glycerol dissociation, which poisons these surfaces even at high potentials. Pt(111) surface structure does not favor the C-C-C bond breaking at potentials as low as 0.05 V. However, Pt(111) is less poisoned by residues of glycerol dissociation and, for this reason, it is more active for glycerol oxidation than Pt(100) and Pt(110) at low potentials. Carbonyl containing compounds and CO2 were detected as reaction products of the glycerol oxidation on all investigated single-crystal Pt surfaces. The ratio between CO2 and carbonyl containing compounds is clearly much higher for Pt(100) and Pt(110) than for Pt(111). (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

By means of in situ IR spectroscopy we investigate the effect of dissolved alkali cations on the electro-oxidation of ethylene glycol on platinum in alkaline media. The results revealed that the increase in the oxidation currents (Li(+) < Na(+) < K(+)) is reflected in the increase in the ratio between carbonate and oxalate produced.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In this paper we present results on the electro-oxidation of ethanol on unsupported (carbon free) platinum nanoparticles, considering the effects of the alcohol concentration. The case of the so-called dual pathway mechanism during the electro-oxidation of ethanol showed to be influenced by the surface coverage of adsorbed carbon monoxide (COad) at unsupported platinum. The influences of adsorbed intermediates were followed by in situ infrared spectroscopy (FTIR) and by electrochemical experiments. Unsupported platinum showed that the reaction leads to the formation of CO2 and acetic acid as main products at low concentrations of ethanol (0.01 to 0.1 mol L-1). At least in this case of 0.01 mol L-1 ethanol, most formation of CO2 occurred via COad (indirect pathway). At higher concentration of ethanol, however, most CO2 was formed via a reactive intermediate such as acetaldehyde (direct pathway). In addition, in this higher concentration of ethanol, the acetic acid was produced via formation of adsorbed acetaldehyde (via acetate) at higher overpotentials. In case of the acetic acid formation, a dual pathway was identified during the electro-oxidation of ethanol at low alcohol concentrations, whereas a parallel pathway occurred without the formation of adsorbed acetate intermediates at low overpotentials. (C) 2012 The Electrochemical Society. [DOI: 10.1149/2.101203jes] All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Purpose: Dyslipidemia is characterized by high lipid blood levels that are risk factors for cardiovascular diseases, which are leading causes of death. However, it is unclear whether dyslipidemia is a cause of the dry eye syndrome (DES). Therefore we determined in transgenic mice models of dyslipidemia, whether there is an association with DES development. Methods: Dyslipidemic models included male and female adult mice overexpressing apolipoprotein CIII (Apo CIII), LDL receptor knockout (LDLR-KO) and ApoE knockout (ApoE-KO). They were compared with age-and gender-matched C57BL/6 mice. Ocular health was evaluated based on corneal slit lamp assessment, phenol red thread test (PRT) and impression cytology. Blood lipid profiles and histology of meibomian and lacrimal glands were also evaluated. Effects of high-fat diet and aging were observed in LDLR-KO and ApoCIII strains, respectively. Results: Body weight and lacrimal gland weight were significantly higher in male mice compared to females of the same strain (P < 0.05). Body weight was significantly lower in LDLRKO mice receiving high lipid diet compared to their controls (P = 0.0043). ApoE-KO were hypercholesterolemic and ApoCIII hypertriglyceridemic while LDLR-KO showed increases in both parameters. The PRT test was lower in male LDLR-KO mice with high-fat diet than control mice with standard diet (P = 0.0273). Aging did not affect lacrimal structural or functional parameters of ApoCIII strain. Conclusions: DES development is not solely dependent on dyslipidemia in relevant mice models promoting this condition. On the other hand, lacrimal gland structure and function are differentially impacted by lipid profile changes in male and female mice. This dissociation suggests that other factors beside dyslipidemia impact on tear film dysfunction and DES development.