BACKGROUND: Genetically modified MON 87701 X MON 89788 soybean (Glycine max), which expresses the Cry1Ac and EPSP-synthase proteins, has been registered for commercial use in Brazil. To develop an Insect Resistance Management (IRM) program for this event, laboratory and field studies were conducted to assess the high-dose concept and level of control it provides against Anticarsia gemmatalis and Pseudoplusia includens. RESULTS: The purified Cry1Ac protein was more active against A. gemmatalis [LC50 (FL 95%) = 0.23 (0.150.34) mu g Cry1Ac mL-1 diet] than P. includens [LC50 (FL 95%) = 3.72 (2.654.86) mu g Cry1Ac mL-1 diet]. In bioassays with freeze-dried MON 87701X MON 89788 soybean tissue diluted 25 times in an artificial diet, there was 100% mortality of A. gemmatalis and up to 95.79% mortality for P. includens. In leaf-disc bioassays and under conditions of high artificial infestation in the greenhouse and natural infestation in the field, MON 87701X MON 89788 soybean showed a high level of efficacy against both target pests. CONCLUSIONS: The MON 87701X MON 89788 soybean provides a high level of control against A. gemmatalis and P. includes, but a high-dose event only to A. gemmatalis. Copyright (c) 2012 Society of Chemical Industry
Resumo:
The peptidolytic enzyme THIMET-oligopeptidase (TOP) is able to act as a reducing agent in the peroxidase cycle of myoglobin (Mb) and horseradish peroxidase (HRP). The TOP-promoted recycling of the high valence states of the peroxidases to the respective resting form was accompanied by a significant decrease in the thiol content of the peptidolytic enzyme. EPR (electron paramagnetic resonance) analysis using DBNBS spin trapping revealed that TOP also prevented the formation of tryptophanyl radical in Mb challenged by H2O2. The oxidation of TOP thiol groups by peroxidases did not promote the inactivating oligomerization observed in the oxidation promoted by the enzyme aging. These findings are discussed towards a possible occurrence of these reactions in cells.
Resumo:
In this work, the effect of the indentation load on the results of hardness and fracture toughness, determined by Vickers micro-hardness measurements, of some glasses and glass-ceramics has been investigated. Furthermore, in order to verify the effect of crystallinity on the results, glasses of composition 52.75 wt.% 3CaO center dot P2O5, 30 wt.% SiO2 and 17.25 wt.% MgO were fused at 1600 degrees C for 4 h and annealed at 700 degrees C for 2h, and further heat-treated at 700, 775, 800 and 900 degrees C for 4h. The obtained materials were analyzed by high resolution X-ray diffraction, HRXRD, to determine the crystallization degree in function of the heat-treatment temperature. The hardness of the different specimens was determined by Vickers' micro-hardness measurements under various loads. It has been observed that with increasing crystallization of the materials their hardness increased. Furthermore, it has been possible to verify the so-called indentation size effect (ISE), i.e. hardness decreases as the indentation depth, under higher loads, increases. This effect has been more pronounced in the glass-ceramic samples. Fracture toughness has been determined by the crack length induced by the Vickers indentations and relating them to the applied loads. Glass materials presented a fracture pattern with characteristics of cleavage, forming cracks of the half-penny shaped type, while the glass-ceramic materials exhibited crack bridging effects and Palmqvist type cracks. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The numerical simulation of flows of highly elastic fluids has been the subject of intense research over the past decades with important industrial applications. Therefore, many efforts have been made to improve the convergence capabilities of the numerical methods employed to simulate viscoelastic fluid flows. An important contribution for the solution of the High-Weissenberg Number Problem has been presented by Fattal and Kupferman [J. Non-Newton. Fluid. Mech. 123 (2004) 281-285] who developed the matrix-logarithm of the conformation tensor technique, henceforth called log-conformation tensor. Its advantage is a better approximation of the large growth of the stress tensor that occur in some regions of the flow and it is doubly beneficial in that it ensures physically correct stress fields, allowing converged computations at high Weissenberg number flows. In this work we investigate the application of the log-conformation tensor to three-dimensional unsteady free surface flows. The log-conformation tensor formulation was applied to solve the Upper-Convected Maxwell (UCM) constitutive equation while the momentum equation was solved using a finite difference Marker-and-Cell type method. The resulting developed code is validated by comparing the log-conformation results with the analytic solution for fully developed pipe flows. To illustrate the stability of the log-conformation tensor approach in solving three-dimensional free surface flows, results from the simulation of the extrudate swell and jet buckling phenomena of UCM fluids at high Weissenberg numbers are presented. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
The construction industry is one of the greatest sources of pollution because of the high level of energy consumption during its life cycle. In addition to using energy while constructing a building, several systems also use power while the building is operating, especially the air-conditioning system. Energy consumption for this system is related, among other issues, to external air temperature and the required internal temperature of the building. The facades are elements which present the highest level of ambient heat transfer from the outside to the inside of tall buildings. Thus, the type of facade has an influence on energy consumption during the building life cycle and, consequently, contributes to buildings' CO2 emissions, because these emissions are directly connected to energy consumption. Therefore, the aim is to help develop a methodology for evaluating CO2 emissions generated during the life cycle of office building facades. The results, based on the parameters used in this study, show that facades using structural glazing and uncolored glass emit the most CO2 throughout their life cycle, followed by brick facades covered with compound aluminum panels or ACM (Aluminum Composite Material), facades using structural glazing and reflective glass and brick facades with plaster coating. On the other hand, the typology of facade that emits less CO2 is brickwork and mortar because its thermal barrier is better than structural glazing facade and materials used to produce this facade are better than brickwork and ACM. Finally, an uncertainty analysis was conducted to verify the accuracy of the results attained. (C) 2011 Elsevier Inc. All rights reserved.