10 resultados para Flash-sintering
em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo
Resumo:
Doped barium cerate is a promising solid electrolyte for intermediate temperature fuel cells as a protonic conductor. However, it is difficult to sinter it to high density at a reasonable temperature. Moreover, it presents a high grain boundary resistivity at intermediate temperatures. Flash grain welding was applied to compacted samples, starting from a temperature of 910 degrees C and applying, for a short time, an ac electric polarization of 40 V, 1000 Hz. At that frequency, the resulting current flows through the grain boundaries promoting a welding via a local Joule heating. A large decrease of the grain boundary resistivity was observed by impedance spectroscopy. Scanning electron microscopy observations of polished and etched surfaces revealed highly sintered regions. Attempts were also made to combine flash grain welding with conventional sintering. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Nanostructured Pb0.90Ba0.10Zr0.40Ti0.60O3 dense ceramics presenting an average grain size of 62 +/- 5 nm was prepared by the polymeric precursor method and using the spark plasma sintering technique. The dielectric permittivity curves versus temperature exhibit broad anomaly, indicative of a diffuse phase transition. This result can be explained by the spread of Curie temperatures which are expected to depend on the degree of tetragonality related to the grain size distribution. A pronounced decrease in the maximum of the dielectric permittivity value is attributed to the existence of a large amount of grain boundaries which are non-ferroelectric regions.
Resumo:
The spark plasma sintering (SPS) technique, by using a compacting pressure of 50 MPa, was used to consolidate pre-reacted powders of Bi1.65Pb0.35Sr2Ca2Cu3O10+delta (Bi-2223). The influence of the consolidation temperature, T-D, on the structural and electrical properties has been investigated and compared with those of a reference sample synthesized by the traditional solid-state reaction method and subjected to the same compacting pressure. From the X-ray diffraction patterns, performed in both powder and pellet samples, we have found that the dominant phase is the Bi-2223 in all samples but traces of the Bi2Sr2CaCu2O8+x (Bi-2212) were identified. Their relative density were similar to 85% of the theoretical density and the temperature dependence of the electrical resistivity, rho(T), indicated that increasing T-D results in samples with low oxygen content because the SPS is performed in vacuum. Features of the rho(T) data, as the occurrence of normal-state semiconductor-like behavior of rho(T) and the double resistive superconducting transition, are consistent with samples comprised of grains with shell-core morphology in which the shell is oxygen deficient. The SPS samples also exhibited superconducting critical current density at 77 K, J(c)(77K), between 2 and 10A/cm(2), values much smaller than similar to 22A/cm(2) measured in the reference sample. Reoxygenation of the SPS samples, post-annealed in air at different temperatures and times, was found to improve their microstructural and transport properties. Besides the suppression of the Bragg peaks belonging to the Bi-2212 phase, the superconducting properties of the post-annealed samples and particularly J(c)(77K) were comparable or better than those corresponding to the reference sample. Post-annealed samples at 750 degrees C for 5min exhibited J(c)(77K) similar to 130A/cm(2) even when uniaxially pressed at only 50 MPa. (C) 2012 American Institute of Physics. [http://dx.doi.org/10.1063/1.4768257]
Resumo:
Boiling points (T-B) of acyclic alkynes are predicted from their boiling point numbers (Y-BP) with the relationship T-B(K) = -16.802Y(BP)(2/3) + 337.377Y(BP)(1/3) - 437.883. In turn, Y-BP values are calculated from structure using the equation Y-BP = 1.726 + A(i) + 2.779C + 1.716M(3) + 1.564M + 4.204E(3) + 3.905E + 5.007P - 0.329D + 0.241G + 0.479V + 0.967T + 0.574S. Here A(i) depends on the substitution pattern of the alkyne and the remainder of the equation is the same as that reported earlier for alkanes. For a data set consisting of 76 acyclic alkynes, the correlation of predicted and literature T-B values had an average absolute deviation of 1.46 K, and the R-2 of the correlation was 0.999. In addition, the calculated Y-BP values can be used to predict the flash points of alkynes.
Resumo:
Zirconium tin titanate (ZST) is often used as a dielectric resonator for the fabrication of microwave devices. Pure compositions do not sinter easily by solid state sintering; therefore, sintering ZST requires sintering aids capable of creating defects that could improve diffusion processes and/or promote liquid phase sintering. The mechanisms by which the additives influence the microstructure and, consequently, the ZSTs dielectric properties are not very clear. The effects of ZnO, Bi2O3, and La2O3, on the stoichiometry and dielectric properties of ZST sintered at different temperatures were investigated in this study.
Resumo:
Boiling points (T B) of acyclic alkynes are predicted from their boiling point numbers (Y BP) with the relationship T B(K) = -16.802Y BP2/3 + 337.377Y BP1/3 - 437.883. In turn, Y BP values are calculated from structure using the equation Y BP = 1.726 + Ai + 2.779C + 1.716M3 + 1.564M + 4.204E3 + 3.905E + 5.007P - 0.329D + 0.241G + 0.479V + 0.967T + 0.574S. Here Ai depends on the substitution pattern of the alkyne and the remainder of the equation is the same as that reported earlier for alkanes. For a data set consisting of 76 acyclic alkynes, the correlation of predicted and literature T B values had an average absolute deviation of 1.46 K, and the R² of the correlation was 0.999. In addition, the calculated Y BP values can be used to predict the flash points of alkynes.
Resumo:
Ba0.77Ca0.23TiO3 ceramics were produced in this work starting from nanopowders synthesized via a polymeric precursor method. By adjusting the pH values of the precursor solutions above 7, it was possible to prepare powders weakly aggregated and with a smaller particle size, both facts which traduced into an enhanced nanopowders' sintering process at comparatively lower temperatures. Irrespective of the initial pH value, highly-dense and second phase-free ceramics were obtained following optimal sintering parameters (temperature and time) extracted from dilatometric and density measurements. By considering these and other sintering conditions, moreover, polycrystalline materials with an average grain size varying from 0.35 to 8 mm were produced, the grain growth process involving liquid phase-assisted sintering for heat treatments achieved at 1320 °C. The study of grain size effects on the ferroelectric properties of these materials was conducted, the results being discussed in the light of previous debates, including grain size-dependent degree of tetragonal distortion in such materials, as verified in this work.
Resumo:
Recently, a new ternary phase was discovered in the Ti-Si-B system, located near the Ti6Si2B composition. The present study concerns the preparation of titanium alloys that contain such phase mixed with α-titanium and other intermetallic phases. High-purity powders were initially processed in a planetary ball-mill under argon atmosphere with Ti-18Si-6B and Ti-7.5Si-22.5B at. (%) initial compositions. Variation of parameters such as rotary speed, time, and ball diameters were adopted. The as-milled powders were pressureless sintered and hot pressed. Both the as-milled and sintered materials were characterized by X-ray diffraction, scanning electron microscopy and energy-dispersive spectrometry. Sintered samples have presented equilibrium structures formed mainly by the α-Ti+Ti6Si2B+Ti5Si3+TiB phases. Silicon and boron peaks disappear throughout the milling processes, as observed in the powder diffraction data. Furthermore, an iron contamination of up to 10 at. (%) is measured by X-ray spectroscopy analysis on some regions of the sintered samples. Density, hardness and tribological results for these two compositions are also presented here.
Resumo:
Cutting tools with higher wear resistance are those manufactured by powder metallurgy process, which combines the development of materials and design properties, features of shape-making technology and sintering. The annual global market of cutting tools consumes about US$ 12 billion; therefore, any research to improve tool designs and machining process techniques adds value or reduces costs. The aim is to describe the Spark Plasma Sintering (SPS) of cutting tools in functionally gradient materials, to show this structure design suitability through thermal residual stress model and, lastly, to present two kinds of inserts. For this, three cutting tool materials were used (Al2O3-ZrO2, Al2O3-TiC and WC-Co). The samples were sintered by SPS at 1300 °C and 70 MPa. The results showed that mechanical and thermal displacements may be separated during thermal treatment for analysis. Besides, the absence of cracks indicated coherence between experimental results and the residual stresses predicted.