The effect of CO2 continuous laser irradiation on the surface properties of veneering porcelains has already been tested. The surface observed after laser irradiation is similar to that achieved by auto-glaze in terms of roughness and color parameters (Sgura R, et al. Dental Materials 2011;27(Suppl. 1):e72–73). The purpose of this study was to analyze the surface porosity of porcelain discs after CO2 laser treatment and compare it to auto-glaze treatment, in furnace. A morphological analysis of the porcelain surface was conducted using atomic force microscopy (AFM) and conventional optical microscopy (OM).
Resumo:
Diferentes fatores devem ser considerados nos casos de substituição de restaurações em dentes anteriores, tais como tratamento periodontal e tipo de material utilizado. Nessas situações, uma abordagem multidisciplinar é fundamental. Pacientes com resinas antigas próximas à margem gengivaI normalmente apresentam inflamação do tecido nessa região; por esse motivo, uma adequação prévia é fundamental para o sucesso do tratamento restaurador. Além disso, cuidados na substituição dessas restaurações devem ser considerados pelo profissional e pelo paciente. Os laminados cerâmicos têm sido amplamente utilizados em dentes anteriores; no entanto, esse tratamento deve ser indicado em situações específicas, de tal forma que seja o mais conservador possível. Assim, o presente trabalho demonstra, por meio de um caso clínico, a associação da Periodontia e Dentística na substituição de resinas compostas por laminados cerâmicos, de forma conservadora.
Resumo:
The purpose of the study was to verify the effects of a number of materials' parameters (crystalline content; Young's modulus, E; biaxial flexure strength, sigma(i); Vickers hardness, VH; fracture toughness, K-Ic; fracture surface energy, gamma(f); and index of brittleness, B) on the brittleness of dental ceramics. Five commercial dental ceramics with different contents of glass phase and crystalline particles were studied: a vitreous porcelain (VM7/V), a porcelain with 16 vol% leucite particles (d.Sign/D), a glass-ceramic with 29 vol% leucite particles (Empress/E1), a glass-ceramic with 58 vol% lithium-disilicate needle-like particles (Empress 2/E2), and a glass-infiltrated alumina composite with 65 vol% crystals (In-Ceram Alumina/IC). Discs were constructed according to manufacturers' instructions, ground and polished to final dimensions (12 mm x 1.1 mm). Elastic constants were determined by ultrasonic pulse-echo method. sigma(i) was determined by piston-on-3-balls method in inert condition. VH was determined using 19.6 N load and K-Ic was determined by indentation strength method. gamma(f) was calculated from the Griffith-Irwin relation and B by the ratio of HV to K-Ic. IC and E2 showed higher values of sigma(i), E, K-Ic and gamma(f), and lower values of B compared to leucite-based glass-ceramic and porcelains. Positive correlations were observed for sigma(i) versus K-Ic, and K-Ic versus E-1/2, however, E did not show relationship with HV and B. The increase of crystalline phase content is beneficial to decrease the brittleness of dental ceramics by means of both an increase in fracture surface energy and a lowering in index of brittleness. (C) 2012 Elsevier Ltd and Techna Group Sri. All rights reserved.
Resumo:
Aim. This work tested the effect of the addition of Al2O3/GdAlO3 longitudinal fibers in different contents to veneering porcelain of two dental all ceramic systems. Methods: Fibers (0.5 mm diameter) obtained by the Laser Heated Pedestal Growth (LHPG) method were added to bar-shaped specimens made by veneer porcelain (monolayers) or both the veneer and the core ceramic (bilayers) of two all-ceramic systems: In-Ceram Alumina - glass infiltrated alumina composite (GIA) and In-Ceram 2000 AL Cubes - alumina polycrystal (AP) (VITA Zahnfabrik). The longitudinal fibers were added to veneering porcelain (VM7) in two different proportions: 10 or 17 vol%. The bars were divided into nine experimental conditions (n = 10) according to material used: VM7 porcelain monolayers, VM7/GIA, VM7/AP; and according to the amount of fibers within the porcelain layer: no fibers, 10 vol% or 17 vol%. After grinding and polishing the specimens were submitted to a three point bending test (crosshead speed = 0.5 mm/min) with porcelain positioned at tensile side. Data were analyzed by means of one-way ANOVA and a Tukey's test (alpha = 5%). Scanning electronic microscopy (SEM) was conducted for fractographic analysis. Results. Regarding the groups without fiber addition, VM7/AP showed the highest flexural strength (MPa), followed by VM7/GIA and VM7 monolayers. The addition of fibers led to a numerical increase in flexural strength for all groups. For VM7/GIA bilayers the addition of 17 vol% of fibers resulted in a significant 48% increase in the flexural strength compared to the control group. Fractographic analysis revealed that the crack initiation site was in porcelain at the tensile surface. Cracks also propagated between fibers before heading for the alumina core. Conclusions. The addition of 17 vol% of Al2O3/GdAlO3 longitudinal fibers to porcelain/glass infiltrated alumina bilayers significantly improved its flexural strength. 10 vol% or 17 vol% of fibers inclusion increased the flexural strength for all groups. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
This article evaluates the long-term clinical performance of porcelain laminate veneers bonded to teeth prepared with the use of an additive mock-up and aesthetic pre-evaluative temporary (APT) technique over a 12-year period. Sixty-six patients were restored with 580 porcelain laminate veneers. The technique, used for diagnosis, esthetic design, tooth preparation, and provisional restoration fabrication, was based on the APT protocol. The influence of several factors on the durability of veneers was analyzed according to pre- and postoperative parameters. With utilization of the APT restoration, over 80% of tooth preparations were confined to the dental enamel. Over 12 years, 42 laminate veneers failed, but when the preparations were limited to the enamel, the failure rate resulting from debonding and microleakage decreased to 0%. Porcelain laminate veneers presented a successful clinical performance in terms of marginal adaptation, discoloration, gingival recession, secondary caries, postoperative sensitivity, and satisfaction with restoration shade at the end of 12 years. The APT technique facilitated diagnosis, communication, and preparation, providing predictability for the restorative treatment. Limiting the preparation depth to the enamel surface significantly increases the performance of porcelain laminate veneers. (Int J Periodontics Restorative Dent 2012;32:625-635.)