Resumo:
In this work, a ruthenium hexafluorophosphate complex, [Ru(bpy)(3)](PF6)(2) in poly(methylmethacrylate) (PMMA) was employed to build a single layer light electrochemical cell on indium tin oxide polyester flexible substrate. The electroluminescence spectrum features a relatively broad band peaked near 625 run, with CIE (x,y) color coordinates of (0.61,0.39). The driving voltage is only 3 V, and for the maximum electrical current of 10 mA the brightness reaches 1 cd/m(2). Regarding the useful application of the device, its opto-electrical behavior under mechanical strain was studied considering the central curvature. In these situations, both electrical characterization in DC mode and luminance were analyzed. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
This work shows a comparative study of organic light emitting diodes based on four different europium complexes with the general formula, Eu(CLs)(3)bipyridine, where the central ligands are DBM [tris(dibenzoylmethane)], TTA [tris(1-(2-thieneyl)-4,4,4-trifluoro-1,3-butanedione)], NTA [tris(1-(2-naphthoyl)-3,3,3-trifluoroacetone)] and BTA [tris(1-(2-benzoyl)-3,3,3-trifluoroacetone)]. All devices have a driving voltage of 14-16 V, a very low electrical current at normal operation (less than 1 mA) and a good Wall Plug Efficiency (up to near 10(-3)%). The most suitable central ligand was found to be DBM, with an optical power up to 200 nW (at 612 nm). The BTA exhibits the lowest stability under high applied voltages. The other central ligands have similar results among them. The electroluminescence spectra clearly show the europium ion transitions (with a strong (5)D(0) -> (7)F(2) line) with a CIE color coordinate around (0.56, 0.34). (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
In this work, two ruthenium complexes, [Ru(bpy)(3)](PF6)(2) and [Ru(ph2phcn)(3)](PF6)(2) in poly(inethylinethacrylate) matrix were employed to build single-layer light-emitting electrochemical cells by spin coating on indium tin oxide substrate. In both cases the electroluminescence spectra exhibit a relatively broad band with maxima near to 625 rim and CIE (x, y) color coordinates of (0.64, 0.36), which are comparable with the photoluminescence data in the same medium. The best result was obtained with the [Ru(bpy)(3)](PF6)(2) device where the optical output power approaches 10 mu W at the band maximum with a wall-plug efficiency higher than 0.03%. The lowest driving voltage is about 4 V for an electrical current of 20 mA. (c) 2008 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
Poly(vinyl butyral)-polyaniline-sodium montmorillonite nanocomposites were prepared via polymerization of aniline between clay mineral platelets at two different pH levels (2.0 and 5.0), followed by dispersion of the polyaniline-sodium montmorillonite nanocomposite in a poly(vinyl butyral) solution. A comparison was made of the effect of the pH levels and the polyaniline-sodium montmorillonite nanocomposite precursor on the final structures of the poly(vinyl butyral) nanocomposites and their electrical conductivities. X-ray diffraction patterns revealed the formation of nanocomposites at both pH levels. UV-Vis spectra indicated that the polyaniline formed at both pH levels was conductive, with the UV-Vis spectra presenting a band at 420 nm corresponding to the polaronic form and the beginning of a new band at 600 nm indicating the presence of polaronic segments. FTIR spectra revealed the peaks of the groups present in polyaniline and poly(vinyl butyral) nanocomposites. The electrical conductivities of the polyaniline and poly(vinyl butyral) nanocomposites prepared at pH 2.0 were lower than those of the same nanocomposites prepared at pH 5.0, probably due to the lower formation of polyaniline chains in a more acidic dispersion and to the final configuration of polyaniline in the nanocomposites.
Resumo:
O objetivo foi analisar os atendimentos por queimaduras em serviços de emergência, e fatores associados. Estudo transversal de 761 atendimentos coletados pelo Sistema de Vigilância de Violências e Acidentes em 2009. A maioria foi do sexo masculino (58,6%); adultos de 30 a 49 anos (23,1%) e crianças de 0 a 9 anos (23%). A residência foi o local de ocorrência mais frequente (62,1%), especialmente para crianças e mulheres; em seguida comércio, serviços, indústria e construção (19,1%), especialmente entre homens de 20 a 49 anos. Queimaduras no trabalho foram 29,1% do total. Uso de álcool chegou a 5,1%. Agentes causadores em todas as idades: substância quente (43,6%) e fogo/chama (24,2%); na faixa produtiva: substâncias químicas. As queimaduras entre 0 e 14 anos foram associadas com residência, substância e objeto quente e internação hospitalar; entre os de 15 a 49 anos associaram-se com fogo/chama e choque elétrico, via pública e alta da emergência. Estratégias de prevenção para crianças e trabalhadores devem ser implantadas.
Resumo:
The influence of deposition parameters, namely polymer concentration and pH of the deposition solution, cleaning, and drying steps on the morphology and electrical characteristics of polyaniline and sulfonated polystyrene (PANI/PSS) nanostructured films deposited by the self-assembly technique is evaluated by UV-Vis spectroscopy, optical and atomic force microscopy, and electrical resistance measurements. It is found that stirring the cleaning solution during the cleaning step is crucial for obtaining homogenous films. Stirring of the cleaning solution also influences the amount of PANI adsorbed in the films. In this regard, the drying process seems to be less critical since PANI amount and film thickness are similar in films dried with N-2 flow or with an absorbent tissue. It is observed, however, that drying with N-2 flow results in rougher films. As an additional point, an assessment of the influence of the deposition method (manual versus mechanical) on the film characteristics was carried out. A significant difference on the amount of PANI and film thickness between films prepared by different human operators and by a homemade mechanical device was observed. The variability in film thickness and PANI adsorbed amount is smaller in films mechanically assembled. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
The complete I-V characteristics of SnO(2)-based varistors, particularly of the Pianaro system SCNCr consisting in 98.9%SnO(2)+1%CoO+0.05%Nb(2)O(5)+0.05%Cr(2)O(3), all in mol%, have been seldom reported in the literature. A comparative study at low and high currents of the nonohmic behavior of SCNCr- and ZnO-based varistors (modified Matsuoka system) is proposed in this work. The SCNCr system showed higher nonlinearity coefficients in the whole range of measured current. The electrical breakdown field (E(b)) was twice as high for the SCNCr system (5400 V/cm) than for the ZnO varistor (2600 V/cm) due to a smaller average grain size of the former (4.5 mu m) with respect to the latter (8.5 mu m). Nevertheless, we consider that another important factor responsible for the high E(b) in the SCNCr system is the great number of electrically active interfaces (85%) as determined with electrostatic force microscopy (EFM). It was also established that the SCNCr system might be produced in disks of smaller dimensions than that of commercial ZnO-based product, with a 5.0 cm(-1) minimal area-volume (A/V) ratio. The SCNCr reached the saturation current in a short time because of the high resistivity of the grains, which is five times higher than that of the grains in ZnO-based varistors.
Resumo:
Ion implantation of metal species into insulators provides a tool for the formation of thin, electrically conducting, surface layers with experimenter-controlled resistivity. High energy implantation of Pt and Ti into alumina accelerator components has been successfully employed to control high voltage surface breakdown in a number of cases. In the work described here we have carried out some basic investigations related to the origin of this phenomenon. By comparison of the results of alumina implanted with Ti at 75 keV with the results of prior investigations of polymers implanted with Pt at 49 eV and Au at 67 eV, we describe a physical model of the effect based on percolation theory and estimate the percolation parameters for the Ti-alumina composite. We estimate that the percolation dose threshold is about 4 x 10(16) cm(-2) and the maximum dose for which the system remains an insulator-conductor composite is about 10 x 10(16) cm(-2). The saturation electrical conductivity is estimated to be about 50 S/m. We conclude that the observed electrical conductivity properties of Ti-implanted alumina can be satisfactorily described by percolation theory. (C) 2012 American Institute of Physics. [http://dx.doi.org/10.1063/1.3697900]
Resumo:
The effects of substituting Si by M4+ cations in soda-lime silica glasses were analyzed by impedance spectroscopy in the frequency range of 1 Hz-1 MHz. The glass composition was (mol%) 22Na(2)O center dot 8CaO center dot 65SiO(2)center dot 5MO(2), M = Si, Ti, Ge, Zr, Sn, and Ce. Although the Na+ concentration in the glasses is constant, the Zr-containing glass exhibits the highest dc conductivity and the lowest activation energy, while the Ce-containing glass exhibits the lowest conductivity. The activation energies obtained experimentally agree with those obtained by a theoretical equation proposed by Anderson and Stuart. The differences in electrical conductivity presented by the several M-containing glasses are attributed to the effect that the M4+ ion has on the mobility of the diffusing Na+ ion. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
Plasticized natural macromolecules-based polymer electrolyte samples were prepared and characterized. The plasticization of chitosonium acetate with glycerol increased the ionic conductivity value from 3.0 x 10(-7) S/cm to 1.1 x 10(-5) S/cm. The conductivity temperature relationship of the samples exhibits either VTF or Arrhenius type depending on the glycerol concentration in the sample. The dielectric studies evidencing the relaxation process in the plasticized sample at low frequency region are due to the electric polarization effect. Moreover, the samples were transparent in the Vis region, showed thermal stability up to 160 degrees C and good surface uniformity.
Resumo:
The development of new procedures for quickly obtaining accurate information on the physiological potential of seed lots is essential for developing quality control programs for the seed industry. In this study, the effectiveness of an automated system of seedling image analysis (Seed Vigor Imaging System - SVIS) in determining the physiological potential of sun hemp seeds and its relationship with electrical conductivity tests, were evaluated. SVIS evaluations were performed three and four days after sowing and data on the vigor index and the length and uniformity of seedling growth were collected. The electrical conductivity test was made on 50 seed replicates placed in containers with 75 mL of deionised water at 25 ºC and readings were taken after 1, 2, 4, 8 and 16 hours of imbibition. Electrical conductivity measurements at 4 or 8 hours and the use of the SVIS on 3-day old seedlings can effectively detect differences in vigor between different sun hemp seed lots.