21 resultados para Biodegradable

em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The concept behind a biodegradable ligament device is to temporarily replace the biomechanical functions of the ruptured ligament, while it progressively regenerates its capacities. However, there is a lack of methods to predict the mechanical behaviour evolution of the biodegradable devices during degradation, which is an important aspect of the project. In this work, a hyper elastic constitutive model will be used to predict the mechanical behaviour of a biodegradable rope made of aliphatic polyesters. A numerical approach using ABAQUS is presented, where the material parameters of the model proposal are automatically updated in correspondence to the degradation time, by means of a script in PYTHON. In this method we also use a User Material subroutine (UMAT) to apply a failure criterion base on the strength that decreases according to a first order differential equation. The parameterization of the material model proposal for different degradation times were achieved by fitting the theoretical curves with the experimental data of tensile tests on fibres. To model all the rope behaviour we had considered one step of homogenisation considering the fibres architectures in an elementary volume. (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The influence of glycerol concentration (C-g), process temperature (T-p), drying temperature (T-s), and relative humidity (RH) on the properties of achira flour films was initially assessed. The optimized process conditions were C-g of 17g glycerol/100g flour, T-p of 90 degrees C, T-s of 44.8 degrees C, and RH of 36.4%. The films produced under these conditions displayed high mechanical strength (7.0 MPa), low solubility (38.3%). and satisfactory elongation values (14.6%). This study showed that achira flour is a promising source for the development of biodegradable films with good mechanical properties, low water vapor permeability, and solubility compared to films based on other tubers. (c) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this this study, glycerol content and its incorporation method on tensile and barrier properties of biodegradable films (BF) based on cassava starch were analyzed. ANOVA showed that the glycerol incorporation method did not influence the results (P > 0.05), however the glycerol content influenced significantly the tensile and barrier properties of the films (P < 0.05). Films prepared with lower glycerol content presented better tensile and barrier properties than films with higher content. Films were then prepared with addition of clay nanoparticles and their tensile and barrier properties and glass transition temperature were measured. ANOVA indicated that both glycerol and clay nanoparticles influenced significantly the tensile and barrier properties (P < 0.05), diminishing film permeability when clay nanoparticles were present, while the glass transition temperature was not influenced (P > 0.05). (C) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Aims: The long-term clinical performance of drug-eluting stents (DES) coated with biodegradable polymers is poorly known. Methods and results: A total of 274 coronary patients were randomly allocated to paclitaxel-eluting stents, sirolimus-eluting stents, or bare metal stems (2:2:1 ratio). The two DES used the same biodegradable polymers and were identical except for the drug. At three years, the pooled DES population had similar rates of cardiac death or myocardial infarction (9.0% vs. 7.1; p=0.6), but lower risk of repeat interventions (10.0% vs. 29.9%; p<0.01) than controls with bare stents. The cumulative 3-year incidence of definite or probable stent thrombosis in the pooled DES group was 2.3% (first year: 1.8%; second year: 0.4%; third year: zero). There were no significant differences in outcomes between paclitaxel- and sirolimus-eluting stents. Conclusions: The biodegradable-polymer coated DES releasing either paclitaxel or sirolimus were effective in reducing the 3-year rate of re-interventions.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This work addresses the synthesis of carbon nanomaterials (CNMs) by up-cycling common solid wastes. These feedstocks could supersede the use of costly and often toxic or highly flammable chemicals, such as hydrocarbon gases, carbon monoxide, and hydrogen, which are commonly used as feedstocks in current nanomanufacturing processes for CNMs. Agricultural sugar cane bagasse and corn residues, scrap tire chips, and postconsumer polyethylene (PE) and polyethylene terephthalate (PET) bottle shreddings were either thermally treated by sole pyrolysis or by sequential pyrolysis and partial oxidation. The resulting gaseous carbon-bearing effluents were then channeled into a heated reactor. CNMs, including carbon nanotubes, were catalytically synthesized therein on stainless steel meshes. This work revealed that the structure of the resulting CNMs is determined by the feedstock type, through the disparate mixtures of carbon-bearing gases generated when different feedstocks are pyrolyzed. CNM characterization was conducted by scanning and transmission electron microscopy as well as by Raman spectroscopy and by thermogravimetric analysis. Gas chromatography was used to characterize the gases in the synthesis chamber. This work demonstrated an alternative method for efficient manufacturing of CNMs using both biodegradable and nonbiodegradable agricultural and municipal carbonaceous wastes.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Low liquid-solid ratio (LSR) can be used to obtain high-content xylo-oligosaccharide (XOS) spend liquor by hot water pretreatment. Developing a technology based on low LSR results in more efficient water usage in the system and thus in lower capital and operating costs. Xylans from xylan rich agro-industrial waste are abundant hemicellulosic polymers with enormous potential for industrial applications. Currently, freeze-dried xylo-oligosaccharides are used as bio-based polymers and hydrolysates containing high xylose contents are converted to several chemical products. In this study, sugarcane bagasse was treated with water at low LSRs and mild temperatures in order to assess the effects of varying the pretreatment conditions on the xylo-oligosaccharide and xylose concentrations, and use a central composite experimental design to optimize the process parameters. The pretreatments were performed in the ranges temperature: 143.3-176.7 degrees C, time: 20-70 min and LSR: 1 : 1 to 11 : 1 (g g(-1)). The maximum concentrations of xylose and xylan were 13.76 and 36.18 g L-1 (equivalent to 48.29 g L-1 of xylan), respectively, which were achieved by treating bagasse at 170 degrees C for 60 min, with LSR of 3 g g(-1). The amount of xylan removed under these conditions was almost 57%. The soluble xylan consisted mainly of xylo-oligosaccharides (74 wt% of the identified compound in the spent liquor).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This study assess the effects of bioceramic and poly(lactic-co-glycolic acid) composite (BCP/PLGA) on the viability of cultured macrophages and human dental pulp fibroblasts, and we sought to elucidate the temporal profile of the reaction of pulp capping with a composite of bioceramic of calcium phosphate and biodegradable polymer in the progression of delayed dentine bridge after (30 and 60 days) in vivo. Histological evaluation of inflammatory infiltrate and dentin bridge formation were performed after 30 and 60 days. There was similar progressive fibroblast growth in all groups and the macrophages showed viability. The in vivo study showed that of the three experimental groups: BCP/PLGA composite, BCP and calcium hydroxide (Ca(OH)(2)) dentin bridging was the most prevalent (90 %) in the BCP/PLGA composite after 30 days, mild to moderate inflammatory response was present throughout the pulp after 30 days. After 60 days was observed dentine bridging in 60 % and necrosis in 40 %, in both groups. The results indicate that understanding BCP/PLGA composite is biocompatible and by the best tissue response as compared to calcium hydroxide in direct pulp capping may be important in the mechanism of delayed dentine bridge after 30 and 60 days.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Loaded microspheres with a silicon (IV) phthalocyanine derivative (NzPC) acting as a photosensitizer were prepared from polyhydroxybutyrate-co-valerate (PHBHV) and poly(ecaprolactone) (PCL) polymers using the emulsification solvent evaporation method (EE). The aim of our study was to prepare two systems of these biodegradable PHBHV/PCL microspheres. The first one containing only photosensitizer previously incorporated in the PHBHV and poly(ecaprolactone) (PCL) microspheres and the second one with the post magnetization of the DDS with magnetic nanoparticles. Magnetic fluid is successfully used for controlled incorporation of nanosized magnetic particles within the micron-sized template. This is the first time that we could get a successful pos incorporation of nanosized magnetic particles in a previously-prepared polymeric template. This procedure opens a great number of possibilities of post-functionalization of polymeric micro or nanoparticles with different bioactive materials. The NzPC release profile of the systems is ideal for PDT, the zeta potential and the size particle are stable upon aging in time. In vitro studies were evaluated using gingival fibroblastic cell line. The dark citotoxicity, the phototoxicity and the AC magnetic field assays of the as-prepared nanomagnetic composite were evaluated and the cellular viability analyzed by the classical test of MU.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Gelatin-based films containing both Yucca schidigera extract and low concentrations of glycerol (0.25-8.75 g per 100 g protein) were produced by extrusion (EF) and characterized in relation to their mechanical properties and moisture content. The formulations that resulted in either larger or smaller elongation values were used to produce films via both blown extrusion (EBF) and casting (CF) and were characterized with respect to their mechanical properties, water vapor permeability, moisture content, solubility, morphology and infrared spectroscopy. The elongation of the EF films was significantly higher than that of the CF and EBF films. The transversal section possessed a compact, homogeneous structure for all of the films studied. The solubility of the films (36-40%) did not differ significantly between the different processes evaluated. The EBF films demonstrated lower water vapor permeability (0.12 g mm m-(2) h(-1) kPa(-1)) than the CF and EF films. The infrared spectra did not indicate any strong interactions between the added compounds. Thermoplastic processing of the gelatin films can significantly increase their elongation; however, a more detailed assessment and optimization of the extrusion conditions is necessary, along with the addition of partially hydrophobic compounds, such as surfactants. (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The objective of this study was to compare the bone repair along a mandibular body osteotomy stabilized with 2.0 mm absorbable and metallic systems. 12 male, adult mongrel dogs were divided into two groups (metallic and absorbable) and subjected to unilateral osteotomy between the mandibular third and fourth premolars, which was stabilized by applying two 4-hole plates. At 2 and 18 weeks, three dogs from each group were killed and the osteotomy sites were removed and divided equally into three parts: the upper part was labelled the tension third (TT), the lower part the compression third (CT), and the part between the TT and CT the intermediary third (IT). Regardless of the treatment system, union between the fragments was observed at 18 weeks and the CT showed more advanced stages of bone repair than the TT. Histometric analysis did not reveal any significant differences among the 3 parts or systems in the distance between bone fragments at 2 weeks. Although at 18 weeks the proportions of newly formed bone did not differ among TT, IT and CT, significantly enhanced bone formation was observed in all sections for the metallic group. The patterns of repair were distinct between treatments.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this study, we investigated the effects of contaminated water on the blood parameters of the fish Prochilodus lineatus exposed during 7 and 20 days. Blood was collected with heparinized syringes, and blood smears were prepared and stained with Leishman stain. Slides were examined and photographed using a Leica light microscope. Total white blood cell counts and differential counts of thrombocytes and leukocytes were obtained for statistical analysis. The group exposed to water samples from Lago Azul exhibited an increase in the number of leukocytes and in the total number of white blood cells, suggesting that the chemical contaminants in this environment were acting similarly to antigens in this fish species, causing the proliferation of defense cells. In the group exposed to detergent during 20 days, the number of thrombocytes decreased. These results suggest that the variations in the number of leukocytes were indicators of environmental pollution and that biodegradable detergents may, after a certain time of exposure, affect vital functions in fish, such as coagulation and prevention of infections, which directly involves thrombocytes. Microsc. Res. Tech., 2012. (c) 2011 Wiley Periodicals, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Formation of oriented or aligned micro- and nanofibers using biocompatible materials opens the possibility to obtain engineered tissues that can be used in medicine, environmental engineering, security and defense, among other applications. Pectin, a heteropolysaccharide, is a promising material to be incorporated into the fibers because, besides being biocompatible, this material is also biodegradable and bioactive. In this work, the formation of oriented fibers using solutions containing pectin and polyethylene oxide (biocompatible polymers), and chloroform (as the solvent) is investigated. The injection of solution into an intense electric field defined between two parallel electrodes was used to obtain oriented fibers. This novel approach is a modification of the conventional electrospinning process. The presence of pectin in the fibers was confirmed by FTIR analysis. Fibers with diameters of hundreds of nanometers and several centimeters long can be collected. The incorporation of pectin leads to a higher variation of the diameter of the fibers, and a trend to larger fiber diameters. This behavior can be related to the presence of pectin clusters in the fibers. (C) 2012 The Electrochemical Society. [DOI: 10.1149/2.057203jes] All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Nano-biocomposites based on a biodegradable bacterial copolyester, poly(hydroxybutyrate-co-hydroxyvalerate), have been elaborated with an organo-modified montmorillonite (OMMT) clay as nanofiller, and acetyl tributyl citrate as plasticizer. The corresponding (nano)structures, thermal and mechanical properties, permeability, and biodegradability have been determined. Polyhydroxyalkanoates are very thermal sensitive then to follow the degradation the corresponding matrices have been analyzed by size exclusion chromatography. The results indicate that the addition of the plasticizer decreases the thermo-mechanical degradation, during the extrusion. These nano-biocomposites show an intercalated/exfoliated structure with good mechanical and barrier properties, and an appropriated biodegradation kinetic. Intending to understand the changes in the thermal properties, the nano-biocomposites were characterized by thermal gravimetric analysis and differential scanning calorimetry. The presence of the OMMT clay did not influence significantly the transition temperatures. However, the filler not only acted as a nucleating agent which enhanced the crystallization, but also as a thermal barrier, improving the thermal stability of the biopolymer. The results indicated that the addition of the plasticizer reduces the glass transition temperature and the crystalline melting temperature. The plasticizer acts as a processing aid and increases the processing temperature range (lower melting temperature).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Blending polypropylene (PP) with biodegradable poly(3-hydroxybutyrate) (PHB) can be a nice alternative to minimize the disposal problem of PP and the intrinsic brittleness that restricts PHB applications. However, to achieve acceptable engineering properties, the blend needs to be compatibilized because of the immiscibility between PP and PHB. In this work, PP/PHB blends were prepared with different types of copolymers as possible compatibilizers: poly(propylene-g-maleic anhydride) (PPMAH), poly (ethylene-co-methyl acrylate) [P(EMA)], poly(ethylene-co-glycidyl methacrylate) [P(EGMA)], and poly(ethylene-co-methyl acrylate-co-glycidyl methacrylate) [P(EMAGMA)]. The effect of each copolymer on the morphology and mechanical properties of the blends was investigated. The results show that the compatibilizers efficiency decreased in this order: P(EMAGMA) > P(EMA) > P(EGMA) > PP-MAH; we explained this by taking into consideration the affinity degree of the compatibilizers with the PP matrix, the compatibilizers properties, and their ability to provide physical and/or reactive compatibilization with PHB. (C) 2011 Wiley Periodicals, Inc. J Appl Polym Sci 123: 3511-3519, 2012

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this study was to evaluate the potential application of biodegradable nanoparticles containing a photosensitizer in photodynamic therapy. The poly (D,L lactic-co-glycolic acid) nanoparticles were studied by steady-state techniques, time-resolved fluorescence, and laser flash photolysis. The external morphology of the nanoparticles was established by scanning electron microscopy, and the biological activity was evaluated by in vitro cell culture by 3-(4,5 dimethylthiazol-2,5 biphenyl) tetrazolium bromide assay. The particles were spherical in shape exhibiting a 435 nm diameter with a low tendency to aggregate. The loading efficiency was 77%. The phthalocyanine-loaded-nanoparticles maintained their photophysical behavior after encapsulation. The cellular viability was determined, obtaining 70% of cellular death. All the performed physical-chemical, photophysical, and photobiological measurements indicated that the phthalocyanine-loaded-nanoparticles are a promising drug delivery system for photodynamic therapy and photoprocesses. (C) 2012 Laser Institute of America.