Resumo:
The ‘particle size effect’ and its manifestation in abrasion still attracts considerable debate as to its origins and the ranking of its likely causes. Experiments have been conducted to study the important contribution that the formation of wear debris can have on the progression of wear. The experiments consist of unlubricated (dry) pin-on-disk tests with silicon carbide coated paper of varying particle size, with different pin material, diameter and loads. It has been observed that the influence of debris formation on wear rate is more pronounced for fine abrasives and soft-wearing materials. Consequently, it is proposed that the particle size effect can be explained in terms of geometrical scaling and the evolution of third-body effects with diminishing particle diameter.
Resumo:
The extreme diversity of conditions acting on railways necessitates a variety of experimental approaches to study the critical wear mechanisms that present themselves at the contact interface. This work investigates the effects of contact pressure and geometry in rolling-contact wear tests by using discs with different radii of curvature to simulate the varying contact conditions that may be typically found in the field. It is commonly adapted to line contact interface as it has constant contact pressure. But practical scenario of the rail wheel interface, the contact area increase and contact pressure change as tracks worn off. The tests were conducted without any significant amount of traction, but micro slip was still observed due to contact deformation. Moreover, variation of contact pressure was observed due to contact patch elongation and diameter reduction. Rolling contact fatigue, adhesive and sliding wear were observed on the curved contact interface. The development of different wear regimes and material removal phenomena were analysed using microscopic images in order to broaden the understanding of the wear mechanisms occurring in the rail-wheel contact.
Resumo:
This work investigates the effects of contact pressure and geometry in rolling-contact wear tests by using discs with different radii of curvature to simulate the varying contact conditions that may be typically found in the field. The tests were conducted without any significant amount of traction, but micro slip was still observed due to contact deformation. Moreover, variation of contact pressure was observed due to contact patch elongation and diameter reduction. Rolling contact fatigue, adhesive and sliding wear were observed on the curved contact interface. The development of different wear regimes and material removal phenomena were analyzed using microscopic images in order to broaden the understanding of the wear mechanisms occurring in the rail-wheel contact.
Resumo:
Roller mills are typically used to crush sugarcane to express the juice from which sugar is manufactured. The mill rolls need to provide sufficient grip to ensure minimal sliding of the sugarcane along the roll surface. The rolls are subject to pressures up to 55 MPa from the sugarcane bagasse (as the sugarcane is called after first being crushed between a pair of rolls). The insoluble component of sugarcane includes typically 10% ash that largely originates from soil that is harvested with the cane. The sugarcane juice is acidic with pH typically between 5.0 and 5.5. As a result of ash and juice, the mill rolls are subjected to a range of abrasive and corrosive wear mechanisms. Solutions to provide grip and resist wear involve the selection of an appropriate roll shell material and compatible hard facing to provide the desired grip and wear characteristics. This paper reviews the various solutions that have been adopted for grip and durability for mill rolls and highlights the advantages and disadvantages of each method.
Resumo:
Purpose: The aim of this cross-over study was to investigate the changes in corneal thickness, anterior and posterior corneal topography, corneal refractive power and ocular wavefront aberrations, following the short term use of rigid contact lenses. Method: Fourteen participants wore 4 different types of contact lenses (RGP lenses of 9.5 mm and 10.5 mm diameter, and for comparison a PMMA lens of 9.5 mm diameter and a soft silicone hydrogel lens) on 4 different days for a period of 8 h on each day. Measures were collected before and after contact lens wear and additionally on a baseline day. Results: Anterior corneal curvature generally showed a flattening with both of the RGP lenses and a steepening with the PMMA lens. A significant negative correlation was found between the change in corneal swelling and central and peripheral posterior corneal curvature (all p ≤ 0.001). RGP contact lenses caused a significant decrease in corneal refractive power (hyperopic shift) of approximately 0.5 D. The PMMA contact lenses caused the greatest corneal swelling in both the central (27.92 ± 15.49 μm, p < 0.001) and peripheral (17.78 ± 12.11 μm, p = 0.001) corneal regions, a significant flattening of the posterior cornea and an increase in ocular aberrations (all p ≤ 0.05). Conclusion: The corneal swelling associated with RGP lenses was relatively minor, but there was slight central corneal flattening and a clinically significant hyperopic change in corneal refractive power after the first day of lens wear. The PMMA contact lenses resulted in significant corneal swelling and reduced optical performance of the cornea.
Resumo:
Purpose To examine the influence of short-term miniscleral contact lens wear on corneal shape, thickness and anterior surface aberrations. Methods Scheimpflug imaging was captured before, immediately following and 3 hours after a short period (3 hours) of miniscleral contact lens wear for 10 young (mean 27 ± 5 years), healthy participants. Natural diurnal variations were considered by measuring baseline diurnal changes obtained on a separate control day without contact lens wear. Results Small but significant anterior corneal flattening was observed immediately following lens removal (overall mean 0.02 ± 0.03 mm, p < 0.001) which returned to baseline levels three hours after lens removal. During the three hour recovery period significant corneal thinning (-13.4 ± 10.5 μm) and posterior surface flattening (0.03 ± 0.02 mm) were also observed (both p < 0.01). The magnitude of posterior corneal flattening during recovery correlated with the amount of corneal thinning (r = 0.69, p = 0.03). Central corneal clearance (maximum tear reservoir depth) was not associated with corneal swelling following lens removal (r = -0.24, p > 0.05). An increase in lower-order corneal astigmatism Z(2,2) was also observed following lens wear (mean -0.144 ± 0.075 μm, p = 0.02). Conclusions Flattening of the anterior corneal surface was observed immediately following lens wear, while ‘rebound’ thinning and flattening of the posterior surface was evident following the recovery period. Modern miniscleral contact lenses that vault the cornea may slightly influence corneal shape and power but do not induce clinically significant corneal oedema during short-term wear.
Resumo:
Purpose: In the present study, we consider mechanical properties of phosphate glasses under high temperatureinduced and under friction-induced cross-linking, which enhance the modulus of elasticity. Design/methodology/approach: Two nanomechanical properties are evaluated, the first parameter is the modulus of elasticity (E) (or Young's modulus) and the second parameter is the hardness (H). Zinc meta-, pyro - and orthophosphates were recognized as amorphous-colloidal nanoparticles were synthesized under laboratory conditions and showed antiwear properties in engine oil. Findings: Young's modulus of the phosphate glasses formed under high temperature was in the 60-89 GPa range. For phosphate tribofilm formed under friction hardness and the Young's modulus were in the range of 2-10 GPa and 40-215 GPa, respectively. The degree of cross-linking during friction is provided by internal pressure of about 600 MPa and temperature close to 1000°C enhancing mechanical properties by factor of 3 (see Fig 1). Research limitations/implications: The addition of iron or aluminum ions to phosphate glasses under high temperature - and friction-induced amorphization of zinc metaphosphate and pyrophosphate tends to provide more cross-linking and mechanically stronger structures. Iron and aluminum (FeO4 or AlO4 units), incorporated into phosphate structure as network formers, contribute to the anion network bonding by converting the P=O bonds into bridging oxygen. Future work should consider on development of new of materials prepared by solgel processes, eg., zinc (II)-silicic acid. Originality/value: This paper analyses the friction pressure-induced and temperature–induced the two factors lead phosphate tribofilm glasses to chemically advanced glass structures, which may enhance the wear inhibition. Adding the coordinating ions alters the pressure at which cross-linking occurs and increases the antiwear properties of the surface material significantly.