The degradation of high voltage electrical insulation is a prime factor that can significantly influence the reliability performance and the costs of maintaining high voltage electricity networks. Little information is known about the system of localized degradation from corona discharges on the relatively new silicone rubber sheathed composite insulators that are now being widely used in high voltage applications. This current work focuses on the fundamental principles of electrical corona discharge phenomena to provide further insights to where damaging surface discharges may localize and examines how these discharges may degrade the silicone rubber material. Although water drop corona has been identified by many authors as a major cause of deterioration of silicone rubber high voltage insulation until now no thorough studies have been made of this phenomenon. Results from systematic measurements taken using modern digital instrumentation to simultaneously record the discharge current pulses and visible images associated with corona discharges from between metal electrodes, metal electrodes and water drops, and between waters drops on the surface of silicone rubber insulation, using a range of 50 Hz voltages are inter compared. Visual images of wet electrodes show how water drops can play a part in encouraging flashover, and the first reproducible visual images of water drop corona at the triple junction of water air and silicone rubber insulation are presented. A study of the atomic emission spectra of the corona produced by the discharge from its onset up to and including spark-over, using a high resolution digital spectrometer with a fiber optic probe, provides further understanding of the roles of the active species of atoms and molecules produced by the discharge that may be responsible for not only for chemical changes of insulator surfaces, but may also contribute to the degradation of the metal fittings that support the high voltage insulators. Examples of real insulators and further work specific to the electrical power industry are discussed. A new design concept to prevent/reduce the damaging effects of water drop corona is also presented.
Resumo:
This paper describes the results of experiments made in the vicinity of EHV overhead lines to investigate sources of clouds of charged particles using simultaneously-recording arrays of electric field meters to measure direct electric fields produced under ion clouds. E-field measurements, made at one metre above ground level, are correlated with wind speed and direction, and with measurements from ionisation counters and audible corona effects to identify possible positions of sources of corona on adjacent power lines. Measurements made in dry conditions on EHV lines in flat remote locations with no adjacent buildings or large vegetation indicate the presence of discrete ion sources associated with high stress points on some types of line hardware such as connectors and conductor spacers. Faulty line components such as insulators and line fittings are also found to be a possible source of ion clouds.
Resumo:
Waterfalls attract tourists because they are aesthetically appealing landscape features that are not part of everyday experience. It is generally understood that falls are usually seen at their best when there is a copious flow of water, especially after heavy rain. Guidebooks often contain this observation when referring to waterfalls, sometimes warning readers that the flow may be severely reduced during dry periods. Indeed, many visitors are disappointed when they see falls at such times. Some are saddened when the discharge of a waterfall has been depleted by the abstraction of water upstream for power generation or other purposes. While, for those in search of the Sublime or merely the superlative, size is often important, small waterfalls can give great pleasure to lovers of landscape beauty. According to guidebooks, however, even these falls are usually best seen after rain. Drawing on tourist and travel literature and personal journals from the eighteenth century to the present, and with reference to examples from different parts of the world, this paper discusses the importance of discharge in the tourist experience of waterfalls.
Resumo:
Along with their essential role in electricity transmission and distribution, some powerlines also generate large concentrations of corona ions. This study aimed at comprehensive investigation of corona ions, vertical dc e-field, ambient aerosol particle charge and particle number concentration levels in the proximity of some high/sub-transmission voltage powerlines. The influence of meteorology on the instantaneous value of these parameters, and the possible existence of links or associations between the parameters measured were also statistically investigated. The presence of positive and negative polarities of corona ions was associated with variation in the mean vertical dc e-field, ambient ion and particle charge concentration level. Though these variations increased with wind speed, their values also decreased with distance from the powerlines. Predominately positive polarities of ions were recorded up to a distance of 150 m (with the maximum values recorded 50 m downwind of the powerlines). At 200 m from the source, negative ions predominated. Particle number concentration levels however remained relatively constant (103 particle cm-3) irrespective of the sampling site and distance from the powerlines. Meteorological factors of temperature, humidity and wind direction showed no influence on the electrical parameters measured. The study also discovered that e-field measurements were not necessarily a true representation of the ground-level ambient ion/particle charge concentrations.
Resumo:
Positive and negative small ions, aerosol ion and number concentration and dc electric fields were monitored at an overhead high-voltage power line site. We show that the emission of corona ions was not spatially uniform along the lines and occurred from discrete components such as a particular set of spacers. Maximum ion concentrations and atmospheric dc electric fields were observed at a point 20 m downwind of the lines. It was estimated that less than 7% of the total number of aerosol particles was charged. The electrical parameters decreased steadily with further downwind distance but remained significantly higher than background.
Resumo:
While the communicative turn in policy-making has encouraged the public deliberation of policy decisions it has arguably had a more limited impact on the ability of public processes to deal with wicked problems. Wicked policy problems are characterised by high levels of complexity, uncertainty and divergence of values. However, some wicked problems present the additional challenge of high levels of psychosocial sensitivity and verbal proscription. Because these unspeakable policy problems frequently involve a significant moral dimension, the regulation of intimate processes or bodies, and strong elements of abjection and symbolic pollution they are quite literally problems that we don’t like to think about or talk about. However, the potential environmental and social impacts of these problems require that they be addressed. In this paper I present the preliminary findings of a research project focussed on the idea of the unspeakable policy problem and how its unspeakable nature can impact upon public participation and policy and environmental outcomes.
Resumo:
The common goal of tissue engineering is to develop substitutes that can closely mimic the structure of extracellular matrix (ECM). However, similarly important is the intensive material properties which have often been overlooked, in particular, for soft tissues that are not to bear load assumingly. The mechanostructural properties determine not only the structural stability of biomaterials but also their physiological functionality by directing cellular activity and regulating cell fate decision. The aim here is to emphasize that cells could sense intensive material properties like elasticity and reside, proliferate, migrate and differentiate accordinglyno matter if the construct is from a natural source like cartilage, skin etc. or of synthetic one. Meanwhile, the very objective of this work is to provide a tunable scheme for manipulating the elasticity of collagen-based constructs to be used to demonstrate how to engineer cell behavior and regulate mechanotransduction. Articular cartilage was chosen as it represents one of the most complex hierarchical arrangements of collagen meshwork in both connective tissues and ECM-like biomaterials. Corona discharge treatment was used to produce constructs with varying density of crosslinked collagen and stiffness accordingly. The results demonstrated that elastic modulus increased up to 33% for samples treated up to one minute as crosslink density was found to increase with exposure time. According to the thermal analysis, longer exposure to corona increased crosslink density as the denaturation enthalpy increased. However the spectroscopy results suggested that despite the stabilization of the collagen structure the integrity of the triple helical structure remained intact. The in vitro superficial culture of heterologous chondrocytes also determined that the corona treatment can modulate migration with increased focal adhesion of cells due to enhanced stiffness, without cytotoxicity effects, and providing the basis for reinforcing three-dimensional collagen-based biomaterials in order to direct cell function and mediate mechanotransduction.
Resumo:
Various reactor configurations for generating atmospheric-pressure discharges were tested, and several types of nanostructures, including Mo nanoflakes, were successfully synthesized. Here, we present photographs of the discharges, as well as SEM images of representative nanostructures.
Resumo:
Characteristics of electrical breakdown of a planar magnetron enhanced with an electromagnet and a hollow-cathode structure, are studied experimentally and numerically. At lower pressures the breakdown voltage shows a dependence on the applied magnetic field, and the voltage necessary to achieve the self-sustained discharge regime can be significantly reduced. At higher pressures, the dependence is less sensitive to the magnetic field magnitude and shows a tendency of increased breakdown voltage at the stronger magnetic fields. A model of the magnetron discharge breakdown is developed with the background gas pressure and the magnetic field used as parameters. The model describes the motion of electrons, which gain energy by passing the electric field across the magnetic field and undergo collisions with neutrals, thus generating new bulk electrons. The electrons are in turn accelerated in the electric field and effectively ionize a sufficient amount of neutrals to enable the discharge self-sustainment regime. The model is based on the assumption about the combined classical and near-wall mechanisms of electron conductivity across the magnetic field, and is consistent with the experimental results. The obtained results represent a significant advance toward energy-efficient multipurpose magnetron discharges.
Resumo:
The effect of ambipolar fluxes on nanoparticle charging in a typical low-pressure parallel-plate glow discharge is considered. It is shown that the equilibrium values of the nanoparticle charge in the plasma bulk and near-electrode areas are strongly affected by the ratio S ath i of the ambipolar flux and the ion thermal velocities. Under typical experimental conditions the above ratio is neither S ath i≪ 1 nor S ath i≫1, which often renders the commonly used approximations of the purely thermal or "ion wind" ion charging currents inaccurate. By using the general approximation for the ambipolar drift-affected ion flux on the nanoparticle surface, it appears possible to obtain more accurate values of the nanoparticle charge that usually deviate within 10-25 % from the values obtained without a proper accounting for the ambipolar ion fluxes. The implications of the results obtained for glow discharge modeling and nanoparticle manipulation in low-pressure plasmas are discussed.
Resumo:
Corona discharge is responsible for the small ions found near overhead power lines, and these are capable of modifying the ambient electrical environment such as the dc electric field at ground level (Fews, Wilding et al. 2002). Once produced, small ions quickly attach to aerosol particles in the air, producing ‘large ions’ which are roughly 1 nm to 1 µm in diameter. However, very few studies have reported measurements of ions produced by power lines and its impact on particle charge concentrations. In this present study, the measurements were conducted as a function of normal downwind distance from a 275kV power line for investigating the effect of corona ions on air ions, aerosol particle charge concentration and dc e-filed.
Resumo:
High voltage powerlines may give rise to corona breakdown, resulting in the release of large concentrations of charged ions into the surrounding environment. These ions quickly attach to aerosols and the resulting charged particles are carried by prevalent winds. This paper describes a study carried out at a site near an overhead double circuit ac transmission voltage powerline to investigate factors that control the rate at which charged particles are produced, and to determine the total particle number concentrations, total particle charge concentrations and vertical dc electric fields in the proximity of the line. Measured mean values of these three parameters at a perpendicular distance of 50m from the line were 1.8 x 103 particle cm-3, 518 ions cm3 and 520 V m-1 respectively. The net electric charge was positive and the electric field was directed downwards. These parameters were correlated with each other and monitored at four different distances from the line. Effects of meteorological parameters such as wind speed and wind direction were also investigated.
Resumo:
Pre-breakdown discharge activity in SF6 and SF6 +2% N2 at 1 bar absolute has been investigated to assess the feasibility of adding small amounts of N2 to SF6 to improve the luminosity of the pre-breakdown discharges. It has been shown that small amounts of N2 does not significantly alter the breakdown strength of the mixture but will have a profound influence on the pre-breakdown discharge activity under 50 Hz voltages and lightning impulse voltages. This influence is attributed to the following three mechanisms: 1. The increased availability of free electrons due to the lower ionisation potential of the N2 compared to SF6 2. The removal of high energy electrons from the discharge by electron scattering due to negative ion resonance in N2, thus effectively increasing the attachment of SF6. 3. The creation of longer lived SF6- ions by the attachment of the scattered low energy electrons from N2 thus effectively enhancing the negative ion space charge.
Resumo:
This paper presents preliminary results of an investigation into the detection of partial discharges on the rise of impulse voltages from a point-to-plane gap in SF6. A parallel RC detection impedance is placed in the earth path of a point. Computer simulations are done to determine the values of R and C that will result in the smallest impulse voltage signal and the largest discharge signal across the detection impedance. These simulations and the experimental work show that the impulse voltage signal can not be sufficiently attenuated during the rise time of the applied voltage impulse using the RC detection impedance alone. An alternative discharge detection method is proposed in which a resonant partial discharge coupler is used. Elimination of noise and the impulse voltage signal can be achieved by shorting the coupler plate to the ground plane in the middle of the disk. However, due to the bandwidth of the measuring equipment and noise from the impulse generator it was not possible to detect discharges on the rising edge of a 1.5s voltage impulse using a coupler shorted in the middle. It was found that for this particular coupler, with no shorting points, and if the rising edge of the voltage impulse is longer than 5us, (10us) PD activity can be detected on the rising edge.