7 resultados para Sealant

em Queensland University of Technology - ePrints Archive


Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper investigates the influence of structural sealant joints on the blast performance of laminated glass (LG) panels, using a comprehensive numerical procedure. A parametric study was carried out by varying the width, thickness and the Young’s modulus (E) of the structural silicone sealant joints and the behavior of the LG panel was studied under two different blast loads. Results show that these parameters influence the blast response of LG panels, especially under the higher blast load. Sealant joints that are thicker, have smaller widths and lower E values increase the flexibility at the supports and hence increase the energy absorption of the LG panel while reducing the support reactions. Results also confirmed that sealant joints designed according to current standards perform well under blast loads. Modeling techniques presented in this paper could be used to complement and supplement the guidance in existing design standards. The new information generated in this paper will contribute towards safer and more economical designs of entire facade systems including window glazing, frames and supporting structures.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This study investigated a novel drug delivery system (DDS), consisting of polycaprolactone (PCL) or polycaprolactone 20% tricalcium phosphate (PCL-TCP) biodegradable scaffolds, fibrin Tisseel sealant and recombinant bone morphogenetic protein-2 (rhBMP-2) for bone regeneration. PCL and PCL-TCP-fibrin composites displayed a loading efficiency of 70% and 43%, respectively. Fluorescence and scanning electron microscopy revealed sparse clumps of rhBMP-2 particles, non-uniformly distributed on the rods’ surface of PCL-fibrin composites. In contrast, individual rhBMP-2 particles were evident and uniformly distributed on the rods’ surface of the PCL-TCP-fibrin composites. PCL-fibrin composites loaded with 10 and 20 μg/ml rhBMP-2 demonstrated a triphasic release profile as quantified by an enzyme-linked immunosorbent assay (ELISA). This consisted of burst releases at 2 h, and days 7 and 16. A biphasic release profile was observed for PCL-TCP-fibrin composites loaded with 10 μg/ml rhBMP-2, consisting of burst releases at 2 h and day 14. PCL-TCP-fibrin composites loaded with 20 μg/ml rhBMP-2 showed a tri-phasic release profile, consisting of burst releases at 2 h, and days 10 and 21. We conclude that the addition of TCP caused a delay in rhBMP-2 release. Sodium dodecyl sulphate polyacrylamide gel electrophoresis (SDS-PAGE) and alkaline phosphatase assay verified the stability and bioactivity of eluted rhBMP-2 at all time points

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper presents a rigorous and a reliable analytical procedure using finite element (FE) techniques to study the blast response of laminated glass (LG) panel and predict the failure of its components. The 1st principal stress (σ11) is used as the failure criterion for glass and the von mises stress (σv) is used for the interlayer and sealant joints. The results from the FE analysis for mid-span deflection, energy absorption and the stresses at critical locations of glass, interlayer and structural sealant are presented in the paper. These results compared well with those obtained from a free field blast test reported in the literature. The tensile strength (T) of the glass has a significant influence on the behaviour of the LG panel and should be treated carefully in the analysis. The glass panes absorb about 80% of the blast energy for the treated blast load and this should be minimised in the design.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper presents a comprehensive numerical procedure to treat the blast response of laminated glass (LG) panels and studies the influence of important material parameters. Post-crack behaviour of the LG panel and the contribution of the interlayer towards blast resistance are treated. Modelling techniques are validated by comparing with existing experimental results. Findings indicate that the tensile strength of glass considerably influences the blast response of LG panels while the interlayer material properties have a major impact on the response under higher blast loads. Initially, glass panes absorb most of the blast energy, but after the glass breaks, interlayer deforms further and absorbs most of the blast energy. LG panels should be designed to fail by tearing of the interlayer rather than failure at the supports to achieve a desired level of protection. From this aspect, material properties of glass, interlayer and sealant joints play important roles, but unfortunately they are not accounted for in the current design standards. The new information generated in this paper will enhance the capabilities of engineers to better design LG panels under blast loads and use better materials to improve the blast response of LG panels.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This thesis develops and applies an analytical method to treat the blast response of glass façades and studies the influence of controlling parameters such as all component materials and geometric properties, support conditions and energy absorption, and hence establishes a framework for their design for a credible blast event.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper reviews current design standards and test methods for blast-resistant glazing design and compares a typical design outcome with that from comprehensive finite-element (FE) analysis. Design standards are conservative and are limited to the design of relatively small glazed panels. Standard test methods are expensive, create environmental pollution, and can classify the hazard ratings of only smaller glazed panels. Here the design of a laminated glass (LG) panel is carried out according to an existing design standard, and then its performance is examined using comprehensive FE modeling and analysis. Finite-element results indicate that both glass panes crack, the interlayer yields with little damage, and the sealant joints do not fail for the designed blast load. This failure pattern satisfies some of the requirements for minimal hazard rating in the design standard. It is evident that interlayer thickness and material properties are important during the post-crack stage of an LG panel, but they are not accounted for in the design standards. The new information generated in this paper will contribute toward an enhanced blast design of LG panels.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A novel protective covering with a layered and staggered structure was proposed to protect concrete against projectile impact. Experimental study was conducted to investigate the ballistic behaviour of the concrete targets against 12.7 mm armour-piercing incendiary projectile at velocities ranging from 537.7 to 596.5 m/s. The results showed that the concrete targets with protective covering exhibited superior integrity with no damage on the distal surface, whereas the concrete targets without protective covering were fractured with penetrating cracks throughout the thickness of the target. Moreover, the protected concrete targets displayed significantly reduced penetration depth compared with the concrete targets without protective covering. The protective covering with epoxy adhesive interlayers had a bigger protection factor than that with silicone sealant interlayers, but the former suffered more severe damage than the latter.