300 resultados para Scanning electron microscopic
Resumo:
The microstructure of YBa2Cu3O7-delta (Y-123) materials partially-melted in air and quenched from the temperature range 900-1100 degrees C, has been characterized using a combination of X-ray diffractometry, optical microscopy, scanning electron microscopy, electron microprobe analyses, transmission electron microscopy and energy and wave dispersive X-ray spectrometries. The microstructural studies reveal significant changes in the character of the quenched partial-melt as a function of temperature and time before quenching. BaCu2O2 and BaCuO2 are found to co-exist in stoichiometric samples quenched from the temperature range 920-960 degrees C. Under suitable cooling conditions, large pockets of melt cristallize as BaCuO2 with an exsolution of BaCu2O2 in the form of thin plates (approximate to 50-100 nm thick) along facets. Y2BaCuO5 (Y-211) additions are associated with the formation of BaCu2O2 at 1100 degrees C. Preliminary results on the effects of PtO2 and CeO2 additions to Y-123 (and Y-123 with Y-211 additions) show that these enhace the formation of BaCu2O2 at the melting temperature of 1100 degrees C. (C) 1998 Elsevier Science S.A. All rights reserved.
Resumo:
Orebodies at Ok Tedi contain a number of different fluorine bearing minerals. Some of these minerals report to concentrate and are responsible for the presence of the penalty element, fluorine, within the concentrate. Previous analytical work has tended to examine geological samples for content, rather than determine the metallurgical behaviour of the different mineralogical species. This investigation utilised X-Ray Diffraction combined with Scanning Electron Microscope/Electron Microprobe to identify the fluorine bearing minerals in flotation test products. Seven fluorine bearing minerals were identified, viz., talc, phlogopite, amphibole (tremolite and actinolite), sphene, apatite, biotite and clay. Talc was found exclusively in the skarn ore type. Phlogopite and amphiboles (tremolite and actinolite) were found to occur in both skarn and porphyry ores, while sphene, apatite, biotite and clay were found only in the porphyry ores. Of the fluorine bearing minerals observed, only talc exhibited natural hydrophobicity to any significant degree. Phlogopite and the amphibole minerals were found to be hydrophillic, whilst the remaining minerals occurred in insufficient quantities to determine the flotation behaviour. Ok Tedi copper concentrate fluorine content prior to skarn ore treatment in the mill (typically 350ppm) was previously identified as deriving from phlogopite, while talc was believed to be the source of intermittent high concentrate fluorine contents when skarn ores were treated. This paper provides supporting evidence for this belief, and reports the nature of fluorine bearing mineral flotation behaviour.
Resumo:
The microstructure of YBa2Cu3O7-δ (YBCO) materials, melt-textured in air and quenched from the temperature range 900-990°C, has been characterized using a combination of x-ray diffractometry, optical microscopy, scanning electron microscopy, transmission electron microscopy, and energy dispersive x-ray spectrometry. BaCu2O2 and BaCuO2 were found to coexist in samples quenched from the temperature range 920-960°C. The formation of BaCu2O2 preceded the formation of YBCO. Once the YBCO had formed, BaCu2O2 was present at the solidification front filling the space between nearly parallel platelets of YBCO. Large Y2BaCuO5 particles at the solidification front appeared divided into smaller ones as a result of their dissolution in the liquid that quenched as BaCu2O2.
Resumo:
The structure and composition of reaction products between Bi-Sr-Ca-Cu-oxide (BSCCO) thick films and alumina substrates have been characterized using a combination of electron diffraction, scanning electron microscopy and energy dispersive X-ray spectrometry (EDX). Sr and Ca are found to be the most reactive cations with alumina. Sr4Al6O12SO4 is formed between the alumina substrates and BSCCO thick films prepared from paste with composition close to Bi-2212 (and Bi-2212 + 10 wt.% Ag). For paste with composition close to Bi(Pb)-2223 + 20 wt.% Ag, a new phase with f.c.c. structure, lattice parameter about a = 24.5 A and approximate composition Al3Sr2CaBi2CuOx has been identified in the interface region. Understanding and control of these reactions is essential for growth of high quality BSCCO thick films on alumina. (C) 1997 Elsevier Science S.A.
Resumo:
The microstructure of Bi-Sr-Ca-Cu-oxide (BSCCO) thick films on alumina substrates has been characterized using a combination of X-ray diffractometry, scanning electron microscopy, transmission electron microscopy of sections across the film/substrate interface and energy-dispersive X-ray spectrometry. A reaction layer formed between the BSCCO films and the alumina substrates. This chemical interaction is largely responsible for off-stoichiometry of the films and is more significant after partial melting of the films. A new phase with fee structure, lattice parameter a = 2.45 nm and approximate composition Al3Sr2CaBi2CuOx has been identified as reaction product between BSCCO and Al2O3.
Resumo:
Raman spectroscopy, X-ray diffraction (XRD), and scanning electron microscopy (SEM) have been used to compare samples of YBa2Cu3O7 (YBCO) synthesised by the solid-state method and a novel co-precipitation technique. XRD results indicate that YBCO prepared by these two methods are phase pure, however the Raman and SEM results show marked differences between these samples.
Freshwater sensitivity of corrensite and chlorite/smectite in hydrocarbon reservoirs - an ESEM study
Resumo:
An Environmental Scanning Electron Microscope (ESEM) has been used to investigate the freshwater sensitivity of secondary corrensite (regularly interstratified chlorite/smectite) and chlorite-rich chlorite/smectite in order to determine whether hydrocarbon reservoirs hosting these clays should be regarded as freshwater sensitive. ESEM experiments involved an examination and close comparison of selected clay areas in three samples at high magnification before, during and after prolonged freshwater treatments. Corrensite and chlorine/smectite in the samples did not visibly swell when immersed in fresh water. After soaking in fresh water for up to three months, these clays retained their original morphology and associated porosity. Hence, the presence of corrensite or chlorite/smectite in a hydrocarbon reservoir need not indicate that the reservoir is freshwater sensitive. © 1994.
Resumo:
The environmental scanning electron microscope (ESEM) has been used to image liquid hydrocarbons in sandstones and oil shales. Additionally, the fluid sensitivity of selected clay minerals in hydrocarbon reservoirs was assessed via three case studies: HCl acid sensitivity of authigenic chlorite in sandstone reservoirs, freshwater sensitivity of authigenic illite/smectite in sandstone reservoirs, and bleach sensitivity of a volcanic reservoir containing abundant secondary chlorite/corrensite. The results showed the suitability of using ESEM for imaging liquid hydrocarbon films in hydrocarbon reservoirs and the importance of simulating in situ fluid-rock interactions for hydrocarbon production programmes. In each case, results of the ESEM studies greatly enhanced prediction of reservoir/borehole reactions and, in some cases, contradicted conventional wisdom regarding the outcome of potential engineering solutions. (C) 1993 Wiley-Liss, Inc.
Resumo:
Experiments were carried out on the sodium hypochlorite bleach sensitivity of a deep subsurface andesitic reservoir in order to predict possible deleterious mineral transformations during a downhole clean-up job. Experiments involved examination of core samples from the reservoir using an Environmental Scanning Electron Microscope (ESEM) with an attached Energy Dispersive Spectrometer (EDS) before and after the samples were immersed in bleach. Bleach immersion of whole-rock samples resulted in rapid (less than 1 min) precipitation of abundant 3.0-10.0-μm-wide calcite rhombs within clay-associated micropores and on clay and feldspar grain surfaces. Abundant microporefilling calcite rhombs also formed in pure separates of constituent chlorite/corrensite, whereas no calcite formed in a pure separate of constituent zeolite. These experiments indicate that corrensite is the likely calcium source in this experimental fluid-rock system. Formation of calcite occurs via a cation exchange reaction in which calcium in the smectitic interlayers of corrensite exchanges for sodium in the bleach. Serious formation damage due to calcite precipitation would have occurred in the andesite reservoir had it been exposed to bleach. This finding gives credence to earlier suggestions that cation exchange reactions have the potential to cause calcite precipitation in some sandstone reservoirs when exposed to drilling, completion or stimulation fluids. © 1993.
Resumo:
The effect of HCl on authigenic chlorite in three different sandstones has been examined uisng an Environmental Scanning Electron Microscope (ESEM), together with conventional analytical techniques. The ESEM enabled chlorites to be directly observed in situ at high magnifications during HCl treatment, and was particularly effective in allowing the same chlorite areas to be closely compared before and after acid treatment. Chlorites were reacted with 1M to 10M HCl at temperatures up to 80°C and for periods up to five months. After all treatments, chlorites show extensive leaching of iron, magnesium and aluminum, and their crystalline structure is destroyed. However, despite these major compositional and structural changes, chlorites show little or no visible evidence of acid attack, with precise morphological detail of individual plates preserved in all samples following acid treatments. Chlorite dissolution, sensu stricto, did not occur as a result of acidization of the host sandstones. Acid-treated chlorides are likely to exits in a structurally weakened state that may make them susceptible to physical disintegration during fluid flow. Accordingly, fines migration may be a significant engineering problem associated with the acidization of chlorite-bearing sandstones. © 1993.
Resumo:
The water sensitivity of authigenic smectite- and illite-rich illite/smectites in sandstone reservoirs has been investigated using an Environmental Scanning Electron Microscope (ESEM). The ESEM enabled the illite/smectites to be directly observed in situ at high magnification during freshwater immersion, and was also particularly effective in allowing the same selected illite/smectite areas to be closely compared before and after freshwater treatments. The tendency of authigenic smectite-rich illite/smectite to swell on contact with fresh water varies greatly. Smectite-rich illite/smectite may osmotically swell to many times its original volume to form a gel which greatly reduces porosity and permeability, or may undergo only a subtle morphological change which has little or no adverse effect on reservoir quality. Authigenic illite-rich illite/smectite in sandstones does not swell when immersed in fresh water. Even after prolonged soaking in fresh water, illite-rich illite/smectite particles retain their original morphology. Accordingly, illite-rich illite/smectite in sandstones is unlikely to cause formation damage if exposed to freshwater-based fluids. © 1993.
Resumo:
Samples from the Callide Coal Measures, Queensland, Australia, containing the minor maceral, micrinite, have been studied using optical and electron-optical techniques to determine the precise compositional and structural nature of micrinite when in association with vitrinite macerals. Emphasis has been placed on direct spatial correlation of optical and electron-optical data due to the fine grain size (<1μm) of micrinite and its relatively low abundance compared with other macerals in the Callide Basin coals. Precise elemental, morphological and structural data, including electron diffraction, provides unambiguous evidence for the presence of kaolinite in the component known as micrinite. Indeed, micrinite consists predominantly of fine-grained kaolinite (>90 per cent of the component) and, as such, should not be considered a maceral.
Resumo:
Detailed investigation of an intermediate member of the reddingite–phosphoferrite series, using infrared and Raman spectroscopy, scanning electron microcopy and electron microprobe analysis, has been carried out on a homogeneous sample from a lithium-bearing pegmatite named Cigana mine, near Conselheiro Pena, Minas Gerais, Brazil. The determined formula is (Mn1.60Fe1.21Ca0.01Mg0.01)∑2.83(PO4)2.12⋅(H2O2.85F0.01)∑2.86 indicating predominance in the reddingite member. Raman spectroscopy coupled with infrared spectroscopy supports the concept of phosphate, hydrogen phosphate and dihydrogen phosphate units in the structure of reddingite-phosphoferrite. Infrared and Raman bands attributed to water and hydroxyl stretching modes are identified. Vibrational spectroscopy adds useful information to the molecular structure of reddingite–phosphoferrite.
Resumo:
Titanium oxide nanotubes were obtained by an electrochemical anodization method. Scanning electron microscope results demonstrate that the diameter of the tubes is about 120 nm and the length of the tubes is around 13 μm. Transmission electron microscope results indicate that the nanotubes are assembled by numerous nanoparticles and tube-like structure remains well after heat treatment at 400-600 °C. The photocatalysis performance of the nanotubes was evaluated in terms of the decomposition rate of methyl orange under UV irradiation. The results show that the photocatalytic activity was enhanced through the heating treatment of the nanotubes, and the nanotubes heated at 600 °C exhibits the best photocatalytic activity. X-ray diffraction patterns indicate that there is no phase transformation during the heat treatment. Therefore, the enhanced activity can be attributed to the improvement of nanotubes crystallinity, which may provide more insights about the effect of the crystallinity on the photocatalytic performance.
Resumo:
Knowledge of the elements present in house dusts is important in understanding potential health effects on humans. In this study, dust samples collected from 10 houses in south-east Queensland have been analysed by scanning electron microscopy and X-ray microanalysis to measure the inorganic element compositions and to investigate the form of heavy metals in the dusts. The overall analytical results were then used to discriminate between different localities using chemometric techniques. The relative amounts of elements, particularly of Si, Ca, and Fe, varied between size fractions and between different locations for the same size fraction. By analysing individual small particles, many other constituents were identified including Ti, Cr, Mn, Ni, Cu, Zn, Ba, Ag, W, Au, Hg, Pb, Bi, La and Ce. The heavy metals were mostly concentrated in small particles in the smaller size fractions, which allowed detection by particle analysis, though their average concentrations were very low.