Resumo:
The hydrotalcite based upon manganese known as charmarite Mn4Al2(OH)12CO3•3H2O has been synthesised with different Mn/Al ratios from 4:1 to 2:1. Impurities of manganese oxide, rhodochrosite and bayerite at low concentrations were also produced during the synthesis. The thermal stability of charmarite was investigated using thermogravimetry. The manganese hydrotalcite decomposed in stages with mass loss steps at 211, 305 and 793°C. The product of the thermal decomposition was amorphous material mixed with manganese oxide. A comparison is made with the thermal decomposition of the Mg/Al hydrotalcite. It is concluded that the synthetic charmarite is slightly less stable than hydrotalcite.
Resumo:
Dynamic and controlled rate thermal analysis (CRTA) has been used to characterise alunites of formula [M(Al)3(SO4)2(OH)6 ] where M+ is the cations K+, Na+ or NH4+. Thermal decomposition occurs in a series of steps. (a) dehydration, (b) well defined dehydroxylation and (c) desulphation. CRTA offers a better resolution and a more detailed interpretation of water formation processes via approaching equilibrium conditions of decomposition through the elimination of the slow transfer of heat to the sample as a controlling parameter on the process of decomposition. Constant-rate decomposition processes of water formation reveal the subtle nature of dehydration and dehydroxylation.
Resumo:
Raman spectroscopy has been used to study the arsenate minerals haidingerite Ca(AsO3OH)•H2O and brassite Mg(AsO3OH)•4H2O. Intense Raman bands in haidingerite spectrum observed at 745 and 855 cm-1 are assigned to the (AsO3OH)2- ν3 antisymmetric stretching and ν1 symmetric stretching vibrational modes. For brassite two similarly assigned intense bands are found at 809 and 862 cm-1. The observation of multiple Raman bands in the (AsO3OH)2- stretching and bending regions suggests that the arsenate tetrahedrons in the crystal structures of both minerals studied are strongly distorted. Broad Raman bands observed at 2842 cm-1 for haidingerite and 3035 cm-1 for brassite indicate strong hydrogen bonding of water molecules in the structure of these minerals. OH…O hydrogen bond lengths were calculated from the Raman spectra based on empiric relations.
Resumo:
Structural changes in intercalated kaolinite after wet ball-milling were examined by scanning electron microscopy (SEM), X-ray diffraction (XRD), specific surface area (SSA) and Fourier Transform Infrared spectroscopy (FTIR). The X-ray diffraction pattern at room temperature indicated that the intercalation of potassium acetate into kaolinite causes an increase of the basal spacing from 0.718 to 1.42 nm, and with the particle size reduction, the surface area increased sharply with the intercalation and delamination by ball-milling. The wet ball-milling kaolinite after intercalation did not change the structural order, and the particulates have high aspect ratio according SEM images.
Resumo:
Mottramite mineral originated from Tsumeb Corporation Mine, Tsumeb, Otavi, Namibia, is used in the present work. The mineral contains of vanadium and copper to the extent of 22.73% and 16.84% by weight respectively as V2O5 and CuO. An EPR study of sample confirms the presence of Cu(II) with g = 2.2. Optical absorption spectrum of mottramite indicates that Cu(II) is present in rhombic environment. NIR results are due to water fundamentals.
Resumo:
The unusual behaviour of fine lunar regolith like stickiness and low heat conductivity is dominated by the structural arrangement of its finest fraction in the outer-most topsoil layer. Here, we show the previously unknown phenomenon of building a globular 3-D superstructure within the dust fraction of the regolith. New technology, Transmission X-ray Microscopy (TXM) with tomographic reconstruction, reveals a highly porous network of cellular void system in the lunar finest dust fraction aggregates. Such porous chained aggregates are composed of sub-micron in size particles that build cellular void networks. Voids are a few micrometers in diameter. Discovery of such a superstructure within the finest fraction of the lunar topsoil allow building a model of heat transfer which is discussed.
Resumo:
A voglite mineral sample of Volrite Canyon #1 mine, Frey Point, White Canyon Mine District, San Juan County, Utah, USA is used in the present study. An EPR study on powdered sample confirms the presence of Mn(II) and Cu(II). Optical absorption spectral results are due to Cu(II) which is in distorted octahedron. NIR results are indicating the presence of water fundamentals.
Resumo:
The application of near-infrared and infrared spectroscopy has been used for identification and distinction of basic Cu-sulphates that include devilline, chalcoalumite and caledonite. Near-infrared spectra of copper sulphate minerals confirm copper in divalent state. Jahn-Teller effect is more significant in chalcoalumite where 2B1g ® 2B2g transition band shows a larger splitting (490 cm-1) confirming more distorted octahedral coordination of Cu2+ ion. One symmetrical band at 5145 cm-1 with shoulder band 5715 cm-1 result from the absorbed molecular water in the copper complexes are the combinations of OH vibrations of H2O. One sharp band at around 3400 cm-1 in IR common to the three complexes is evidenced by Cu-OH vibrations. The strong absorptions observed at 1685 and 1620 cm-1 for water bending modes in two species confirm strong hydrogen bonding in devilline and chalcoalumite. The multiple bands in v3 and v4(SO4)2- stretching regions are attributed to the reduction of symmetry to the sulphate ion from Td to C2V. Chalcoalumite, the excellent IR absorber over the range 3800-500 cm-1 is treated as most efficient heat insulator among the Cu-sulphate complexes.
Resumo:
The kaolinite-like phyllosilicate minerals bismutoferrite BiFe3+2Si2O8(OH) and chapmanite SbFe3+2Si2O8(OH) have been studied by Raman spectroscopy and complemented with infrared spectra. Tentatively interpreted spectra were related to their molecular structure. The antisymmetric and symmetric stretching vibrations of the Si-O-Si bridges, SiOSi and OSiO bending vibrations, (Si-Oterminal)- stretching vibrations, OH stretching vibrations of hydroxyl ions, and OH bending vibrations were attributed to observed bands. Infrared bands 3289-3470 cm-1 and Raman bands 1590-1667 cm-1 were assigned to adsorbed water. O-H...O hydrogen bond lengths were calculated from the Raman and infrared spectra.
Resumo:
Insight into the unique structure of hydrotalcites has been obtained using Raman spectroscopy. Gallium containing hydrotalcites of formula Mg4Ga2(CO3)(OH)12•4H2O (2:1 Ga-HT) to Mg8Ga2(CO3)(OH)20•4H2O (4:1 Ga-HT) have been successfully synthesised and characterized by X-ray diffraction and Raman spectroscopy. The d(003) spacing varied from 7.83 Å for the 2:1 hydrotalcite to 8.15 Å for the 3:1 gallium containing hydrotalcite. Raman spectroscopy complemented with selected infrared data has been used to characterise the synthesised gallium containing hydrotalcites of formula Mg6Ga2(CO3)(OH)16•4H2O. Raman bands observed at around 1046, 1048 and 1058 cm-1 were attributed to the symmetric stretching modes of the (CO32-) units. Multiple ν3 CO32- antisymmetric stretching modes are found at around 1346, 1378, 1446, 1464 and 1494 cm-1. The splitting of this mode indicates the carbonate anion is in a perturbed state. Raman bands observed at 710 and 717 cm-1 assigned to the ν4 (CO32-) modes support the concept of multiple carbonate species in the interlayer.
Resumo:
Near-infrared (NIR) and Fourier transform infrared (FTIR) spectroscopy have been used to determine the mineralogical character of isomorphic substitutions for Mg2+ by divalent transition metals Fe, Mn, Co and Ni in natural halotrichite series. The minerals are characterised by d-d transitions in NIR region 12000-7500 cm-1. NIR spectrum of halotrichite reveals broad feature from 12000 to 7500 cm-1 with a splitting of two bands resulting from ferrous ion transition 5T2g ® 5Eg. The presence of overtones of OH- fundamentals near 7000 cm-1 confirms molecular water in the mineral structure of the halotrichite series. The appearance of the most intense peak at around 5132 cm-1 is a common feature in the three minerals and is derived from combination of OH- vibrations of water molecules and 2 water bending modes. The influence of cations like Mg2+, Fe2+, Mn2+, Co2+, Ni2+ shows on the spectra of halotrichites. Especially wupatkiite-OH stretching vibrations in which bands are distorted conspicuously to low wave numbers at 3270, 2904 and 2454 cm-1. The observation of high frequency 2 mode in the infrared spectrum at 1640 cm-1 indicates coordination of water molecules is strongly hydrogen bonded in natural halotrichites. The splittings of bands in 3 and 4 (SO4)2- stretching regions may be attributed to the reduction of symmetry from Td to C2v for sulphate ion. This work has shown the usefulness of NIR spectroscopy for the rapid identification and classification of the halotrichite minerals.
Resumo:
Several specimens of Libyan Desert Glass (LDG), an enigmatic natural glass from Egypt, were subjected to investigation by micro-Raman spectroscopy. The spectra of inclusions inside the LDG samples were successfully measured through the layers of glass and the mineral species were identified on this basis. The presence of cristobalite as typical for high-temperature melt products was confirmed, together with co-existing quartz. TiO2 was determined in two polymorphic species, rutile and anatase. Micro-Raman spectroscopy proved also the presence of minerals unusual for high-temperature glasses such as anhydrite and aragonite.
Resumo:
An investigation has been made of the interactions between silicone oil and various solid substrates immersed in aqueous solutions. Measurements were made using an atomic force microscope (AFM) using the colloid-probe method. The silicone oil drop is simulated by coating a small silica sphere with the oil, and measuring the force as this coated sphere is brought close to contact with a flat solid surface. It is found that the silicone oil surface is negatively charged, which causes a double-layer repulsion between the oil drop and another negatively charged surface such as mica. With hydrophilic solids, this repulsion is strong enough to prevent attachment of the drop to the solid. However, with hydrophobic surfaces there is an additional attractive force which overcomes the double-layer repulsion, and the silicone oil drop attaches to the solid. A "ramp" force appears in some, but not all, of the data sets. There is circumstantial evidence that this force results from compression of the silicone oil film coated on the glass sphere.
Resumo:
Thermogravimetric analysis-mass spectrometry, X-ray diffraction and scanning electron microscopy (SEM) were used to characterize eight kaolinite samples from China. The results show that the thermal decomposition occurs in three main steps (a) desorption of water below 100 °C, (b) dehydration at about 225 °C, (c) well defined dehydroxylation at around 450 °C. It is also found that decarbonization took place at 710 °C due to the decomposition of calcite impurity in kaolin. The temperature of dehydroxylation of kaolinite is found to be influenced by the degree of disorder of the kaolinite structure and the gases evolved in the decomposition process can be various because of the different amount and kinds of impurities. It is evident by the mass spectra that the interlayer carbonate from impurity of calcite and organic carbon is released as CO2 around 225, 350 and 710 °C in the kaolinite samples.
Resumo:
Two kinds of coal-bearing kaolinite from China were analysed by X-ray diffraction (XRD), Thermogravimetric analysis-mass spectrometry (TG-MS), infrared emission spectroscopy. Thermal decomposition occurs in a series of steps attributed to (a) desorption of water at 68 °C for Datong coal bearing strata kaolinite and 56 °C for Xiaoxian with mass losses of 0.36 % and 0.51 % (b) decarbonization at 456 °C for Datong coal bearing strata kaolinite and 431 °C for Xiaoxian kaolinite, (c) dehydroxylation takes place in two steps at 589 and 633 °C for Datong coal bearing strata kaolinite and at 507 °C and 579 °C for Xiaoxian kaolinite. This mineral were further characterised by infrared emission spectroscopy (IES). Well defined hydroxyl stretching bands at around 3695, 3679, 3652 and 3625 cm-1 are observed. At 650 °C all intensity in these bands is lost in harmony with the thermal analysis results. Characteristic functional groups from coal are observed at 1918, 1724 and 1459 cm-1. The intensity of these bands decrease by thermal treatment and is lost by 700 °C.