197 resultados para Pulsed laser deposition (PLD)
Resumo:
Advances in solid-state switches and power electronics techniques have led to the development of compact, efficient and more reliable pulsed power systems. This paper proposes an efficient scheme that utilizes modular switch-capacitor units in obtaining high voltage levels with fast rise time (dv/dt) using low voltage solid-state switches. The proposed pulsed power supply has flexibility in terms of controlling energy and generating broad range of voltage levels. The energy flow can be controlled as the stored energy can be adjusted by a current source utilized at the first stage of the system. Desirable voltage level can be obtained by connecting adequate number of switch-capacitor units. Moreover, the proposed topology is load independent. Therefore it can easily supply wide range of applications especially the low impedance ones. The effectiveness of the proposed approach is verified by simulations
Resumo:
Advances in solid-state switches and power electronics techniques have led to the development of compact, efficient and more reliable pulsed power systems. Although, the power rating and operation speed of the new solid-state switches are considerably increased, their low blocking voltage level puts a limits in the pulsed power operation. This paper proposes the advantage of parallel and series configurations of pulsed power modules in obtaining high voltage levels with fast rise time (dv/dt) using only conventional switches. The proposed configuration is based on two flyback modules. The effectiveness of the proposed approach is verified by numerical simulations, and the advantages of each configuration are indicated in comparison with a single module.
Resumo:
In this paper characteristic of a DBD (Dielectric Barrier Discharge) plasma lamp is investigated based on the lamp intensity and power consumption. A pulsed power supply with controllable parameters based on a push-pull converter is developed for lamp excitation at different voltage levels and repetition rate. The experimentations were conducted for 28 different operating points with the frequency range of 2 kHz to 15 Khz at output voltage levels of between 7.4 kV up to 13 kV. The obtained results show the feasibility of finding an optimum operation point due to nonlinear behaviour of the DBD lamp.
Resumo:
The electron Volt Spectrometer (eVS) is an inverse geometry filter difference spectrometer that has been optimised to measure the single atom properties of condensed matter systems using a technique known as Neutron Compton Scattering (NCS) or Deep Inelastic Neutron Scattering (DINS). The spectrometer utilises the high flux of epithermal neutrons that are produced by the ISIS neutron spallation source enabling the direct measurement of atomic momentum distributions and ground state kinetic energies. In this paper the procedure that is used to calibrate the spectrometer is described. This includes details of the method used to determine detector positions and neutron flight path lengths as well as the determination of the instrument resolution. Examples of measurements on 3 different samples are shown, ZrH2, 4He and Sn which show the self-consistency of the calibration procedure.
Resumo:
The deposition of small metal clusters (Cu, Au and Al) on f.c.c. metals (Cu, Au and Ni) has been studied by molecular dynamics simulation using Finnis–Sinclair (FS) potential. The impact energy varied from 0.01 to 10 eV/atom. First, the deposition of single cluster was simulated. We observed that, even at much lower energy, a small cluster with (Ih) icosahedral symmetry was reconstructed to match the substrate structure (f.c.c.) after deposition. Next, clusters were modeled to drop, one after the other, on the surface. The nanostructure was found by soft landing of Au clusters on Cu with increasing coverage, where interfacial energy dominates. While at relatively higher deposition energy (a few eV), the ordered f.c.c.-like structure was observed in the first adlayer of the film formed by Al clusters depositing on Ni substrate. This characteristic is mainly attributive to the ballistic collision. Our results indicate that the surface morphology synthesized by cluster deposition could be controlled by experimental parameters, which will be helpful for controlled design of nanostructure.
Resumo:
The impact induced chemisorption of hydrocarbon molecules (CH3 and CH2) on H-terminated diamond (001)-(2x1) surface was investigated by molecular dynamics simulation using the many-body Brenner potential. The deposition dynamics of the CH3 radical at impact energies of 0.1-50 eV per molecule was studied and the energy threshold for chemisorption was calculated. The impact-induced decomposition of hydrogen atoms and the dimer opening mechanism on the surface was investigated. Furthermore, the probability for dimer opening event induced by chemisorption of CH, was simulated by randomly varying the impact position as well as the orientation of the molecule relative to the surface. Finally, the energetic hydrocarbons were modeled, slowing down one after the other to simulate the initial fabrication of diamond-like carbon (DLC) films. The structure characteristic in synthesized films with different hydrogen flux was studied. Our results indicate that CH3, CH2 and H are highly reactive and important species in diamond growth. Especially, the fraction of C-atoms in the film having sp(3) hybridization will be enhanced in the presence of H atoms, which is in good agreement with experimental observations. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
In this paper, the deposition of C-20 fullerenes on a diamond (001)-(2x1) surface and the fabrication of C-20 thin film at 100 K were investigated by a molecular dynamics (MD) simulation using the many-body Brenner bond order potential. First, we found that the collision dynamic of a single C-20 fullerene on a diamond surface was strongly dependent on its impact energy. Within the energy range 10-45 eV, the C-20 fullerene chemisorbed on the surface retained its free cage structure. This is consistent with the experimental observation, where it was called the memory effect in "C-20-type" films [P. Melion , Int. J. Mod. B 9, 339 (1995); P. Milani , Cluster Beam Synthesis of Nanostructured Materials (Springer, Berlin, 1999)]. Next, more than one hundred C-20 (10-25 eV) were deposited one after the other onto the surface. The initial growth stage of C-20 thin film was observed to be in the three-dimensional island mode. The randomly deposited C-20 fullerenes stacked on diamond surface and acted as building blocks forming a polymerlike structure. The assembled film was also highly porous due to cluster-cluster interaction. The bond angle distribution and the neighbor-atom-number distribution of the film presented a well-defined local order, which is of sp(3) hybridization character, the same as that of a free C-20 cage. These simulation results are again in good agreement with the experimental observation. Finally, the deposited C-20 film showed high stability even when the temperature was raised up to 1500 K.
Resumo:
In this paper, the influence of the impact energy on the initial fabrication of thin films formed by low energy cluster deposition was investigated by molecular dynamics simulation of All 3 clusters depositing on Ni(0 0 1) substrate. In the case of soft-landing, (0.01 eV/atom), clusters are rearranged from I-h symmetry into fcc-like clusters on the surface. Then they aggregate each other, which result in thin film growing in 3D island mode. While, growth will be in layer-by-layer mode at the impact energy of a few electron volt due to the transient lateral spread of cluster atoms induced by dense collision cascade. This effect has been traced to collision cascade inside the cluster. which is enhanced by collision with a hard Ni substrate. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
The electron Volt Spectrometer (eVS) is an inverse geometry filter difference spectrometer that has been optimised to measure the single atom properties of condensed matter systems using a technique known as Neutron Compton Scattering (NCS) or Deep Inelastic Neutron Scattering (DINS). The spectrometer utilises the high flux of epithermal neutrons that are produced by the ISIS neutron spallation source enabling the direct measurement of atomic momentum distributions and ground state kinetic energies. In this paper the procedure that is used to calibrate the spectrometer is described. This includes details of the method used to determine detector positions and neutron flight path lengths as well as the determination of the instrument resolution. Examples of measurements on 3 different samples are shown, ZrH2, 4He and Sn which show the self-consistency of the calibration procedure.
Resumo:
The surface area of inhaled particles deposited in the alveolar region, as reported by the TSI nanoparticle surface area monitor (NSAM), was compared with the corresponding value estimated by a TSI scanning mobility particle sizer (SMPS) for a range of environmentally relevant aerosols, including petrol emissions, ETS, laser printer emissions, cooking emissions and ambient aerosols. The SMPS values were based on a mobility size distribution assuming spherical particles using the appropriate size-dependent alveolar-deposition factors provided by the ICRP. In most cases, the two instruments showed good linear agreement. With petrol emissions and ETS, the linearity extended to over 103 μm2 cm-3. With printer emissions, there was good linearity up to about 300 μm2 cm-3 while the NSAM increasingly overestimated the surface area at higher concentrations. The presence of a nucleation event in ambient air caused the NSAM to over-estimate the surface area by a factor of 2. We summarize these results and conclude that the maximum number concentration up to which the NSAM is accurate clearly depends on the type of aerosol being sampled and provide guidance for the use of the instrument.
Resumo:
c-axis-oriented YBa2Cu3O7-x (YBCO) thin films were laser deposited on (001) yttria-stabilized ZrO2 (YSZ) substrates with different surface morphologies. The in-plane orientation of the films on smooth substrates was sensitive to the deposition conditions, often resulting in mixed orientations. However, a strongly dominating [110] YBCO//[110]YSZ orientation was obtained at a deposition temperature of 770°C. Films on substrates with surface steps, induced by depositing a homoepitaxial buffer layer or by thermally annealing the substrate, had a [110]YBCO//[100]YSZ orientation when deposited at the same temperature. It was concluded that the [110]YBCO//[100] YSZ orientation was promoted by a graphoepitaxial mechanism. Films prepared under identical conditions on smooth and stepped substrates grew with extended c axes on the former. It is proposed that the extension can be induced by disorder, invoked by a low oxygen pressure and a low density of adsorption sites. The disorder may be eliminated by either an increase of the oxygen pressure or an increase of the density of adsorption sites in the form of steps. The film microstructure influenced the microwave surface resistance, which was similar for films with one exclusive in-plane orientation and higher for films with mixed orientations. The films on the stepped surfaces had superior superconducting properties; inductive measurements gave a Tc onset of 88 K, a ΔT(90%-10%) c of 0.2 K, and the transport jc was 1.5×106 A/cm2 at 83 K, for films on substrates with homoepitaxial buffer layers.
Resumo:
Gold is often considered as an inert material but it has been unequivocally demonstrated that it possesses unique electronic, optical, catalytic and electrocatalytic properties when in a nanostructured form.[1] For the latter the electrochemical behaviour of gold in aqueous media has been widely studied on a plethora of gold samples, including bulk polycrystalline and single-crystal electrodes, nanoparticles, evaporated films as well as electrodeposited nanostructures, particles and thin films.[1b, 2] It is now well-established that the electrochemical behaviour of gold is not as simple as an extended double-layer charging region followed by a monolayer oxide-formation/-removal process. In fact the so-called double-layer region of gold is significantly more complicated and has been investigated with a variety of electrochemical and surface science techniques. Burke and others[3] have demonstrated that significant processes due to the oxidation of low lattice stabilised atoms or clusters of atoms occur in this region at thermally and electrochemically treated electrodes which were confirmed later by Bond[4] to be Faradaic in nature via large-amplitude Fourier transformed ac voltammetric experiments. Supporting evidence for the oxidation of gold in the double-layer region was provided by Bard,[5] who used a surface interrogation mode of scanning electrochemical microscopy to quantify the extent of this process that forms incipient oxides on the surface. These were estimated to be as high as 20% of a monolayer. This correlated with contact electrode resistance measurements,[6] capacitance measurements[7] and also electroreflection techniques...
Resumo:
Chemical vapor deposition (CVD) is widely utilized to synthesize graphene with controlled properties for many applications, especially when continuous films over large areas are required. Although hydrocarbons such as methane are quite efficient precursors for CVD at high temperature (∼1000 °C), finding less explosive and safer carbon sources is considered beneficial for the transition to large-scale production. In this work, we investigated the CVD growth of graphene using ethanol, which is a harmless and readily processable carbon feedstock that is expected to provide favorable kinetics. We tested a wide range of synthesis conditions (i.e., temperature, time, gas ratios), and on the basis of systematic analysis by Raman spectroscopy, we identified the optimal parameters for producing highly crystalline graphene with different numbers of layers. Our results demonstrate the importance of high temperature (1070 °C) for ethanol CVD and emphasize the significant effects that hydrogen and water vapor, coming from the thermal decomposition of ethanol, have on the crystal quality of the synthesized graphene.
Resumo:
The thick piles of late-Archean volcaniclastic sedimentary successions that overlie the voluminous greenstone units of the eastern Yilgarn Craton, Western Australia, record the important transition from the cessation in mafic-ultramafic volcanism to cratonisation between about 2690 and 2655 Ma. Unfortunately, an inability to clearly subdivide the superficially similar sedimentary successions and correlate them between the various geological terranes and domains of the eastern Yilgarn Craton has led to uncertainty about the timing and nature of the region's palaeogeographic and palaeotectonic evolution. Here, we present the results of some 2025 U–Pb laser-ablation-ICP-MS analyses and 323 Sensitive High-Resolution Ion Microprobe (SHRIMP) analyses of detrital zircons from 14 late-Archean felsic clastic successions of the eastern Yilgarn Craton, which have enabled correlation of clastic successions. The results of our data, together with those compiled from previous studies, show that the post-greenstone sedimentary successions include two major cycles that both commenced with voluminous pyroclastic volcanism and ended with widespread exhumation and erosion associated with granite emplacement. Cycle One commences with an influx of rapidly reworked feldspar-rich pyroclastic debris. These units, here-named the Early Black Flag Group, are dominated by a single population of detrital zircons with an average age of 2690–2680 Ma. Thick (up to 2 km) dolerite bodies, such as the Golden Mile Dolerite, intrude the upper parts of the Early Black Flag Group at about 2680 Ma. Incipient development of large granite domes during Cycle One created extensional basins predominantly near their southeastern and northwestern margins (e.g., St Ives, Wallaby, Kanowna Belle and Agnew), into which the Early Black Flag Group and overlying coarse mafic conglomerate facies of the Late Black Flag Group were deposited. The clast compositions and detrital-zircon ages of the late Black Flag Group detritus match closely the nearby and/or stratigraphically underlying successions, thus suggesting relatively local provenance. Cycle Two involved a similar progression to that observed in Cycle One, but the age and composition of the detritus were notably different. Deposition of rapidly reworked quartz-rich pyroclastic deposits dominated by a single detrital-zircon age population of 2670–2660 Ma heralded the beginning of Cycle Two. These coarse-grained quartz-rich units, are name here the Early Merougil Group. The mean ages of the detrital zircons from the Early Merougil Group match closely the age of the peak in high-Ca (quartz-rich) granite magmatism in the Yilgarn Craton and thus probably represent the surface expression of the same event. Successions of the Late Merougil Group are dominated by coarse felsic conglomerate with abundant volcanic quartz. Although the detrital zircons in these successions have a broad spread of age, the principal sub-populations have ages of about 2665 Ma and thus match closely those of the Early Merougil Group. These successions occur most commonly at the northwestern and southeastern margins of the granite batholiths and thus are interpreted to represent resedimented units dominted by the stratigraphically underlying packages of the Early Merougil Group. The Kurrawang Group is the youngest sedimentary units identified in this study and is dominated by polymictic conglomerate with clasts of banded iron formation (BIF), granite and quartzite near the base and quartz-rich sandstone units containing detrital zircons aged up to 3500 Ma near the top. These units record provenance from deeper and/or more-distal sources. We suggest here that the principal driver for the major episodes of volcanism, sedimentation and deformation associated with basin development was the progressive emplacement of large granite batholiths. This interpretation has important implication for palaeogeographic and palaeotectonic evolution of all late-Archean terranes around the world.
Resumo:
Significance: Chronic wounds represent a major burden on global healthcare systems and reduce the quality of life of those affected. Significant advances have been made in our understanding of the biochemistry of wound healing progression. However, knowledge regarding the specific molecular processes influencing chronic wound formation and persistence remains limited. Recent Advances: Generally, healing of acute wounds begins with hemostasis and the deposition of a plasma-derived provisional matrix into the wound. The deposition of plasma matrix proteins is known to occur around the microvasculature of the lower limb as a result of venous insufficiency. This appears to alter limb cutaneous tissue physiology and consequently drives the tissue into a ‘preconditioned’ state that negatively influences the response to wounding. Critical Issues: Processes, such as oxygen and nutrient suppression, edema, inflammatory cell trapping/extravasation, diffuse inflammation, and tissue necrosis are thought to contribute to the advent of a chronic wound. Healing of the wound then becomes difficult in the context of an internally injured limb. Thus, interventions and therapies for promoting healing of the limb is a growing area of interest. For venous ulcers, treatment using compression bandaging encourages venous return and improves healing processes within the limb, critically however, once treatment concludes ulcers often reoccur. Future Directions: Improved understanding of the composition and role of pericapillary matrix deposits in facilitating internal limb injury and subsequent development of chronic wounds will be critical for informing and enhancing current best practice therapies and preventative action in the wound care field.