457 resultados para RAPID SYNTHESIS
Resumo:
Thermally stable mesoporous TiO2/SiO2 hybrid films with pore size of 50 nm have been synthesized by adopting the polymeric micelle-assembly method. A triblock copolymer, poly(styrene-b-2-vinyl pyridine-b-ethylene oxide), which serves as a template for the mesopores, was utilized to form polymeric micelles. The effective interaction of titanium tetraisopropoxide (TTIP) and tetraethyl orthosilicate (TEOS) with the polymeric micelles enabled us to fabricate stable mesoporous films. By changing the molar ratio of TEOS and TTIP, several mesoporous TiO2/SiO2 hybrid films with different compositions can be synthesized. The presence of amorphous SiO2 phase effectively retards the growth of anatase TiO2 crystal in the pore walls and retains the original mesoporous structure, even at higher temperature (650 °C). These TiO2/SiO2 hybrid films are of very high quality, without any cracks or voids. The addition of SiO2 phase to mesoporous TiO2 films not only adsorbs more organic dyes, but also significantly enhances the photocatalytic activity compared to mesoporous pure TiO2 film without SiO2 phase.
Resumo:
Controlling the morphology and size of titanium dioxide (TiO2) nanostructures is crucial to obtain superior photocatalytic, photovoltaic, and electrochemical properties. However, the synthetic techniques for preparing such structures, especially those with complex configurations, still remain a challenge because of the rapid hydrolysis of Ti-containing polymer precursors in aqueous solution. Herein, we report a completely novel approach-three- dimensional (3D) TiO2 nanostructures with favorable dendritic architectures-through a simple hydrothermal synthesis. The size of the 3D TiO2 dendrites and the morphology of the constituent nano-units, in the form of nanorods, nanoribbons, and nanowires, are controlled by adjusting the precursor hydrolysis rate and the surfactant aggregation. These novel configurations of TiO2 nanostructures possess higher surface area and superior electrochemical properties compared to nanoparticles with smooth surfaces. Our findings provide an effective solution for the synthesis of complex TiO2 nano-architectures, which can pave the way to further improve the energy storage and energy conversion efficiency of TiO 2-based devices.
Resumo:
Y2SiO5 has potential applications as a high-temperature structural ceramic and environmental/thermal barrier coating. In this work, we synthesized single-phase Y2SiO5 powders utilizing a solid-liquid reaction method with LiYO2 as an additive. The reaction path of the Y2O3/SiO2/LiYO2 mixture with variation in temperatures and the role of the LiYO2 additive on preparation process were investigated in detail. The powders obtained by this method have good sinterability. Through a pressureless sintering process, almost fully dense Y2SiO5 bulk material was achieved with a very high density of 99.7% theoretical.
Resumo:
In this article, a novel pressureless solid-liquid reaction method is presented for preparation of yttrium disilicate (γ-Y2Si2O7). Single-phase γ-Y2Si2O7 powder was synthesized by calcination of SiO2 and Y2O3 powders with the addition of LiYO2 at 1400 °C for 4 h. The addition of LiYO2 significantly decreased the synthesis temperature, shortened the calcination time, and enhanced the stability of γ-Y2Si2O7. The sintering of these powders in air and O2 was studied by means of thermal mechanical analyzer. It is shown that the γ-Y2Si2O7 sintered in oxygen had a faster densification rate and a higher density than that sintered in air. Furthermore, single-phase γ-Y2Si2O7 with a density of 4.0 g/cm3 (99% of the theoretical density) was obtained by pressureless sintering at 1400 °C for 2 h in oxygen. Microstructures of the sintered samples are studied by scanning electron microscope.
Resumo:
Nanoconfined synthesized crystalline fullerene mesoporous carbon (C60-FMC) with bimodal pore architectures of 4.95 nm and 10-15 nm pore sizes characterized by XRD, TEM, nitrogen adsorption/ desorption isotherm and solid-state NMR, and the material was used for protein immobilization. The solid-state 13C NMR spectrum of C60-FMC along with XRD, BET and TEM confirms the formation of fullerene mesoporous carbon structure C60-FMC. The immobilization of albumin (from bovine serum, BSA) protein biomolecule in a buffer solution at pH 4.7 was used to determine the adsorption properties of the C60-FMC material and its structural changes investigated by FT-IR. We demonstrated that the C60-FMC with high surface area and pore volumes have excellent adsorption capacity towards BSA protein molecule. Protein adsorption experiments clearly showed that the C60-FMC with bimodal pore architectures (4.95 nm and 10-15 nm) are suitable material to be used for protein adsorption
Resumo:
Highly ordered mesoporous carbon (MC) has been synthesized from sucrose, a non-toxic and costeffective source of carbon. X-ray diffraction, N2 adsorption–desorption isotherm and transmission electron micrograph (TEM) were used to characterize the MC. The XRD patterns show the formation of highly ordered mesoporous structures of SBA15 and mesoporous carbon. The N2 adsorptiondesorption isotherms suggest that the MC exhibits a narrow pore-size distribution with high surface area of 1559 m2/g. The potential application of MC as a novel electrode material was investigated using cyclic voltammetry for riboflavin (vitamin B2) and dopamine. MC-modified glassy carbon electrode (MC/GC) shows increase in peak current compared to GC electrode in potassium ferricyanide which clearly suggest that MC/GC possesses larger electrode area (1.8 fold) compared with bare GC electrode. The electrocatalytic behavior of MC/GC was investigated towards the oxidation of riboflavin (vitamin B2) and dopamine using cyclic voltammetry which show larger oxidation current compared to unmodified electrode and thus MC/GC may have the potential to be used as a chemically modified electrode.
Resumo:
We report the synthesis and characterisation of new examples of meso-hydroxynickel(II) porphyrins with 5,15-diphenyl and 10-phenyl-5,15-diphenyl/diaryl substitu- tion. The OH group was introduced by using carbonate or hydroxide as nucleophile by using palladium/phosphine cat- alysis. The NiPor OHs exist in solution in equilibrium with the corresponding oxy radicals NiPor OC. The 15-phenyl group stabilises the radicals, so that the 1H NMR spectra of {NiPor OH} are extremely broad due to chemical exchange with the paramagnetic species. The radical concentration for the diphenylporphyrin analogue is only 1%, and its NMR line-broadening was able to be studied by variable-tempera- ture NMR spectroscopy. The EPR signals of NiPor OC are con- sistent with somewhat delocalised porphyrinyloxy radicals, and the spin distributions calculated by using density func- tional theory match the EPR and NMR spectroscopic obser- vations. Nickel(II) meso-hydroxy-10,20-diphenylporphyrin was oxidatively coupled to a dioxo-terminated porphodimethene dyad, the strongly red-shifted electronic spectrum of which was successfully modelled by using time-dependent DFT calculations.