430 resultados para Molecular films
Resumo:
The development of novel organic polymer thin films is essential for the advancement of many emerging fields including organic electronics and biomedical coatings. In this study, the effect of synthesis conditions, namely radio frequency (rf) deposition power, on the material properties of polyterpenol thin films derived from nonsynthetic environmentally friendly monomer was investigated. At lower deposition powers, the polyterpenol films preserved more of the original monomer constituents, such as hydroxy functional groups; however, they were also softer and more hydrophilic compared to polymers fabricated at higher power. Enhanced monomer fragmentation and consequent reduction in the presence of the polar groups in the structure of the high-power samples reduced their optical band gap value from 2.95 eV for 10 W to 2.64 eV for 100 W. Regardless of deposition power, all samples were found to be optically transparent with smooth, defect-free, and homogenous surfaces.
Resumo:
In the fields of organic electronics and biotechnology, applications for organic polymer thin films fabricated using low-temperature non-equilibrium plasma techniques are gaining significant attention because of the physical and chemical stability of thin films and the low cost of production. Polymer thin films were fabricated from non-synthetic terpinen-4-ol using radiofrequency polymerization (13.56 MHz) on low loss dielectric substrates and their permittivity properties were ascertained to determine potential applications for these organic films. Real and imaginary parts of permittivity as a function of frequency were measured using the variable angle spectroscopic ellipsometer. The real part of permittivity (k) was found to be between 2.34 and 2.65 in the wavelength region of 400–1100 nm, indicating a potential low-k material. These permittivity values were confirmed at microwave frequencies. Dielectric properties of polyterpenol films were measured by means of split post dielectric resonators (SPDRs) operating at frequencies of 10 GHz and 20 GHz. Permittivity increased for samples deposited at higher RF energy – from 2.65 (25 W) to 2.83 (75 W) measured by a 20-GHz SPDR and from 2.32 (25 W) to 2.53 (100 W) obtained using a 10-GHz SPDR. The error in permittivity measurement was predominantly attributed to the uncertainty in film thickness measurement.
Resumo:
Organic plasma polymers are currently attracting significant interest for their potential in the areas of flexible optoelectronics and biotechnology. Thin films of plasma-polymerized polyterpenol fabricated under varied deposition conditions were studied using nanoindentation and nanoscratch analyses. Coatings fabricated at higher deposition power were characterized by improved hardness, from 0.33 GPa for 10 W to 0.51 GPa for 100 W at 500-μN load, and enhanced wear resistance. The elastic recovery was estimated to be between 0.1 and 0.14. Coatings deposited at higher RF powers also showed less mechanical deformation and improved quality of adhesion. The average (R a) and root mean square (R q) surface roughness parameters decreased, from 0.44 nm and 0.56 nm for 10 W to 0.33 nm and 0.42 nm for 100 W, respectively.
Resumo:
This study presents the effect of iodine doping on optical and surface properties of polyterpenol thin films deposited from non-synthetic precursor by means of plasma polymerisation. Spectroscopic ellipsometry studies showed iodine doping reduced the optical band gap from 2.82 eV to 1.50 eV for pristine and doped samples respectively. Higher levels of doping notably reduced the transparency of films, an issue if material is considered for applications that require high transparency. Contact angle studies demonstrated higher hydrophilicity for films deposited at increased doping levels, results confirmed by XPS Spectroscopy and FTIR. Doping had no significant effect on the surface profile or roughness of the film.
Resumo:
Owing to the structural flexibility, uncomplicated processing and manufacturing capabilities, plasma polymers are the subject of active academic as well as industrial research. Polymer thin films prepared from non-synthetic monomers combine desirable optical and physical properties with biocompatibility and environmental sustainability. However, the ultimate expediency and implementation of such materials will dependent on the stability of these properties under varied environmental conditions. Polyterpenol thin films were manufactured at different deposition powers. Under ambient conditions, the bulk of ageing occurred within first 150h after deposition and was attributed to oxidation and volumetric relaxation. Films observed for further 12 months showed no significant changes in thickness or refractive index. Thermal degradation behaviour indicated thermal stability increased for the films manufactured at higher RF powers. Annealing the films to 405°C resulted in full degradation, with retention between 0.29 and 0.99%, indicating films' potential as sacrificial material.
Resumo:
Poly(linalool) thin films were fabricated using RF plasma polymerisation. All films were found to be smooth, defect-free surfaces with average roughness of 0.44 nm. The FTIR analysis of the polymer showed a notable reduction in –OH moiety and complete dissociation of C=C unsaturation compared to the monomer, and presence of a ketone band absent from the spectrum of the monomer. Poly(linalool) were characterised by chain branching and a large quantity of short polymer chains. Films were optically transparent, with refractive index and extinction coefficient of 1.55 and 0.001 (at 500 nm) respectively, indicating a potential application as an encapsulating (protective) coating for circuit boards. The optical band gap was calculated to be 2.82 eV, which is in the semiconducting energy gap region.
Resumo:
This paper describes the synthesis and characterization of a novel organic polymer coating for the prevention of the growth of Pseudomonas aeruginosa on the solid surface of three-dimensional objects. Substrata were encapsulated with polyterpenol thin films prepared from terpinen-4-ol using radio frequency plasma enhanced chemical vapor deposition. Terpinen-4-ol is a constituent of tea tree oil with known antibacterial properties. The influence of deposition power on the chemical structure, surface composition, and ultimately the antibacterial inhibitory activity of the resulting polyterpenol thin films was studied using X-ray photoelectron spectroscopy (XPS), water contact angle measurement, atomic force microscopy (AFM), and 3-D interactive visualization and statistical approximation of the topographic profiles. The experimental results were consistent with those predicted by molecular simulations. The extent of bacterial attachment and extracellular polymeric substances (EPS) production was analyzed using scanning electron microscopy (SEM) and confocal scanning laser microscopy (CSLM). Polyterpenol films deposited at lower power were particularly effective against P. aeruginosa due to the preservation of original terpinen-4-ol molecules in the film structure. The proposed antimicrobial and antifouling coating can be potentially integrated into medical and other clinically relevant devices to prevent bacterial growth and to minimize bacteria-associated adverse host responses.
Resumo:
Terpinen-4-ol is the main constituent of Melaleuca alternifolia essential oil known for its biocidal and anti-inflammatory properties. The possibility of fabricating polymer thin films from terpinen-4-ol using radio frequency (RF) plasma polymerisation for the prevention of the growth of Pseudomonas aeruginosa was investigated, and the properties of the resultant films compared against their biologically active precursor. Films fabricated at 10 W prevented bacterial attachment and EPS secretion, whilst polyterpenol films deposited at 25 W demonstrated no biocidal activity against the pathogen.
Resumo:
Recent advancements in the area of organic polymer applications demand novel and advanced materials with desirable surface, optical and electrical properties to employ in emerging technologies. This study examines the fabrication and characterization of polymer thin films from non-synthetic Terpinen-4-ol monomer using radio frequency plasma polymerization. The optical properties, thickness and roughness of the thin films were studied in the wavelength range 200–1000 nm using ellipsometry. The polymer thin films of thickness from 100 nm to 1000 nm were fabricated and the films exhibited smooth and defect-free surfaces. At 500 nm wavelength, the refractive index and extinction coefficient were found to be 1.55 and 0.0007 respectively. The energy gap was estimated to be 2.67 eV, the value falling into the semiconducting Eg region. The obtained optical and surface properties of Terpinen-4-ol based films substantiate their candidacy as a promising low-cost material with potential applications in electronics, optics, and biomedical industries.
Resumo:
Linkage with essential hypertension has been claimed for a microsatellite marker near the angiotensinogen gene (AGT; chromosome 1q42), as has association for the AGT variants M235T, G(-6)A and A(-20)C. To more rigorously evaluate AGT as a candidate gene for hypertension we performed sibpair analysis with multiple microsatellite markers surrounding this locus and using more sophisticated analysis programs. We also performed an association study of the AGT variants in unrelated subjects with a strong family history (two affected parents). For the linkage study, single and multiplex polymerase chain reaction (PCRs) and automated genescan analysis were conducted on DNA from 175 Australian Anglo-Celtic Caucasian hypertensives for the following markers: D1S2880-(2.1 cM)-D1S213-(2.8 cM)-D1S251-(6.5 cM)-AGT-(2.0 cM) -D1S235. Statistical evaluation of genotype data by nonparametric methods resulted in the following scores: Single-point analysis - SPLINK, P > 0.18; APM method, P > 0.25; ASPEX, MLOD < 0.28; SIB-PAIR, P > 0. 24; Multipoint analysis - MAPMAKER/SIBS, MLOD < 0.24; GENEHUNTER, P > 0.35. Exclusion scores of Lod -4.1 to -5.1 were obtained for these markers using MAPMAKER/SIBS for a lambda(s) of 1.6. The association study of G(-6)A, A(-20)C and M235T variants in 111 hypertensives with strong family history and 190 normotensives with no family history showed significant linkage disequilibrium between particular haplotypes, but we could find no association with hypertension. The present study therefore excludes AGT in the etiology of hypertension, at least in the population of Australian Anglo-Celtic Caucasians studied.