79 resultados para silicone rubber
Resumo:
A fractal method was introduced to quantitatively characterize the dispersibility of modified kaolinite (MK) and precipitated silica (PS) in styrene–butadiene rubber (SBR) matrix based on the lower magnification transmission electron microscopic images. The fractal dimension (FD) is greater, and the dispersion is worse. The fractal results showed that the dispersibility of MK in the latex blending sample is better than that in the mill blending samples. With the increase of kaolinite content, the FD increases from 1.713 to 1.800, and the dispersibility of kaolinite gradually decreases. There is a negative correlation between the dispersibility and loading content. With the decrease of MK and increase of PS, the FD significantly decreases from 1.735 to 1.496 and the dipersibility of kaolinite remarkably increases. The hybridization can improve the dispersibility of fillers in polymer matrix. The FD can be used to quantitatively characterize the aggregation and dispersion of kaolinite sheets in rubber matrix.
Resumo:
A series of rubber composites were prepared by blending styrene-butadiene rubber (SBR) latex and the different particle sized kaolinites. The thermal stabilities of the rubber composites were characterized using thermogravimetry, digital photography, scanning electron microscopy, X-ray diffraction, Fourier transform infrared spectroscopy, and Raman spectroscopy. Kaolinite SBR composites showed much greater thermal stability when compared with that of the pure SBR. With the increase of kaolinite particle size, the pyrolysis products became much looser; the char layer and crystalline carbon content gradually decreased in the pyrolysis residues. The pyrolysis residues of the SBR composites filled with the different particle sized kaolinites showed some remarkable changes in structural characteristics. The increase of kaolinite particle size was not beneficial to form the compact and stable crystalline carbon in the pyrolysis process, and resulted in a negative influence in improving the thermal stability of kaolinite/SBR composites.
Resumo:
Cross-link density, microstructure and mechanical properties of styrene butadiene rubber (SBR) composites filled with different particle sized kaolinites are investigated. With the increase of kaolinite particle size, the cross-link density of the filled SBR composites, the dispersibility and orientation degree of kaolinite particles gradually decrease. Some big cracks in filled rubber composites are distributed along the fringe of kaolinite aggregates, and the absorbance of all the absorption bands of kaolinites gradually increase with the increase of kaolinite particle size. All mechanical property indexes of kaolinite filled SBR composites decrease due to the decrease of cross-linking and reduction of interface interaction between filler and rubber matrix.
Resumo:
We thank Dr Shedden and Dr Pall for their insightful comments and the opportunity to clarify a number of points from our work.1 The “protection factor” (PF) expressed as the inverse of the transmittance of contact lens (CL) material (1/Tλ), where T is the percentage transmittance of ultraviolet radiation (UVR) in a given waveband (UVC, UVB or UVA) of the UV spectrum for contact lenses is the standard method for reporting PF values and as such there should not be any controversy. We have calculated the PF for each wavelength across the entire UV spectrum (UVC, UVB, UVA) as presented in figure 3 of our previous publication.1 In that article, we were simply stating the observation when transmission in the UVC spectra band is considered especially because appreciable amounts of potentially carcinogenic short UV wavelengths was shown to be present in sunlight in our region three decades ago2 and these short wavelength photons are reported to be more biologically damaging to ocular tissues.3 In addition, the depletion of the Ozone layer is still continuing. Nevertheless, we understand the concern of the authors that the results of the PF might be confusing to those who are not familiar with the science of UVR and as such we have made some revisions to the findings of the calculated PF...
Resumo:
A 60-year-old male experienced a marked unilateral myopic shift of 20 D following attempted removal of intravitreal heavy silicone oil (HSO) used in the treatment of inferior proliferative vitreous retinopathy following retinal detachment. Examination revealed HSO adherent to the corneal endothelium forming a convex interface with the aqueous, obscuring the entire pupil, which required surgical intervention to restore visual acuity. This case highlights the potential ocular complications associated with silicone oil migration into the anterior chamber, which include corneal endothelial decompensation and a significant increase in myopia.
Resumo:
Cosmetically tinted soft contact lenses are an attractive option for contact lens wearers. Data that we have gathered from annual contact lens fitting surveys demonstrate that those wearing tinted lenses are more likely to be female (4.6% of all soft lenses fitted vs. 1.6% for males; p < 0.0001) and younger (27 11 years vs. 33 13 years for those wearing non-tinted lenses; p < 0.0001). Tinted lenses tend to be worn more on a part-time basis and are replaced less frequently than non-tinted lenses. The decline in fitting tinted lenses over the past 12 years may be due to (a) the current limited availability of tinted lenses in silicone hydrogel materials and daily disposable replacement frequencies, which together represent a significant majority (78%) of new soft lenses fits today, (b) growing concerns among lens wearers and practitioners relating to the risks of complications associated with the wearing of tinted lenses, and (c) reduced promotion of such lenses by the contact lens industry.
Resumo:
Despite the current market popularity of silicone hydrogel contact lenses, conventional hydrogel lenses still represent a significant proportion of the overall contact lens market. Data gathered from annual UK contact lens fitting surveys over the past 13 years indicate that 64% of hydrogel lenses prescribed during this period were of low/medium water content (<60% water). Whereas, in the past, practitioners would choose the water content of a hydrogel lens to meet specific clinical needs, this choice appears today to be largely governed by product availability.
Resumo:
Objectives. To evaluate the performance of the dynamic-area high-speed videokeratoscopy technique in the assessment of tear film surface quality with and without the presence of soft contact lenses on eye. Methods. Retrospective data from a tear film study using basic high-speed videokeratoscopy, captured at 25 frames per second, (Kopf et al., 2008, J Optom) were used. Eleven subjects had tear film analysis conducted in the morning, midday and evening on the first and seventh day of one week of no lens wear. Five of the eleven subjects then completed an extra week of hydrogel lens wear followed by a week of silicone hydrogel lens wear. Analysis was performed on a 6 second period of the inter-blink recording. The dynamic-area high-speed videokeratoscopy technique uses the maximum available area of Placido ring pattern reflected from the tear interface and eliminates regions of disturbance due to shadows from the eyelashes. A value of tear film surface quality was derived using image rocessing techniques, based on the quality of the reflected ring pattern orientation. Results. The group mean tear film surface quality and the standard deviations for each of the conditions (bare eye, hydrogel lens, and silicone hydrogel lens) showed a much lower coefficient of variation than previous methods (average reduction of about 92%). Bare eye measurements from the right and left eyes of eleven individuals showed high correlation values (Pearson’s correlation r = 0.73, p < 0.05). Repeated measures ANOVA across the 6 second period of measurement in the normal inter-blink period for the bare eye condition showed no statistically significant changes. However, across the 6 second inter-blink period with both contact lenses, statistically significant changes were observed (p < 0.001) for both types of contact lens material. Overall, wearing hydrogel and silicone hydrogel lenses caused the tear film surface quality to worsen compared with the bare eye condition (repeated measures ANOVA, p < 0.0001 for both hydrogel and silicone hydrogel). Conclusions. The results suggest that the dynamic-area method of high-speed videokeratoscopy was able to distinguish and quantify the subtle, but systematic worsening of tear film surface quality in the inter-blink interval in contact lens wear. It was also able to clearly show a difference between bare eye and contact lens wearing conditions.
Resumo:
In paper has been to investigate the morphological patterns and kinetics of PDMS spreading on silicon wafer using combination of techniques like ellipsometry, atomic force microscope (AFM), scanning electron microscope (SEM) and optical microscopy. A macroscopic silicone oil drops as well as PDMS water based emulsions were studied after deposition on a flat surface of silicon wafer in air, water and vacuum. our own measurements using an imaging ellipsometer, which also clearly shows the presence of a precursor film. The diffusion constant of this film, measured with a 60 000 cS PDMS sample spreading on a hydrophilic silicon wafer, is Df = 1.4 10-11 m2/s. Regardless of their size, density and method of deposition, droplets on both types of wafer (hydrophilic and hydrophobic) flatten out over a period of many hours, up to 3 days. During this process neighbouring droplets may coalesce, but there is strong evidence that some of the PDMS from the droplets migrates into a thin, continuous film that covers the surface in between droplets. The thin film appears to be ubiquitous if there has been any deposition of PDMS. However, this statement needs further verification. One question is whether the film forms immediately after forced drying, or whether in some or all cases it only forms by spreading from isolated droplets as they slowly flatten out.
Resumo:
Noise and vibration in complex ship structures are becoming a prominent issue for ship building industry and ship companies due to the constant demand of building faster ships of lighter weight, and the stringent noise and libration regulation of the industry. In order to retain the full benefit of building faster ships without compromising too much on ride comfort and safety, noise and vibration control needs to be implemented. Due to the complexity of ship structures, the coupling of different wave types and multiple wave propagation paths, active control of global hull modes is difficult to implement and very expensive. Traditional passive control such as adding damping materials is only effective in the high frequency range. However, most severe damage to ship structures is caused by large structural deformation of hull structures and high dynamic stress concentration at low frequencies. The most discomfort and fatigue of passengers and the crew onboard ships is also due to the low frequency noise and vibration. Innovative approaches are therefore, required to attenuate the noise and vibration at low frequencies. This book was developed from several specialized research topics on vibration and vibration control of ship structures, mostly from the author's own PhD work at the University of Western Australia. The book aims to provide a better understanding of vibration characteristics of ribbed plate structures, plate/plate coupled structures and the mechanism governing wave propagation and attenuation in periodic and irregular ribbed structures as well as in complex ship structures. The book is designed to be a reference book for ship builders, vibro-acoustic engineers and researchers. The author also hopes that the book can stimulate more exciting future work in this area of research. It is the author's humble desire that the book can be some use for those who purchase it. This book is divided into eight chapters. Each chapter focuses on providing solution to address a particular issue on vibration problems of ship structures. A brief summary of each chapter is given in the general introduction. All chapters are inter-dependent to each other to form an integration volume on the subject of vibration and vibration control of ship structures and alike. I am in debt to many people in completing this work. In particular, I would like to thank Professor J. Pan, Dr N.H. Farag, Dr K. Sum and many others from the University of Western Australia for useful advices and helps during my times at the University and beyond. I would also like to thank my wife, Miaoling Wang, my children, Anita, Sophia and Angela Lin, for their sacrifice and continuing supports to make this work possible. Financial supports from Australian Research Council, Australian Defense Science and Technology Organization and Strategic Marine Pty Ltd at Western Australia for this work is gratefully acknowledged.
Resumo:
The formation of hypertrophic scars is a frequent medical outcome of wound repair and often requires further therapy with treatments such as Silicone Gel Sheets (SGS) or apoptosis-inducing agents, including bleomycin. Although widely used, knowledge regarding SGS and their mode of action is limited. Preliminary research has shown that small amounts of amphiphilic silicone present in SGS have the ability to move into skin during treatment. We demonstrate herein that a commercially available analogue of these amphiphilic siloxane species, the rake copolymer GP226, decreases collagen synthesis upon exposure to cultures of fibroblasts derived from hypertrophic scars (HSF). By size exclusion chromatography, GP226 was found to be a mixture of siloxane species, containing five fractions of different molecular weight. By studies of collagen production, cell viability and proliferation, it was revealed that a low molecular weight fraction (fraction IV) was the most active, reducing the number of viable cells present following treatment and thereby reducing collagen production as a result. Upon exposure of fraction IV to human keratinocytes, viability and proliferation was also significantly affected. HSF undergoing apoptosis after application of fraction IV were also detected via real-time microscopy and by using the TUNEL assay. Taken together, these data suggests that these amphiphilic siloxanes could be potential non-invasive substitutes to apoptotic-inducing chemical agents that are currently used as scar treatments.
Resumo:
An investigation has been made of the interactions between silicone oil and various solid substrates immersed in aqueous solutions. Measurements were made using an atomic force microscope (AFM) using the colloid-probe method. The silicone oil drop is simulated by coating a small silica sphere with the oil, and measuring the force as this coated sphere is brought close to contact with a flat solid surface. It is found that the silicone oil surface is negatively charged, which causes a double-layer repulsion between the oil drop and another negatively charged surface such as mica. With hydrophilic solids, this repulsion is strong enough to prevent attachment of the drop to the solid. However, with hydrophobic surfaces there is an additional attractive force which overcomes the double-layer repulsion, and the silicone oil drop attaches to the solid. A "ramp" force appears in some, but not all, of the data sets. There is circumstantial evidence that this force results from compression of the silicone oil film coated on the glass sphere.
Resumo:
In order to effect permanent closure in burns patients suffering from full thickness wounds, replacing their skin via split thickness autografting, is essential. Dermal substitutes in conjunction with widely meshed split thickness autografts (+/- cultured keratinocytes) reduce scarring at the donor and recipient sites of burns patients by reducing demand for autologous skin (both surface area and thickness), without compromising dermal delivery at the wound face. Tissue engineered products such as Integra consist of a dermal template which is rapidly remodelled to form a neodermis, at which time the temporary silicone outer layer is removed and replaced with autologous split thickness skin. Whilst provision of a thick tissue engineered dermis at full thickness burn sites reduces scarring, it is hampered by delays in vascularisation which results in clinical failure. The ultimate success of any skin graft product is dependent upon a number of basic factors including adherence, haemostasis and in the case of viable tissue grafts, success is ultimately dependent upon restoration of a normal blood supply, and hence this study. Ultimately, the goal of this research is to improve the therapeutic properties of tissue replacements, through impregnation with growth factors aimed at stimulating migration and proliferation of microvascular endothelial cells into the donor tissue post grafting. For the purpose of my masters, the aim was to evaluate the responsiveness of a dermal microvascular endothelial cell line to growth factors and haemostatic factors, in the presence of the glycoprotein vitronectin. Vitronectin formed the backbone for my hypothesis and research due to its association with both epithelial and, more specifically, endothelial migration and proliferation. Early work using a platform technology referred to as VitroGro (Tissue Therapies Ltd), which is comprised of vitronectin bound BP5/IGF-1, aided keratinocyte proliferation. I hypothesised that this result would translate to another epithelium - endothelium. VitroGro had no effect on endothelial proliferation or migration. Vitronectin increases the presence of Fibroblast Growth Factor (FGF) and Vascular Endothelial Growth Factor (VEGF) receptors, enhancing cell responsiveness to their respective ligands. So, although Human Microvascular Endothelial Cell line 1 (HMEC-1) VEGF receptor expression is generally low, it was hypothesised that exposure to vitronectin would up-regulate this receptor. HMEC-1 migration, but not proliferation, was enhanced by vitronectin bound VEGF, as well as vitronectin bound Epidermal Growth Factor (EGF), both of which could be used to stimulate microvascular endothelial cell migration for the purpose of transplantation. In addition to vitronectin's synergy with various growth factors, it has also been shown to play a role in haemostasis. Vitronectin binds thrombin-antithrombin III (TAT) to form a trimeric complex that takes on many of the attributes of vitronectin, such as heparin affinity, which results in its adherence to endothelium via heparan sulfate proteoglycans (HSP), followed by unaltered transcytosis through the endothelium, and ultimately its removal from the circulation. This has been documented as a mechanism designed to remove thrombin from the circulation. Equally, it could be argued that it is a mechanism for delivering vitronectin to the matrix. My results show that matrix-bound vitronectin dramatically alters the effect that conformationally altered antithrombin three (cATIII) has on proliferation of microvascular endothelial cells. cATIII stimulates HMEC-1 proliferation in the presence of matrix-bound vitronectin, as opposed to inhibiting proliferation in its absence. Binding vitronectin to tissues and organs prior to transplant, in the presence of cATIII, will have a profound effect on microvascular infiltration of the graft, by preventing occlusion of existing vessels whilst stimulating migration and proliferation of endothelium within the tissue.