140 resultados para porous silicon


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Insulating nanoporous materials are promising platforms for soft-ionizing membranes; however, improvement in fabrication processes and the quality and high breakdown resistance of the thin insulator layers are needed for high integration and performance. Here, scalable fabrication of highly porous, thin, silicon dioxide membranes with controlled thickness is demonstrated using plasma-enhanced chemical-vapor-deposition. The fabricated membranes exhibit good insulating properties with a breakdown voltage of 1 × 107 V/cm. Our calculations suggest that the average electric field inside a nanopore of the membranes can be as high as 1 × 106 V/cm; sufficient for ionization of wide range of molecules. These metal–insulator–metal nanoporous arrays are promising for applications such soft ionizing membranes for mass spectroscopy.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Silicon batteries have attracted much attention in recent years due to their high theoretical capacity, although a rapid capacity fade is normally observed, attributed mainly to volume expansion during lithiation. Here, we report for the first time successful synthesis of Si/void/SiO2/void/C nanostructures. The synthesis strategy only involves selective etching of SiO2 in Si/SiO2/C structures with hydrofluoric acid solution. Compared with reported results, such novel structures include a hard SiO2-coated layer, a conductive carbon-coated layer, and two internal void spaces. In the structures, the carbon can enhance conductivity, the SiO2 layer has mechanically strong qualities, and the two internal void spaces can confine and accommodate volume expansion of silicon during lithiation. Therefore, these specially designed dual yolk-shell structures exhibit a stable and high capacity of 956 mA h g−1 after 430 cycles with capacity retention of 83%, while the capacity of Si/C core-shell structures rapidly decreases in the first ten cycles under the same experimental conditions. The novel dual yolk-shell structures developed for Si can also be extended to other battery materials that undergo large volume changes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Porous titanium dioxide synthesized with a bicontinuous surfactant template is a promising method that leads to a high active surface area electrode. The template used is based on a water/isooctane/dioctyl sodium sulfosuccinate salt together with lecithin. Several parameters were varied during the synthesis to understand and optimize channel formation mechanisms. The material is patterned in stacked conical channels, widening towards the centre of the grains. The active surface area increased by 116% when the concentration of alkoxide precursors was decreased and increased by 241% when the template formation temperature was decreased to 10C. Increasing the oil phase viscosity tends to widen the pore aperture, thus decreasing the overall active surface area. Changing the phase proportions alters the microemulsion integrity and disrupts channel formation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Intermittent microwave convective (IMCD) drying is an advanced drying technology that improves both energy efficiency and food quality during the drying of food materials. Despite numerous experimental studies available for IMCD, there is no complete multiphase porous media model available to describe the process. A multiphase porous media model considering liquid water, gases and the solid matrix inside the food during drying can provide in depth understanding of IMCD. In this article, firstly a multiphase porous media model was developed for IMCD. Then the model is validated against experimental data by comparing moisture content and temperature distributions after each heating and tempering periods. The profile of vapour pressures and evaporation during IMCD are presented and discussed. The relative contribution of water and vapour fluxes due to gas pressure and diffusion demonstrated that the fluxes due are relatively higher in IMCD compared to convection drying and this makes the IMCD faster.