A one-step melt-mixing method is proposed to study dispersion and re-agglomeration phenomena of the as-received and functionalized graphite nanoplates in polypropylene melts. Graphite nanoplates were chemically modified via 1,3-dipolar cycloaddition of an azomethine ylide and then grafted with polypropylene-graft-maleic anhydride. The effect of surface functionalization on the dispersion kinetics, nanoparticle re-agglomeration and interface bonding with the polymer is investigated. Nanocomposites with 2 or 10 wt% of as-received and functionalized graphite nanoplates were prepared in a small-scale prototype mixer coupled to a capillary rheometer. Samples were collected along the flow axis and characterized by optical microscopy, scanning electron microscopy and electrical conductivity measurements. The as-received graphite nanoplates tend to re-agglomerate upon stress relaxation of the polymer melt. The covalent attachment of a polymer to the nanoparticle surface enhances the stability of dispersion, delaying the re-agglomeration. Surface modification also improves interfacial interactions and the resulting composites presented improved electrical conductivity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Artigo publicado a convite da Society for Polymer Engineers

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Due to the increasing need of low voltage actuators, independent from electrochemical processes, electroactive actuators based on poly(vinylidene fluoride) composites with 10, 25 and 40 % of 1-ethyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide, [C2mim] [NTf2], ionic liquid are prepared by solvent casting and melting. We show that the charge structure of [C2mim] [NTf2] induces the complete piezoelectric -phase crystallization of the PVDF within the composite and decreases its crystallinity fraction significantly. [C2mim] [NTf2] also works as a plasticizer of PVDF, reducing the elastic modulus down to 12 % of the initial value. Moreover, the composites show significant displacement and bending under applied voltages of 2, 5 and 10 Vpp. The displacement and bending of the composite membranes are also evaluated as a function of [C2mim] [NTf2] content and sample thickness. Increasing amounts of ionic liquid result in larger deformations independently of the applied voltage.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(vinylidene fluoride), PVDF, has been blended with different ionic liquids (IL) in order to evaluate the effect of the different IL anions and cations on the electroative -phase, thermal, mechanical and electrical properties of the polymer blend. [C2MIM][Cl], [C6MIM][Cl], [C10MIM][Cl], [C2MIM][NTf2], [C6MIM][NTf2], [C10MIM][NTf2] have been selected and were introduced in the polymer at a weight percentage of 40 wt%. It was found that the incorporation of ILs into the PVDF matrix leads to an increase of the -phase content due to the strong electrostatic interactions between the dipolar moments of PVDF and the ILs. Further, the incorporation of ILs into PVDF strongly decreases the elastic modulus and increases the electrical conductivity of the blend with respect to the pure polymer matrix, all these effects being accompanied by a modification of the crystallization kinetics, as indicated by the modified spherulitic microstructure. Thus, novel PVDF/IL blends films with high transparency, excellent antistatic properties, and highly polar crystal form fraction were successfully achieved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of different anions within the ionic liquid in the characteristics of solid polymer electrolytes (SPEs) based on P(VDF-TrFE) has been investigated. 1-ethyl-3-methylimidazolium acetate, [C2mim][OAc], 1-ethyl-3-methylimidazolium triflate, [C2mim][(CF3SO3)3], 1-ethyl-3-methylimidazolium lactate, [C2mim][Lactate], 1-ethyl-3-methylimidazolium thiocyanate, [C2mim][SNC] and 1-ethyl-3-methylimidazolium hydrogen sulphate [C2mim][HSO4] have been used in SPE prepared by thermally induced phase separation (TIPS). The polymer phase, thermal and electrochemical properties of the SPE have been determined. The thermal and electrical properties of the SPEs strongly depend on the selected IL, as determined by their different interactions with the polymer matrix. The room temperature ionic conductivity increases in the following way for the different anions: [SNC] > [CF3SO3)3] > [HSO4] > [Lactate] > [OAc], which is mainly dependent on the viscosity of the ionic liquid.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The sol-gel method was employed in the synthesis of di-urethane cross-linked poly( caprolactone) (PCL(530)/siloxane biohybrid ormolytes incorporating either a mixture of lithium triflate (LiCF3SO3) and the ionic liquid (IL) 1-ethyl-3-methyl imidazolium tetrafluoroborate ([Emim]BF4), or solely with [Emim]BF4 or LiCF3SO3. The ormolyte doped with [Emim]BF4 is thermally more stable and exhibits higher ionic conductivity (4 x 10-4 and 2 x 10-3 S cm-1 at 36 and 98 ºC, respectively) than those containing the LiCF3SO3/[Emim]BF4 mixture or just LiCF3SO3. The three ormolytes were employed in the production of glass/ITO/ormolyte/WO3/ITO/glass electrochromic devices (ECDs) designated as ECD@Y with Y = Li-[Emim]BF4, [Emim]BF4 and Li. The three ECDs displayed fast switching speed (ca. 30 s). ECD@Li-[Emim]BF4 exhibited an electrochromic contrast of 18.4 % and an optical density change of 0.11 in the visible region, the coloration efficiency attained at 555 nm was 159 and 80.2 cm-2 C-1 in the “on” and “off” states, respectively, and the open circuit memory was 48 hours. In the “on” state the CIE 1931 color space coordinates were x = 0.29 and y = 0.30, corresponding to blue color.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The sol-gel method was employed in the synthesis of di-urethane cross-linked poly(-caprolactone) (d-PCL(530)/siloxane biohybrid ormolytes incorporating copper perchlorate, (Cu(ClO4)2). The highest ionic conductivity of the d PCL(530)/siloxanenCu(ClO4)2 system is that with n = 10 (1.4 x 10-7 and 1.4 x 10-5 S cm-1, at 25 and 100 ºC, respectively). In an attempt to understand the ionic conductivity/ionic association relationship, we decide to inspect the chemical environment experienced by the Cu2+ ions in the d-PCL(530)/siloxane medium. The observed EPR spectra are typical of isolated monomeric Cu2+ ions in axially distorted sites. The molecular orbital coefficients obtained from the EPR spin Hamiltonian parameters and the optical absorption band suggests that bonding between the Cu2+ and its ligand in the ormolytes are moderately ionic. Investigation by photoluminescence spectroscopy did not evidence or allow selective excitation of transitions corresponding to complexed Cu2+ species.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

New polymer electrolytes (PEs) based on chitosan and three ionic liquid (IL) families ([C2mim][CnSO3], [C2mim][CnSO4] and [C2mim][diCnPO4]) were synthesized by the solvent casting method. The effect of the length of the alkyl chain of the IL anion on the thermal, morphological and electrochemical properties of the PEs was studied. The solid polymer electrolytes (SPE) membranes were analyzed by differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), X-ray diffraction (XRD), scanning electron microscopy (SEM), energy dispersive X-ray (EDX), polarized optical microscopy (POM), atomic force microscopy (AFM), complex impedance spectroscopy (ionic conductivity) and cyclic voltammetry (CV). The obtained results evidenced an influence of the alkyl chain length of the IL anion on the temperature of degradation, birefringence, surface roughness and ionic conductivity of the membranes. The DSC, XRD and CV results showed independency from the length of the IL-anion-alkyl chain. The PEs displayed an predominantly amorphous morphology, a minimum temperature of degradation of 135 °C, a room temperature (T = 25 °C) ionic conductivity of 7.78 × 10−4 S cm−1 and a wide electrochemical window of ∼ 4.0 V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Biopolymer-based materials have been of particular interest and they are alternatives to synthetic polymers based on the decreasing oil resources. The polymer electrolytes were doped with choline-based IL N,N,Ntrimethyl- N-(2-hydroxyethyl)ammonium bis(trifluoromethylsulfonyl)imide ([N1 1 1 2(OH)][NTf2]), or Er (CF3SO3)3 or both. The polymer electrolytes were employed in the production of glass/ITO/WO3/electrolyte/ CeO2–TiO2/ITO/glass electrochromic devices (ECDs). The lowest onset temperature for the degradation of all the SPEs is at ~130 °C for the Gellan Er (CF3SO3)3 (10:1) this temperature range of stability is wide enough for a material to be applied as an electrolyte/separator component in electrochemical devices. The three ECDs displayed fast switching speed (ca. 15 s). Gellan [N1 1 1 2(OH)][NTf2] Er (CF3SO3)3 (5:1:10) exhibited an electrochromic contrast of 4.2% in the visible region, the coloration efficiency attained at 555 nm was 3.5 and 0.90 cm-2 C-1 in the “colored” and “bleached” states, respectively, and the open circuit memorywas 48 h. Preliminary tests performed with a prototype electrochromic device (ECD) incorporating WO3 as cathodic electrochromic layer, are extremely encouraging.