7 resultados para MATERIALS SCIENCE, CHARACTERIZATION
em Universidade do Minho
Resumo:
Tese de Doutoramento Cincia e Engenharia de Polmeros e Compsitos.
Resumo:
In this paper, we present a new course entitled Biomimicry: from life to nanotechnological innovations at the Mines Nancy Engineering School, Nancy, France, and explain how we developed a specific curriculum covering biomimicry. We discuss strategies that can be followed by teachers to explain selected contents in the multi-disciplinary field of biomimicry and/or bioinspiration to undergraduate students and how practical classroom activities can be conducted as individual or team work. We hope that sharing our experience will help teachers and senior researchers disseminate useful concepts and real examples of biomimetic principles and tools for the development of new materials, new/improved design and fabrication strategies, and innovation methodologies.
Resumo:
Microinjection molding of polymer composites with carbon nanotubes (CNT) requires previous production of the nanocomposites, often by melt extrusion. Each processing step has a thermo-mechanical effect on the polymer melt, conveying different properties to the final product. In this work, polyamide 6 and its composites with pristine and functionalized CNT (f-CNT) were processed by a mini twin-screw extrusion, followed by microinjection molding. The morphology induced on the polymer by each process was analyzed by differential scanning calorimetry and wide angle X-ray diffraction. Calorimetric analysis showed a secondary crystallization for the microinjected materials, absent for the extruded materials. The characterization of microinjected polyamide 6 by X-ray diffraction revealed a large contribution of the c phase to the total crystallinity, mainly in the skin region, while the nanocomposites and extruded materials were characterized by a larger contribution of the a phase. Functionalization of CNT did not affect significantly the polymer morphology compared to composites with pristine CNT.
Resumo:
Polymer based wicking structures were fabricated by sintering powders of polycarbonate (PC), ultra-high molecular weight polyethylene and polyamide 12, aiming at selecting a suitable material for an innovative electroencephalography (EEG) bio-electrode. Preliminary experiments showed that PC based wicks displayed the best mechanical properties, therefore more detailed studies were carried out with PC to evaluate the influence of powder granulometry and processing parameters (pressure, temperature and time) on the mechanical properties, porosity, mean pore radius and permeability of the wicks. It was concluded that the mechanical properties are significantly enhanced by increasing the processing time and pressure, although at the expense of a significant decrease of porosity and mean pore diameter (and thus permeability), particularly for the highest applied pressures (74kPa). However, a good compromise between porosity/permeability and mechanical properties could be obtained by sintering PC powders of particle sizes below 500m at 165C for 5min, upon an applied pressure of 56kPa. Moreover, PC proved to be chemically stable in contact with an EEG common used disinfectant. Thus, wicking structures with appropriate properties for the fabrication of reusable bio-electrodes could be fabricated from the sintering of PC powders.
Resumo:
Polyimide co-polymers have been prepared based on different diamines as co-monomers: a diamine without CN groups and a novel synthesized diamine with two CN groups prepared by polycondensation reaction followed by thermal cyclodehydration. Dielectric spectroscopy measurements were performed and the dielectric complex function, ac conductivity and electric modulus of the co-polymers were investigated as a function of CN group content in the frequency range from 0.1 Hz to 107 Hz at temperatures from 25 to 260 C. For all samples and temperatures above 150C, the dielectric constant increases with increasing temperature due to increaseing conductivity. The -relaxation is just detected for the sample without CN groups, being this relaxation overlapped by the electrical conductivity contributions in the remaining samples. For the copolymer samples and the polymer with CN groups an important Maxwell-Wagner-Sillars contribution is detected. The mechanisms responsible for the dielectric relaxation, conduction process and electric modulus response have been discussed as a function of the CN groups content present in the samples.
Resumo:
This paper presents a systematic study for the production of poly(vinylidene fluoride-hexafluoropropylene), P(VDF-HFP), porous films using solvent evaporation (SE) and non-solvent induced phase separation (NIPS) techniques. Parameters such as volume fraction of the copolymer solution, film thickness, time exposure to air, non-solvent and temperature of the coagulation bath were investigated on the morphology, crystallization and mechanical properties of the samples. Films with different porous morphologies including homogeneous pore sizes, macrovoids and spherulites were obtained depending on the processing conditions, which in turn affect the wettability and mechanical properties of the material. Knowing that the phase content of the films also depends on the processing conditions, this paper shows that P(VDF-HFP) films with tailored porous morphology, electroactive phase content, hydrophobicity, cristallinity and mechanical properties can be achieved for a specific application using the adequate SE and NIPS techniques conditions.
Resumo:
Polymer based scintillator composites have been produced by combining polystyrene (PS) and Gd2O3:Eu3+ scintillator nanoparticles. Polystyrene has been used since it is a flexible and stable binder matrix, resistant to thermal and light deterioration and with suitable optical properties. Gd2O3:Eu3+ has been selected as scintillator material due to its wide band gap, high density and visible light yield. The optical, thermal and electrical characteristics of the composites were studied as a function of filler content, together with their performance as scintillator material. Additionally 1wt.% of 2,5 dipheniloxazol (PPO) and 0.01wt.% of (1,4-bis(2-(5-phenioxazolil))-benzol (POPOP) were introduced in the polymer matrix in order to strongly improve light yield, i.e. the measured intensity of the output visible radiation, under X-ray irradiation. Whereas increasing scintillator filler concentration (from 0.25wt.% to 7.5wt.%) increases scintillator light yield, decreases the optical transparency of the composite. The addition of PPO and POPOP, strongly increased the overall 2 transduction performance of the composite due to specific absorption and re-emission processes. It is thus shown that Gd2O3:Eu3+/PPO/POPOP/PS composites in 0.25 wt.% of scintillator content with fluorescence molecules is suitable for the development of innovate large area X-ray radiation detectors with huge demand from the industries.