4 resultados para Layered and staggered structure
em Universidade do Minho
Resumo:
Thermoplastic elastomers based on a triblock copolymer styrene-butadiene-styrene (SBS) with different butadiene/styrene ratios, block structure and carbon nanotube (CNT) content were submitted to accelerated weathering in a Xenontest set up, in order to evaluate their stability to UV ageing. It was concluded that ageing mainly depends on butadiene/styrene ratio and block structure, with radial block structures exhibiting a faster ageing than linear block structures. Moreover, the presence of carbon nanotubes in the SBS copolymer slows down the ageing of the copolymer. The evaluation of the influence of ageing on the mechanical and electrical properties demonstrates that the mechanical degradation is higher for the C401 sample, which is the SBS sample with the largest butadiene content and a radial block structure. On the other hand, a copolymer derivate from SBS, the styrene-ethylene/butadiene-styrene (SEBS) sample, retains a maximum deformation of ~1000% after 80 h of accelerated ageing. The hydrophobicity of the samples decreases with increasing ageing time, the effect being larger for the samples with higher butadiene content. It is also verified that cytotoxicity increases with increasing UV ageing with the exception of SEBS, which remains not cytotoxic up to 80 h of accelerated ageing time, demonstrating its potential for applications involving exposition to environmental conditions.
Resumo:
PhD thesis in Educational Sciences (specialization in Politics of Education).
Resumo:
Tri-layered and bi-layered magnetoelectric (ME) flexible composite structures of varying geometries and sizes consisting on magnetostrictive Vitrovac and piezoelectric poly(vinylidene fluoride) (PVDF) layers were fabricated by direct bonding. From the ME measurements it was determined that tri-layered composites structures (magnetostrictive-piezoelectric-magnetostrictive type), show a higher ME response (75 V.cm-1.Oe-1) than the bi-layer structure (66 V.cm 1.Oe-1). The ME voltage coefficient decreased with increasing longitudinal size aspect ratio between PVDF and Vitrovac layers (from 1.1 to 4.3), being observed a maximum ME voltage coefficient of 66 V.cm-1.Oe-1. It was also observed that the composite with the lowest transversal aspect ratio between PVDF and Vitrovac layers resulted in better ME performance than the structures with higher transversal size aspect ratios. It was further determined an intimate relation between the Vitrovac PVDF Area Area ratio and the ME response of the composites. When such ratio values approach 1, the ME response is the largest. Additionally the ME output value and magnetic field response was controlled by changing the number of Vitrovac layers, which allows the development of magnetic sensors and energy harvesting devices.
Resumo:
Ideal candidates for the repair of robust biological tissues should exhibit diverse features such as biocompatibility, strength, toughness, self-healing ability and a well-defined structure. Among the available biomaterials, hydrogels, as highly hydrated 3D-crosslinked polymeric networks, are promising for Tissue Engineering purposes as result of their high resemblance with native extracellular matrix. However, these polymeric structures often exhibit a poor mechanical behavior, hampering their use in load-bearing applications. During the last years, several efforts have been made to create new strategies and concepts to fabricate strong and tough hydrogels. Although it is already possible to shape the mechanical properties of artificial hydrogels to mimic biotissues, critical issues regarding, for instance, their biocompatibility and hierarchical structure are often neglected. Therefore, this review covers the structural and mechanical characteristics of the developed methodologies to toughen hydrogels, highlighting some pioneering efforts employed to combine the aforementioned properties in natural-based hydrogels.