43 resultados para replacement of corn
em Indian Institute of Science - Bangalore - Índia
Resumo:
With an objective to replace a water droplet from a steel surface by oil we study here the impact of injecting a hydrophilic/lipophilic surfactant into the droplet or into the surrounding oil reservoir. Contact angle goniometery, Grazing angle FTIR spectroscopy and Atomic force microscopy are used to record the oil/water interfacial tension, surface energetics of the substrate under the oil and water phases as well as the corresponding physical states of the substrates. Such energetics reflect the rate at which the excess surfactant molecules accumulate at the water/oil interface and desorb into the phases. The molecules diffuse into the substrate from the phases and build up specific molecular configurations which, with the interfacial tension, control the non-equilibrium progress of and the equilibrium status of the contact line. The study shows that the most efficient replacement of water by the surrounding oil happens when a surfactant is sparingly soluble in the supplier oil phase and highly soluble in the recipient water phase.
Resumo:
The structural stabilizing property of 2,2,2-trifluoroethanol (TFE) in peptides has been widely demonstrated, More recently, TFE has been shown to enhance secondary structure content in globular proteins, and to influence quaternary interactions in protein multimers. The molecular mechanisms by which TFE exerts its Influence on peptide and protein structures remain poorly understood. The present analysis integrates the known physical properties of TFE with a variety of experimental observations on the interaction of TFE with peptides and proteins and on the properties of fluorocarbons. Two features of TFE, namely the hydrophobicity of the trifluoromethyl group and the hydrogen bonding character (strong donor and poor acceptor), emerge as the most important factors for rationalising the observed effects of TFE. A model is proposed for TFE interaction with peptides which involves an initial replacement of the hydration shell by fluoroalcohol molecules, a process driven by apolar interactions and favourable entropy of dehydration. Subsequent bifurcated hydrogen-bond formation with peptide carbonyl groups, which leave intramolecular interactions unaffected, promotes secondary structure formation.
Resumo:
In this paper, inhibition of the glutathione peroxidase activity of two synthetic organoselenium compounds, bis[2-(N,N-dimethylamino)benzyl]diselenide (5) and bis[2-(N,N-dimethylamino)benzyl]selenide (9), by gold(I) thioglucose (1), chloro(triethylphosphine)gold(I), chloro(trimethylphosphine)gold(I), and chloro(triphenylphosphine)gold(I) is described. The inhibition is found to be competitive with respect to a peroxide (H2O2) substrate and noncompetitive with respect to a thiol (PhSH) cosubstrate. The diselenide 5 reacts with PhSH to produce the corresponding selenol (6), which upon treatment with 1 equiv of gold(I) chlorides produces the corresponding gold selenolate complexes 11−13. However, the addition of 1 equiv of selenol 6 to complexes 11−13 leads to the formation of bis-selenolate complex 14 by ligand displacement reactions involving the elimination of phosphine ligands. The phosphine ligands eliminated from these reactions are further converted to the corresponding phosphine oxides (R3PO) and selenides (R3PSe). In addition to the replacement of the phosphine ligand by selenol 6, an interchange between two different phosphine ligands is also observed. For example, the reaction of complex 11 having a trimethylphosphine ligand with triphenylphosphine produces complex 13 by phosphine interchange reactions via the formation of intermediates 15 and 16. The reactivity of selenol 6 toward gold(I) phosphines is found to be similar to that of selenocysteine.
Resumo:
Assembly intermediates of icosahedral viruses are usually transient and are difficult to identify. In the present investigation, site-specific and deletion mutants of the coat protein gene of physalis mottle tymovirus (PhMV) were used to delineate the role of specific amino acid residues in the assembly of the virus and to identify intermediates in this process. N-terminal 30, 34, 35 and 39 amino acid deletion and single C-terminal (N188) deletion mutant proteins of PhMV were expressed in Escherichia coli. Site-specific mutants H69A, C75A, W96A, D144N, D144N-T151A, K143E and N188A were also constructed and expressed. The mutant protein lacking 30 amino acid residues from the N terminus self-assembled to T = 3 particles in vivo while deletions of 34, 35 and 39 amino acid residues resulted in the mutant proteins that were insoluble. Interestingly, the coat protein (pR PhCP) expressed using pRSET B vector with an additional 41 amino acid residues at the N terminus also assembled into T = 3 particles that were more compact and had a smaller diameter. These results demonstrate that the amino-terminal segment is flexible and either the deletion or addition of amino acid residues at the N terminus does not affect T = 3 capsid assembly, in contrast, the deletion of even a single residue from the C terminus (PhN188 Delta 1) resulted in capsids that were unstable. These capsids disassembled to a discrete intermediate with a sedimentation coefficent of 19.4 S. However, the replacement of C-terminal asparagine 188 by alanine led to the formation of stable capsids. The C75A and D144N mutant proteins also assembled into capsids that were as stable as the pR PhCP, suggesting that C75A and D144 are not crucial for the T = 3 capsid assembly. pR PhW96A and pR PhD144N-T151A mutant proteins failed to form capsids and were present as heterogeneous aggregates. Interestingly, the pR PhK143E mutant protein behaved in a manner similar to the C-terminal deletion protein in forming unstable capsids. The intermediate with an s value of 19.4 S was the major assembly product of pR PhH69A mutant protein and could correspond to a 30mer. It is possible that the assembly or disassembly is arrested at a similar stage in pR PhN188 Delta 1, pR PhH69A and pR PhK143E mutant proteins.
Resumo:
We demonstrate the aptitude of supramolecular hydrogel formation using simple bile acid such as lithocholic acid in aqueous solution in the presence of various dimeric or oligomeric amines. By variation of the choice of the amines in such mixtures the gelation properties could be modulated. However, the replacement of lithocholic acid (LCA) by cholic acid or deoxycholic acid resulted in no hydrogel formation. FT-IR studies confirm that the carboxylate and ammonium residues of the two components are involved in the salt (ion-pair) formation. This promotes further assembly of the components reinforced by a continuous hydrogen bonded network leading to gelation. Electron microscopy shows the morphology of the internal organization of gels of two component systems which also depends significantly on the amine part. Variation of the amine component from the simple 1,2-ethanediamine (EDA) to oligomeric amines in such gels of lithocholic acid changes the morphology of the assembly from long one-dimensional nanotubes to three-dimensional complex structures. Single crystal X-ray diffraction analysis with one of the amine-LCA complexes suggested the motif of fiber formation where the amines interact with the carboxylate and hydroxyl moieties through electrostatic forces and hydrogen bonding. From small angle neutron scattering study, it becomes clear that the weak gel from LCA-EDA shows scattering oscillation due to the presence of non-interacting nanotubules while for gels of LCA with oligomeric amines the individual fibers come together to form complex three-dimensional organizations of higher length scale. The rheological properties of this class of two component system provide clear evidence that the flow behavior can be modulated varying the acid-amine ratio.
Resumo:
In the present investigation, the wear behaviour of a creep-resistant AE42 magnesium alloy and its composites reinforced with Saffil short fibres and SiC particles in various combinations is examined in the longitudinal direction i.e., the plane containing random fibre orientation is perpendicular to the steel counter-face. Wear tests are conducted on a pin-on-disc set-up under dry sliding condition having a constant sliding velocity of 0.837 m/s for a constant sliding distance of 2.5 km in the load range of 10-40 N. It is observed that the wear rate increases with increase in load for the alloy and the composites, as expected. Wear rate of the composites is lower than the alloy and the hybrid composites exhibit a lower wear rate than the Saffil short fibres reinforced composite at all the loads. Therefore, the partial replacement of Saffil short fibres by an equal volume fraction of SiC particles not only reduces the cost but also improves the wear resistance of the composite. Microstructural investigation of the surface and subsurface of the worn pin and wear debris is carried out to explain the observed results and to understand the wear mechanisms. It is concluded that the presence of SiC particles in the hybrid composites improves the wear resistance because these particles remain intact and retain their load bearing capacity even at the highest load employed, they promote the formation of iron-rich transfer layer and they also delay the fracture of Saffil short fibres to higher loads. Under the experimental conditions used in the present investigation, the dominant wear mechanism is found to be abrasion for the AE42 alloy and its composites. It is accompanied by severe plastic deformation of surface layers in case of alloy and by the fracture of Saffil short fibres as well as the formation of iron-rich transfer layer in case of composites.
Resumo:
In this paper materials like rice husk ash, burnt clay and red mud are examined for their pozzolanic properties. Rice husk ash, obtained from various sources, is analysed by X-ray diffraction. Compressive strength properties of lime-pozzolana mortars with rice husk ash, burnt clay and red mud as pozzolana are studied. Influence of grinding of rice husk ash and intergrinding with lime are also investigated. Combination pozzolana with partial replacement of burnt clay and red mud by rice husk ash are examined for their pozzolanic properties. Long term strength behaviour of lime-pozzolana mortars is investigated to understand the durability of lime-pozzolana cements.
Resumo:
XPS studies show that the presence of chemisorbed chlorine stabilizes and also enhances molecular dioxygen species on Ag surfaces dosed with either K or Ba. The surface atomic oxygen is found to become depleted on chlorination. The variation in the nature of surface species with respect to temperature shows chlorine-induced diffusion of atomic oxygen into the subsurface region at 300 K. For coverages of potassium up to 8 × 1014 atoms/cm2, preferential chloridation of Ag occurs while at higher potassium coverages, KCl formation is distinctly observed on the surface. In the case of barium, two types of adsorbed chlorine species, Cl(α) and Cl(β), associated with Ag and Ba, respectively, are clearly seen even at low barium coverages. This is believed to be due to the higher valence occupation of barium compared to potassium. The Cl(α) species associated with Ag is found to occupy a preferred site on both K- and Ba-dosed surfaces, involving chemisorptive replacement of O(α) to the subsurface region.
Resumo:
Empirical potential energy calculations have been carried out to determine the preferred conformations of penicillins and penicillin sulphones and their 1-oxa-1-dethia and 1-carba-1-dethia analogues. With the exception of 1-oxa-1-dethia penicillins, all the other compounds favour C2 and the C3 puckered conformations of their five-membered rings. Replacement of C2 methyl groups by hydrogen atoms as in bisnorpenicillin V or oxidation of sulphur in position 1 as in sulphones, makes the C3 puckered form much less favourable. Addition of an amino-acyl group at the C6 atom, however, makes the C3 puckered form more favoured in penicillin G or V and in 1-carba-1-dethia penicillins. Through the replacement of the sulphur atom at position 1 by an oxygen atom or by a -CH2 group increases the non-planarity of the lactam peptide bond, it significantly affects the relative disposition of the C3 carboxyl group with respect to the β-lactam ring. These conformational differences have been correlated with the biological activities of these compounds. The present study suggests that the conformation of the bicyclic ring system may be more important for initial binding with the crosslinking enzyme(s) involved in the biosynthesis of bacterial cell-wall peptidoglycan and that the mode of binding is influenced by the nature of the side-group at the C6 atom. These studies predict, in agreement with experimental results, that the 1-oxa-1-dethia penicillin nulceus is an inhibitor of penicillianses. The study also suggests that the stereospecificities of the crosslinking enzyme(s) and penicillinases are very similar with regard to the nature of the side-group at the 6 atom and the confirmation of the bicyclic ring system. However, the confirmational requirement for the bicyclic ring system appears to be more specific in the former enzyme than in the latter.
Resumo:
The addition of guanosine 5-monophosphate (5′-GMP) to an aqueous solution of Mn2+ ions results in a decrease in ESR signal intensity and an increase in line-width of Mn2+ ions. This can be interpreted in terms of stepwise formation of outersphere and inner-sphere complexes as When Mg2+ is added to a mixture of Mn2+ and 5′-GMP, ESR signal intensity increases, presumably due to the replacement of Mn2+ by Mg2+ in the complex. From the variation of ESR signal intensity as a function of concentration of Mg2+, the product K1K2 for the magnesium complex i s calculated as 125 M−1. This difference in stability constants may indicate that both phosphate group and guanine base are involved in the formation of Mn2+-5′-GMP complex.
Resumo:
The paper deals with a rational approach to the development of general design criteria for non-dissipative vibration isolation systems. The study covers straight-through springmass systems as well as branched ones with dynamic absorbers. Various design options, such as the addition of another spring-mass pair, replacement of an existing system by one with more spring-mass pairs for the same space and material requirements, provision of one or more dynamic absorbers for the desired frequency range, etc., are investigated quantitatively by means of an algebraic algorithm which enables one to write down straightaway the velocity ratio and hence transmissibility of a linear dynamical system in terms of the constituent parameters.
Resumo:
In this study, a series of seeondary- and tertiary-amino-substituted diaryl diselenides were synthesized and studied for their glutathione peroxidase (GPx) like antioxidant activities with H2O2, cumene hydroperoxide, or tBuOOH as substrates and with PhSH or glutathione (GSH) as thiol cosubstrates. This study reveals that replacement of the tert-amino groups in benzylamine-based diselenides by sec-amino moieties drastically enhances the catalytic activities in both the aromatic thiol (PhSH) and GSH assay systems. Particularly, the N-propyl- and N-isopropylamino-substituted diselenides are 8-18 times more active than the corresponding N,N-dipropyl- and N,N-diisopropylamine-based compounds in all three peroxide systems when GSH is used as the thiol cosubstrate. Although the catalytic mechanism of sec-amino-substituted disclenides is similar to that of the tert-amine-based compounds, differences in the stability and reactivity of some of the key intermediates account for the differences in the GPx-like activities. it is observed that the sec-amino groups are better than the tert-amino moieties for generating the catalytically active selenols. This is due to the absence of any significant thiol-exchange reactions in the selenenyl sulfides derived from sec-amine-based diselenides. Furthermore, the seleninic acids (RSeO2H) derived from the sec-amine-based compounds are more stable toward further reactions with peroxides than their tert-amine-based analogues.
Resumo:
The pseudoproline residue (Psi Pro, L-2,2-dimethyl-1,3-thiazolidine-4-carboxylic acid) has been introduced into heterochiral diproline segments that have been previously shown to facilitate the formation of beta-hairpins, containing central two and three residue turns. NMR studies of the octapeptide Boc-Leu-Phe-Val-(D)Pro-Psi Pro-Leu-Phe-Val-OMe (1), Boc-Leu-Val-Val-(D)Pro-Psi Pro-Leu-Val-Val-OMe (2), and the nonapeptide sequence Boc-Leu-Phe-Val-(D)Pro-Psi Pro-(D)Ala-Leu-Phe-Val-OMe (3) established well-registered beta-hairpin structures in chloroform solution, with the almost exclusive population of the trans conformation for the peptide bond preceding the Psi Pro residue. The beta-hairpin conformation of 1 is confirmed by single crystal X-ray diffraction. Truncation of the strand length in Boc-Val-(D)Pro-Psi Pro-Leu-OMe (4) results in air increase in the population of the cis conformer, with a cis/trans ratio of 3.65. Replacement of Psi Pro in 4 by (L)Pro in 5, results in almost exclusive population of the trans form, resulting in an incipient beta-hairpin conformation, stabilized by two intramolecular hydrogen bonds. Further truncation of the sequence gives an appreciable rise in the population of cis conformers in the tripeptide piv-(D)Pro-Psi Pro-Leu-OMe (6). In the homochiral segment Piv-Pro Psi Pro-Leu-OMe (7) only the cis form is observed with the NMR evidence strongly supporting a type VIa beta-turn conformation, stabilized by a 4 -> 1 hydrogen bond between the Piv (CO) and Leu (3) NH groups. The crystal structure of the analog peptide 7a (Piv-Pro-Psi(H,CH3)Pro-Leu-NHMe) confirms the cis peptide bond geometry for the Pro-Psi(H,CH3)pro peptide bond, resulting in a type VIa beta-turn conformation.
Resumo:
Wear of dies is a serious problem in the forging industry. The materials used for the dies are generally expensive steel alloys and the dies require costly heat treatment and surface finishing operations. Degeneration of the die profile implies rejection of forged components and necessitates resinking or replacement of the die. Measures which reduce wear of the die can therefore aid in the reduction of production costs. The work reported here is the first phase of a study of the causes of die wear in forging production where the batch size is small and the machine employed is a light hammer. This is a problem characteristic of the medium and small scale area of the forging industry where the cost of dies is a significant proportion of the total capital investment. For the same energy input and under unlubricated conditions, die wear has been found to be sensitive to forging temperature; in cold forging the yield strength of the die material is the prime factor governing the degeneration of the die profile, whilst in hot forging the wear resistance of the die material is the main factor which determines the rate of die wear. At an intermediate temperature, such as that characteristic of warm forging, the die wear is found to be less than that in both cold and hot forging. This preliminary study therefore points to the fact that the forging temperature must be taken into account in the selection of die material. Further, the forging industry must take serious note of the warm forging process, as it not only provides good surface finish, as claimed by many authors, but also has an inherent tendency to minimize die wear.