21 resultados para immersion

em Indian Institute of Science - Bangalore - Índia


Relevância:

20.00% 20.00%

Publicador:

Resumo:

India possesses a diverse and rich cultural heritage and is renowned as a 'land of festivals'. These festivals attract massive community involvement paving way to new materials such as 'Plaster of Paris' being used for 'modernizing' the representation of idols with very little thought given to the issues of toxicity and environmental impacts. Another dimension to the whole issue is the plight of the artisans and the workers involved in the trade. Owing to the unorganized nature of the industry there is minimal or no guidelines pertaining-to the worker safety and health risks of the people involved. This paper attempts to address the complexities of the inherent hazards as a consequence of these socio-environmental issues and trace the scientific rationale in addressing them in a practical and pragmatic way.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conventional methods for determining the refractive index demand specimens of optical quality, the preparation of which is often very difficult. An indirect determination by matching the refractive indices of specimen and immersion liquid is a practical alternative for photoelastic specimen of nonoptical quality. An experimental arrangement used for this technique and observations made while matching the refractive indices of three different specimens are presented.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Positive nitrogenase activities ranging from 0.18 to 0.78 nmol of C2H4 cm−2 h−1 were detected on the leaf surfaces of different varieties of cotton (Gossypium hirsutum L. and G. herbaceum L.) plants. Beijerinckia sp. was observed to be the predominant nitrogen-fixing microorganism in the phyllosphere of these varieties. A higher level of phyllosphere nitrogen-fixing activity was recorded in the variety Varalaxmi despite a low C/N ratio in the leaf leachates. Leaf surfaces of the above variety possessed the largest number of hairy outgrowths (trichomes) which entrapped a majority of microbes. Immersion of plant roots in nutrient medium containing 32Pi led to the accumulation of label in the trichome-borne microorganisms, thereby indicating a possible transfer of nutrients from leaf to microbes via trichomes. Extrapolation of acetylene reduction values suggested that 1.6 to 3.2 kg of N ha−1 might be contributed by diazotrophs in the phyllosphere of the variety Varalaxmi during the entire growth period.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Drop formation at the conical tips of melting rods has been experimentally studied using the transparent wax-alcohol/acetonitrile system. The effects of cone angle, rod diameter, immersion depth, and bath temperature on the detached drop mass have been studied over a wide range, besides recording useful qualitative information based on visual observation. The experimental results suggest that the phenomenon of drop formation at the tip of melting rods has a close parallel with the drop formation at conical tips, at least on a qualitative basis. However, the results could not be quantified owing to difficulties in characterizing the physical properties of the system, despite efforts to minimize them.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this paper, we present results on water flow past randomly textured hydrophobic surfaces with relatively large surface features of the order of 50 µm. Direct shear stress measurements are made on these surfaces in a channel configuration. The measurements indicate that the flow rates required to maintain a shear stress value vary substantially with water immersion time. At small times after filling the channel with water, the flow rates are up to 30% higher compared with the reference hydrophilic surface. With time, the flow rate gradually decreases and in a few hours reaches a value that is nearly the same as the hydrophilic case. Calculations of the effective slip lengths indicate that it varies from about 50 µm at small times to nearly zero or “no slip” after a few hours. Large effective slip lengths on such hydrophobic surfaces are known to be caused by trapped air pockets in the crevices of the surface. In order to understand the time dependent effective slip length, direct visualization of trapped air pockets is made in stationary water using the principle of total internal reflection of light at the water-air interface of the air pockets. These visualizations indicate that the number of bright spots corresponding to the air pockets decreases with time. This type of gradual disappearance of the trapped air pockets is possibly the reason for the decrease in effective slip length with time in the flow experiments. From the practical point of usage of such surfaces to reduce pressure drop, say, in microchannels, this time scale of the order of 1 h for the reduction in slip length would be very crucial. It would ultimately decide the time over which the surface can usefully provide pressure drop reductions. ©2009 American Institute of Physics

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A rough hydrophobic surface when immersed in water can result in a ``Cassie'' state of wetting in which the water is in contact with both the solid surface and the entrapped air. The sustainability of the entrapped air on such surfaces is important for underwater applications such as reduction of flow resistance in microchannels and drag reduction of submerged bodies such as hydrofoils. We utilize an optical technique based oil total internal reflection of light at the water-air interface to quantify the spatial distribution of trapped air oil such a surface and its variation with immersion time. With this technique, we evaluate the sustainability of the Cassie state on hydrophobic surfaces with four different kinds of textures. The textures studied are regular arrays of pillars, ridges, and holes that were created in silicon by a wet etching technique, and also a texture of random craters that was obtained through electrodischarge machining of aluminum. These surfaces were rendered hydrophobic with a self-assembled layer Of fluorooctyl trichlorosilane. Depending on the texture, the size and shape of the trapped air pockets were found to vary. However, irrespective of the texture, both the size and the number of air pockets were found to decrease with time gradually and eventually disappear, suggesting that the sustainability of the ``Cassie'' state is finite for all the microstructures Studied. This is possibly due to diffusion of air from the trapped air pockets into the water. The time scale for disappearance of air pockets was found to depend on the kind of microstructure and the hydrostatic pressure at the water-air interface. For the surface with a regular array of pillars, the air pockets were found to be in the form of a thin layer perched on top of the pillars with a large lateral extent compared to the spacing between pillars. For other surfaces studied, the air pockets are smaller and are of the same order as the characteristic length scale of the texture. Measurements for the surface with holes indicate that the time for air-pocket disappearance reduces as the hydrostatic pressure is increased.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The time evolution of the film thickness and domain formation of octadecylamine molecules adsorbed oil a mica surface is investigated Using atomic force microscopy. The adsorbed Film thickness is determined by measuring the height profile across the mica-amine interface of a mica surface partially immersed in a 15 mM solution of octadecylamine in chloroform. Using this novel procedure, adsorption of amine on mica is found to occur in three distinct stages, with morphologically distinct domain Formation and growth occurring during each stage. In the first stage, where adsorption is primarily in the thin-film regime, all average Film thickness of 0.2 (+/- 0.3) nm is formed for exposure times below 30 s and 0.8 (+/- 0.2) nm for 60 s of immersion time. During this stage, large sample spanning domains are observed. The second stage, which occurs between 60-300 s, is associated with it regime of rapid film growth, and the film thickness increases from about 0.8 to 25 nm during this stage. Once the thick-film regime is established, further exposure to the amine solution results in all increase in the domain area, and it regime of lateral domain growth is observed. In this stage, the domain area coverage grows from 38 to 75%, and the FTIR spectra reveal an increased level of crystallinity in the film. Using it diffusion-controlled model and it two-step Langmuir isotherm, the time evolution of the film growth is quantitatively captured. The model predicts the time at which the thin to thick film transition occurs as well its the time required for complete film growth at longer times. The Ward-Tordai equation is also solved to determine the model parameters in the monolayer (thin-film) regime, which occurs during the initial stages of film growth.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Seawater aging response was investigated in marine-grade glass/epoxy, glass/vinyl ester, carbon/epoxy and carbon/vinyl ester composites with respect to water uptake, interlaminar shear strength, flexural strength, tensile strength, and tensile fracture surface observations. The reduction of mechanical properties was found to be higher in them initial stages which showed saturation in the longer durations of seawater immersion. The flexural strength and ultimate tensile strength (UTS) dropped by about 35% and 27% for glass/epoxy, 22% and 15% for glass/vinyl ester, 48% and 34% for carbon/epoxy 28%, and 21% carbon/vinyl ester composites respectively. The water uptake behavior of epoxy-based composites was inferior to that of the vinyl system.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Moisture absorption characteristics and its effects on the mechanical properties and failure process of polymers (neat epoxy and polyester resins) and composites with simple (glass, carbon and kevlar) and hybrid (glass-carbon, carbon-kevlar and kevlar-glass) fibres were experimentally determined before and after immersion in water at 343 K for 20 days. The maximum moisture content (Mm) and diffusion coefficient (Dx) of these composites were determined. The degradation in ultimate tensile strength and Young's modulus due to the moisture content were experimentally determined and found to be quite significant. Acoustic emissions, from specimens before and after exposure, were monitored during the load cycle, and revealed a significant change in the failure process of these composites. Scanning Electron Microscope (SEM) studies on failed exposed and unexposed specimens revealed resin leach out and fibre prominence.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The fluid-flow pattern and residence-time distribution (r.t.d.) of the fluid in a continuous casting mould have been studied using a water model. The two recirculating zones below the discharge ports have been found to be asymmetric. The effect of casting speed, discharge port diameter, shroud well depth and the immersion depth on r.t.d. have been investigated. The r.t.d. curve has been well represented by a model of two backmix cells of equal volume in series. The exist of the fluid has been found to be non-uniform across the cross-section of the mould. The fluid-flow pattern has been observed to change with time in a random fashion. Dead volume of upto 31.8% has been found with smaller discharge ports.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The surfactant-assisted seed-mediated growth method was used for the formation of gold nanorods (GNRs) directly on gold (Au) and indium tin oxide (ITO) surfaces. Citrate-stabilized similar to 2.6 nm spherical gold nanoparticles (AuNPs) were first self-assembled on ITO or Au surfaces modified with (3-mercaptopropyl)-trimethoxysilane (MPTS) sol-gel film and then immersed in a cationic surfactant growth solution to form GNRs. The growth of GNRs on the MPTS sol gel film modified ITO surface was monitored by UV-visible spectroscopy. The ITO surface with the attached spherical AuNPs shows a surface plasmon resonance band at 550 nm. The intensity of this absorption band increases while increasing the immersion time of the AuNP-modified ITO surface into the growth solution, and after 5 h, an additional shoulder band around 680 nm was observed. The intensity of this shoulder band increases, and it was shifted to longer wavelength as the immersion time of the AuNP-modified ITO surface into the growth solution increases. After 20 h, a predominant wave at 720 nm was observed along with a band at 550 nm. Further immersion of the modified ITO surface into the growth solution did not change the absorption characteristics. The bands observed at 550 and 720 nm were characteristics of GNRs, corresponding to transverse and longitudinal waves, respectively. The AFM images showed the presence of GNRs on the surface of the MPTS sol gel modified ITO surface with a typical length of similar to 100-120 nm and a width of similar to 20-22 nm in addition to a few spherical AuNPs, indicating that seeded spherical AuNPs were not completely involved in the GNRs' formation. Finally, the electrocatalytic activity of the surface-grown GNRs on the MPTS sol gel film modified Au electrode toward the oxidation of ascorbic acid (AA) was studied. Unlike a polycrystalline Au electrode, the surface-grown GNR-modified electrode shows two well-defined voltammetric peaks for AA at 0.01 and 0.35 V in alkaline, neutral, and acidic pHs. The cause for the observed two oxidation peaks for AA was due to the presence of both nanorods and spherical nanoparticles on the electrode surface. The presence of spherical AuNPs on the MPTS sol gel film oxidized AA at more positive potential, whereas the GNRs oxidized AA at less positive potential. The observed 340 mV less positive potential shift in the oxidation of AA suggested that GNRs are better electrocatalysts for the oxidation of AA than the spherical AuNPs.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The main objective of this investigation was to understand the strength development of clays below fusion or vitrification temperatures of 900°C. The other objective was to establish threshold temperatures to produce a satisfactory construction material from clayey sediments from the Western Beaufort Sea for shore protection of artificial islands with minimum expense of thermal energy. Studies were, therefore, conducted using kaolinite, bentonite, and a clayey sediment from the Beaufort Sea. Unconfined-compressive-strength tests were conducted on clay samples heat treated from 110 to 700°C. Furthermore, to understand the factors responsible for strength-development-thermogravimetric studies and pore-size analysis, using mercury porosimetry, were also conducted. A gradual increase in strength was obtained with an increase in firing temperature. However, substantial and permanent increase in strength occurred only after dehydroxylation of all the clays studied; Clay samples heated to temperatures above dehydroxylation became resistant to disintegration upon immersion in water. Results indicate that the clayey sediments from Western Beaufort Sea have to be heat treated to about 600°C to produce granular material for use as a fill or shore-protection material for artificial islands.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The present work is based on four static molds using nozzles of different port diameter, port angle, and immersion depth. It has been observed that the meniscus is wavy. The wave amplitude shows a parabolic variation with the nozzle exit velocity. The dimensionless amplitude is found to vary linearly with the Froude number. Vortex formation and bubble entrainment by the wave occurs at the meniscus beyond a critical flow rate, depending upon the nozzle configuration, immersion depth, and the mold aspect ratio.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Epoxy systems containing HTBN rubber material and reinforced with E-glass fibres, exposed to a fixed time duration in three separate media were subjected to compressive mode of deformation. The yield stress and fractographic features noted on the compression failed samples are reported in this work. The experiment reveals that the seawater exposed sample exhibits a drop in strength compared to dry (unexposed) sample. This kind of drop is maintained if the media is changed from seawater to distilled water. When HCl is included in seawater. the experiment shows a small rise in strength value. These changes have been attributed to various factors like medium ingress into samples assisting interface failure, the larger-sized Cl- influencing the extent of diffusion of medium into system and finally their participation in the deformation phenomena. The fractographic features reveal interface separations that show either scattered debris or a cleaner surface or display a whitish-coated matrix region depending on whether the tests are done on unexposed samples or on ones following the immersion in the media.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Absorption due to immersion in aqueous media consisting of either saline or seawater or due to exposure to water vapor conditions and the attendant effect on the compressive properties of syntactic foam reinforced with E-glass fibers in the form of chopped strands were studied. Whereas the compressive strength decreased in samples exposed to water vapor, the saline or seawater immersed samples showed increase when compared to the dry sample. The decrease in strength in the vapor-exposed case is ascribed to higher absorption of water and to debonding and damaged features for interfaces. The enhancement of strength values for the samples immersed in saltish media is traced to the larger size of the chloride ion and resultant changes in the stress state around the fiber-bearing regions. Recourse to an analysis of scanning electron microscopic pictures of the compression-failed samples is taken to explain the observed trends.