140 resultados para hydrothermal crystal growth

em Indian Institute of Science - Bangalore - Índia


Relevância:

100.00% 100.00%

Publicador:

Resumo:

We present a theoretical analysis of the dynamics of crystal growth from a supercooled melt. A molecular theory of crystal growth that pays proper attention to the structure at the liquid-solid interface is discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Single crystals of Sr14−xCaxCu24O41 (x=0 and 12) are grown by the travelling solvent floating zone technique using an image furnace. The grown crystals are characterized for their single crystallinity by the X-ray and Neutron Laue method. The magnetic susceptibility measurements in Sr14Cu24O41 show considerable anisotropy along the main crystallographic axes. Low-temperature specific heat measurement and DC susceptibility measurement in Ca-doped crystal showed antiferromagnetic ordering at 2.8 K at ambient pressure. High-pressure AC susceptibility measurement on Ca-doped crystal showed a sharp superconducting transition at 2 K under 40 kbars. Tc onset reached a maximum value of 9.9 K at 54 kbars. The bulk superconductivity of the sample is confirmed by the high-pressure AC calorimetry with Tc max=9.4 K and TN=5 K at 56 kbars.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Crystal growth, electrical and magnetic properties are reported for mixed valence manganite Pr1-xPbxMnO3 (x = 0.2, 0.23, and 0.3). The crystals with x = 0.2 and 0.23 are ferromagnetic and insulating, whereas that with x = 0.3 is ferromagnetic below 200 K and shows an insulator-metal transition at 235 K. This composition shows a magnetoresistance of 90% in a field of 5 T. In the paramagnetic region, the temperature dependence of magnetic susceptibility of the crystals follows a Curie-Weiss behavior. The thermal evolution of magnetization in the ferromagnetic phase varies as T-3/2, in accordance with Bloch's law. The spin-stiffness constant D obtained from the Bloch constant is found to increase linearly with x. The magnetization does not reach complete saturation upto a field of 5 T. A possible contribution of the Pr spins to the total magnetic moment is discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Single crystals of the metalorganic nonlinear optical material zinc tris (thiourea) sulfate (ZTS) were grown from aqueous solution. The morphology of the crystals was indexed. The grown crystals were characterized by recording the powder X-ray diffraction pattern and by identifying the diffracting planes. Spectrophotometric studies on ZTS reveal that it has good transparency for the Nd: YAG laser fundamental wavelength. Differential thermal analysis of ZTS indicates that the material does not sublime before melting but decomposes immediately after melting. The defect content of the crystals was estimated using etching and X-ray topography. The mechanical hardness anisotropy was evaluated in the (100) plane, which indicates the presence of soft directions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Optical quality single crystals of sodium D-isoascorbate monohydrate were grown by a slow cooling technique. The crystal possesses a bulky prismatic morphology. Thermal analyses indicate that the crystals are stable up to 125 degrees C. The optical transmission window ranges from 307 nm to 1450 nm. The principal refractive indices have been measured employing Brewster's angle method. The crystallographic and the principal dielectric axes coincide with each other such that a lies along Z, b along X and c along Y. The optic axis is oriented 58 degrees (at 532 nm) to the crystallographic a axis in the XZ plane and the crystal is negative biaxial. Type 1 and type 2 phase matching curves are generated and experimentally verified. No polarization dependence of the light absorption was observed confirming the validity of Kleinman's symmetry conjecture, leading to a single nonvanishing nonlinear tensor component. According to Hobden's classification the crystal belongs to class 3. The crystal also exhibits second order noncollinear conic sections. The single shot and multiple shot surface laser damage thresholds are determined to be 32.7 GW cm(-2) and 6.5 GW cm(-2) respectively for 1064 nm radiation.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polycrystals of orthorhobic carbonates RCO3 (R = Sr, Ba and Pb) were synthesised for the first time using formic acid as mineraliser. The unit cell parameters of this synthetic pure carbonates are: BaCO3:a=5.309, B=8.889, C=6.401; srCO3:a=5.108, B=8.420, C=6.040; PbCO3: A=5.176, B=8.511, C=6.137.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Phase diagrams for Nd2O3-H2O-CO2 and Gd2O3-H2O-CO2 systems at 1500 atm are given along with the results of selected runs in La, Sm and Eu systems. The stable phases in systems of La and Nd, are Ln(OH)CO3-B, Ln2O2CO3-II and LnOOH, in addition to the Ln(OH)3 phase at extremely low partial pressures of CO2 in the system. The systems become more and more complex with decreasing ionic radi and the number of stable carbonate phases increases. Ln2(CO3)3 · 3H2O orthorhombic (tengerate-like phase) is stable from Sm to Gd in addition to the other phases. The Gd(OH)CO3-A (ancylite-like phase) is hydrothermally stable at XCO2 greater-or-equal, slanted 0.5 while its hexagonal polymorph, Gd(OH)CO3-B is stable at low partial pressures of CO2 in the system.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Cesium hydrogen l-malate monohydrate, CsH(C4H4O5)·H2O, is a new chiral open-framework semi-organic crystalline material with a second-harmonic generation efficiency one order of magnitude greater than KDP. Single crystals of this new material have been grown by the conventional slow cooling technique from aqueous solution. Grown crystals display both platy and prismatic morphologies depending on the imposed supersaturation. Hardness values measured using Vickers hardness indenter show considerable anisotropy. The resistivity behavior at room temperature and above, places the crystal between an ionic conductor and a dielectric. The single-crystal SHG efficiency estimated through Maker fringes experiment gives deff which is 4.24 times that of KDP. Single and multiple shot experiments performed on the grown crystals for the fundamental and second harmonic of pulsed Nd:YAG laser (1064 and 532 nm) show that it exhibits a high laser damage threshold which is a favorable property for nonlinear optical applications.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Good quality single crystals of copper metagermanite, CuGeO3, are grown by flux technique. Growth is carried out at relatively low temperatures by using Bi2O3 along with CuO in an optimal flux ratio. Besides rendering the procedure simple, lower growth temperature reduces growth defect concentration. Single crystals of Cu1 - xCoxGeO3 and CuGe1 - yGayO3 are grown by the same method for different values of x and y to investigate the influence of in-chain and off-chain doping on spin-Peierls (SP) transition. Change in color, morphology and surface features as a result of doping are briefly discussed. Spin-Peierls transition of these crystals is studied by susceptibility measurements on a commercial SQUID magnetometer. Cationic substitution resulted in reduction of spin-Peierls transition temperature (T-SP) of CuGeO3. Substitution of magnetic impurity cobalt in-chain site caused more pronounced effects such as suppression of SP phase.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Crystal growth of YIG from fluxes containing lead sulphate in place of lead oxide in the usual lead oxide-lead fluoride-boron oxide flux system has been tried. Lead sulphate decomposes during crystal growth giving lead oxide and sulphur trioxide. Due to the influence of sulphur trioxide in the system the yield of crystals almost doubles. There is no change either in the morphology of the crystals or their lattice parameter. It is possible that solubility of YIG is different in the new flux and the changed solubility causes the increase in yield of crystals.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Three new three-dimensional zinc-triazolate-oxybis(benzoate) compounds. [{Zn-3(H2O)(2)}{C12H8O(COO)(2)}(2)-{C2H2N3}(2)]center dot 2H(2)O(I), [Zn-7{C12H8O(COO)(2)}(4){C2H2N3}(6)]center dot H2O, (II), and[{Zn-5(OH)(2)}{C12H8O(COO)(2)}(3){C2H2N3}(2)] (III), synthesized by a hydrothermal reaction of a mixture of Zn(OAc)(2)center dot 2H(2)O, 4,4'-oxybis(benzoic acid), 1,2,4-triazole, NaOH, and water. Compound I has an interpenetrated diamond structure and II and III have pillared-layer related structures. The formation of a hydrated phase (I) at low temperature and a completely dehydrated phase (III) at high temperature suggests the importance of thermodynamic factors in the formation of three compounds. Transformation studies of I in the presence of water shows the formation of a simple Zn-OBA compound, [Zn(OBA)(H2O)] (IV), at 150 and 180 degrees C and compound III at 200 degrees C. The compounds have been characterized by single-crystal X-ray diffraction, powder X-ray diffraction. thermogravimetric analysis, IR, and photoluminescence studies.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Single crystals of tin oxide have been grown under conditions obtained in oil fired porcelain tunnel kilns. It was noted that the reducing conditions in the kilns help in the growth of SnO2 crystals at much lower temperatures (1300°C). The growth seems to more pronounced in presence of silicon carbide. The crystals grow as long fibres of 0.1 to 0.5 mm dia. and 10 to 50 mm length. The crystals exhibit rutile structure and the direction of growth seems to be favoured in any one of the major axes a and c.