Resumo:

Pinning by second phase particles offers a potent means for limiting grain growth and enhancing superplasticity in alumina-based ceramics. In the present study, a colloidal technique was used to produce green bodies of alumina-yttria composites; at elevated temperatures, the yttria particles react with alumina to produce YAG particles. The densification and high temperature deformation characteristics of alumina-YAG composites were studied using conventional free sintering and sinter-forging, which involves the application of a compressive stress without any lateral constraints. It is shown that the YAG particles retard both densification and grain growth. The experiments indicate also that the presence of YAG particles does not significantly alter the stress exponent for creep deformation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanoindentation technique was employed to measure the changes in mechanical properties of a glass preform subjected to different levels of UV exposure. The results reveal that short-term exposure leads to an appreciable increase in the Young's modulus (E), suggesting the densification of the glass, confirming the compaction-densification model. However, on prolonged exposure, E decreases, which provides what we believe to be the first direct evidence of dilation in the glass leading into the Type IIA regime. The present results rule out the hypothesis that continued exposure leads to an irreversible compaction and prove that index modulation regimes are intrinsic to the glass matrix.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dense ZrB2-SiC (25-30 vol%) composites have been produced by reactive hot pressing using stoichiometric Zr, B4C, C and Si powder mixtures with and without Ni addition at 40 MPa, 1600 degrees C for 60 min. Nickel, a common additive to promote densification, is shown not to be essential; the presence of an ultra-fine microstructure containing a transient plastic ZrC phase is suggested to play a key role at low temperatures, while a transient liquid phase may be responsible at temperatures above 1350 degrees C. Hot Pressing of non-stoichiometric mixture of Zr, B4C and Si at 40 MPa, 1600 degrees C for 30 min resulted in ZrB2-ZrCx-SiC (15 vol%) composites of similar to 98% RD.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Synthesis and densification of monolithic zirconium carbide (ZrC) has been carried out by reactive hot pressing of zirconium (Zr) and graphite (C) powders in the molar ratios 1:1, 1.25:1, 1.5:1, and 2:1 at 40 MPa, 1200 degrees-1600 degrees C. Monolithic ZrC could be synthesized with a C/Zr ratio similar to 0.5-1.0 and the post heat-treated samples have the lattice parameter in the range 4.665 to 4.698 A. Densification improves with an increasing deviation from the stoichiometry. Fine-grained (similar to 1 mu m) and nearly fully dense material (99% RD) could be obtained at a temperature as low as 1200 degrees C with C/Zr similar to 0.67. Microstructural and XRD observations suggest that densification occurred at low temperatures with nonstoichiometric Zr-C powder mixtures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Wear tests were done in a pin-on-disc machine by sliding MoSi2 pins against hard-steel discs in a normal load range of 5-140 N and a speed of 0.5 m/s under nominally dry conditions in the ambient. The specific wear rate of the pin undergoes two transitions: severe to mild at low load and mild to severe at high load. The mild-wear domain is distinguished by the formation of a protective mechanically mixed layer of steel and its oxides, transferred from the counterface in particulate form. Increasing the hardness by densification and TiB2 reinforcement lowers the specific wear rate and expands the mild-wear load domain. However, even when the volume wear rate is normalised with respect to the real contact area (load/hardness) the non-dimensional wear factor is still seen to decrease with densification and reinforcement. This indicates that fracture toughness may also play an important role in determining the wear-resistance of these materials. The surface coverage on the pin by the mechanically mixed layer increases with densification and reinforcement.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the results of transmission electron microscopy (TEM) study, carried out on a hot-pressed TiB2-20 wt.%MoSi2 composite. One of the important microstructural observations includes the detection of crystalline TiSi2 at triple grain junctions. The densification mechanism is discussed, based on experimental observations and thermodynamic analysis

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this article, we examine the unusual plastic deformation under uniaxial compression of an Al2O3-15 mol % Y2O3 (A15Y) glass synthesized by a wet chemical route At a low temperature of 650-725 degrees C, plastic deformation of this glass is largely non-viscous through shear instabilities In contrast deformation near the crystallization temperature (850 degrees C) occurs homogeneously with work hardening and with a monotonic increase in the true density of the glass by 10-12% accompanied by an increase in hardness (H) and elastic modulus (E) of up to 100% We hypothesize a phenomenon of molecular densification of the amorphous structure through a hierarchy of multiple phases, analogous to density- or entropy-driven amorphous to-amorphous phase transitions (polyamorphism) These results suggest that the present method of preparation and the unusual behavior can trigger a search for many more systems that display such behavior (C) 2010 Acta Materialia Inc Published by Elsevier Ltd All rights reserved

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Devitrification of spray pyrolysed, amorphous ZrO2-Al2O3 solid solution produces nanocrystalline microstructures (grain sizes 10-20 nm). In this study, spray pyrolysed amorphous ZrO2-40 mol% Al2O3 powder displayed good sinterability during decomposition, after spraying, of the nitrate precursors up to 1023K. Hot pressing of fully pyrolysed, pre-sintered (more than 70% dense) pellets at 923K and 750 MPa produced an amorphous pellet with less than 2% porosity. The results indicate the possibility of producing dense, amorphous pellets that can be heat treated further to produce nanocrystalline microstructures conducive for superplasticity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The influence of powder processing and sintering temperature on densification, microstructure and mechanical properties of hydroxyapatite (HAp) ceramics was studied. The as-dried, calcined and processed HAp powders were uniaxially compacted and sintered at various temperatures (1000-1400 degreesC) for 3 h. The as-dried and processed powders, attained 97% of theoretical density (TD) at 1100 degreesC) at higher sintering temperatures, the density of the as-dried powder compact was found to decrease. A uniform microstructure with fine grain size (2.3 pm) was observed for material obtained from processed powder, whereas exaggerated grain growth with closed pores were observed in as-dried and unprocessed powder compacts. The Vickers' hardness, fracture toughness and flexural strength of HAp were determined and a maximum value of 6.3 GPa and 0.88 MPam(1/2) and 60.3 MPa, respectively were obtained for processed compact. The processing of HAp has improved its densification, microstructure homogeneity and mechanical properties. (C) 2002 Elsevier Science Ltd and Techna S.r.l. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, we report the results of a transmission electron microscopy investigation on WC–6 wt% ZrO2nanocomposite, spark plasma sintered at 1300 °C, for varying times of up to 20 min. The primary aim of this work was to understand the evolution of microstructure during such a sintering process. The investigation revealed the presence of nanocrystalline ZrO2particles (30–50 nm) entrapped within submicron WC grains. In addition, relatively coarser ZrO2(60–100 nm) particles were observed to be either attached to WC grain boundaries or located at WC triple grain junctions. The evidence of the presence of a small amount of W2C, supposed to have been formed due to sintering reaction between WC and ZrO2, is presented here. Detailed structural investigation indicated that ZrO2in the spark plasma sintered nanocomposite adopted an orthorhombic crystal structure, and the possible reasons for o-ZrO2formation are explained. The increase in kinetics of densification due to the addition of ZrO2is believed to be caused by the enhanced diffusion kinetics in the presence of nonstoichiometric nanocrystalline ZrO2.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Densification characteristics of amorphous ZrO2-40 mol% Al2O3 powder with 3 to 15 mu m nominal particle size range, produced by spray pyrolysis, have been studied by conducting hot pressing experiments at 573, 723 and 873 K with uniaxial pressures of 250, 500 and 750 MPa. Most of the increase in relative density from the starting value of similar to 40% occurred during loading up to the desired pressure. The increments in density during 1 hour constant pressure dwells were less than 4% at all temperatures and pressure. Inter-particle bonding was not observed at 573 K. Correlation between the results with a viscous sintering model for hot pressing is not satisfactory for describing the behavior as normal viscous sintering.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The present work demonstrates the synthesis of Cu-10 wt% TiB2 composites with a theoretical density of more than 90% by tailoring the spark plasma sintering (SPS) conditions in the temperature range of 400-700 degrees C. Interestingly, 10 wt% Pb addition to Cu-10 wt% TiB2 lowers the sinter density and the difference in the densification behavior of the investigated compositions was discussed in reference to the current profile recorded during a SPS cycle. The sintering kinetics and phase assemblage were also discussed in reference to surface melting of the constituents prior to bulk melting temperature, temperature dependent wettability of Pb on Cu, diffusion kinetics of Cu as well as the formation of various oxides. An important result is that a high hardness of around 2 GPa and relative density close to 92% qtheoretical was achieved for the Cu-10 wt% TiB2-10 wt% Pb composite, and such a combination has never been achieved before using any conventional processing route.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The present paper is aimed to understand the sub-processes triggered by rapid heating during spark plasma sintering as well as to assess the extent to which densification and properties of metallic materials can be enhanced using such superfast consolidation process. Using nanocrystalline Cu-Pb as a model system, the influence of Pb as well as TiB2 addition on the densification mechanisms and properties are discussed. Importantly, a high hardness of 2 GPa is achieved in Cu-based nanocomposites. (C) 2013 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The dominant densification mechanisms for hot pressing of ZrB2-20 vol.% SiC composite at different hot-pressing temperatures and pressures was identified. The dominant densification mechanisms were found to change over a very short temperature range. For hot pressing at 1700 degrees C, the dominant densification mechanism was found to be mechanically driven particle fragmentation and rearrangement only, whereas at 1850 degrees C a plastic flow mechanism started to become dominant after initial particle fragmentation and rearrangement. At 2000 degrees C, the dominant mechanism changed from plastic flow to grain boundary diffusion. (c) 2013 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spark plasma sintering (SPS) is a convenient and rapid means of producing dense ceramic compacts. However, the mechanisms responsible for rapid densification have not been identified satisfactorily, with different studies using an indirect approach yielding varied values for the densification parameters. This study involved SPS in high purity nanocrystalline alumina with temperatures ranging from 1173 to 1423K and stresses from 25 to 100MPa. A direct approach, with analyses at a constant density, revealed a stress exponent of similar to 1 and an inverse grain size dependence of similar to 3, consistent with Coble creep process. Whereas the direct approach gives a stress exponent of similar to 1, the indirect approach used previously gives stress exponents ranging from similar to 2.2 to 3.5 with the same data, thereby revealing potentially spurious values of the densification parameters from conventional indirect approaches to characterizing densification. The rapid densification during SPS is related to the finer grain sizes retained with the rapid heating rates and the imposed stress that enhances the driving force for densification.